PROCESSES FOR DECOMPOSING ALUMINUM CHLORIDE INTO ALUMINA
    1.
    发明申请
    PROCESSES FOR DECOMPOSING ALUMINUM CHLORIDE INTO ALUMINA 审中-公开
    将氯化铝分解成铝的方法

    公开(公告)号:WO2015176166A1

    公开(公告)日:2015-11-26

    申请号:PCT/CA2015/000334

    申请日:2015-05-21

    Abstract: There are provided processes for decomposing AlCl 3 •6H 2 O into γ-Al 2 O 3 that comprise heating the AlCl 3 •6H 2 O at a temperature of about 600°C to about 800°C in the presence of steam and optionally at least one gas (for example chosen from air, argon, nitrogen, carbon dioxide, hydrogen and hydrochloric acid), under conditions suitable to obtain the γ-Al 2 O 3 . For example, the γ-Al 2 O 3 obtained can be suitable for use in an aluminum smelting process or optionally for processes for treating the γ-Al 2 O 3 to obtain high purity alumina, fused alumina, transition alumina, tabular alumina, calcined alumina, ultra-pure alumina or specialty alumina.

    Abstract translation: 提供了将AlCl 3·6H 2 O分解成γ-Al 2 O 3的方法,其包括在蒸汽和任选的至少一种气体(例如选自空气)的情况下,在约600℃至约800℃的温度下加热AlCl 3·6H 2 O ,氩气,氮气,二氧化碳,氢气和盐酸)中,在适于获得γ-Al 2 O 3的条件下进行。 例如,所得到的γ-Al 2 O 3可适用于铝冶炼工艺,也可适用于处理γ-Al2O3以获得高纯度氧化铝,熔融氧化铝,过渡型氧化铝,片状氧化铝,煅烧氧化铝,超纯氧化铝 或特种氧化铝。

    СПОСОБ ПОЛУЧЕНИЯ ГЛИНОЗЕМА ИЗ НИЗКОСОРТНОГО АЛЮМИНИЙСОДЕРЖАЩЕГО СЫРЬЯ
    2.
    发明申请

    公开(公告)号:WO2014104920A1

    公开(公告)日:2014-07-03

    申请号:PCT/RU2012/001145

    申请日:2012-12-29

    CPC classification number: C01F7/306 C01F7/56 C01P2006/80

    Abstract: Изобретение относится к металлургии, в частности к кислотным способам получения глинозема и может быть использовано при переработке низкосортного алюминийсодержащего сырья. Способ получения глинозема включает обработку алюминийсодержащего сырья соляной кислотой с образованием хлоридной пульпы, разделение пульпы с выделением хлоридного раствора, высаливание гексагидрата хлорида алюминия из хлоридного раствора хлоридом кальция, термическое разложение гексагидрата хлорида алюминия с образованием глинозема. Для повышения качества глинозема и снижения энергозатрат хлоридную пульпу нейтрализуют оксидом кальция до достижения рН, равного 1,6-2,2, маточный раствор после высаливания гексагидрата хлорида алюминия постадийно упаривают с селективной кристаллизацией хлоридов щелочных металлов и выделением хлорида кальция в виде кристаллов и/или концентрированного водного раствора, причем часть хлорида кальция возвращают на высаливание гексагидрата хлорида алюминия.

    Abstract translation: 本发明涉及冶金,特别是生产氧化铝的酸法,可用于加工低品位的含铝原料。 生产氧化铝的方法包括用盐酸形成氯化物淤浆处理含铝原料,分离浆料并回收氯化物溶液,使用氯化钙从氯化物溶液中氯化铝六水合盐析出,并将氯化铝六水合物 从而生产氧化铝。 为了提高氧化铝的质量并降低能量消耗,氯化钙浆料使用氧化钙中和至1.6-2.2的pH,并且随着氯化铝六水合物的盐析,母液逐步蒸发,在该过程中碱 选择性地结晶金属氯化物,并以晶体和/或浓缩水溶液的形式回收氯化钙,由此将氯化钙的一部分再循环到氯化铝六水合物的盐析中。

    ALUMINA AND CARBONATE PRODUCTION METHOD FROM AL-RICH MATERIALS WITH INTEGRATED CO2 UTILIZATION
    6.
    发明申请
    ALUMINA AND CARBONATE PRODUCTION METHOD FROM AL-RICH MATERIALS WITH INTEGRATED CO2 UTILIZATION 审中-公开
    具有一体化二氧化碳利用的富含材料的氧化铝和碳酸盐生产方法

    公开(公告)号:WO2015137823A1

    公开(公告)日:2015-09-17

    申请号:PCT/NO2015/050049

    申请日:2015-03-11

    Abstract: A process for alumina and carbonate production from aluminium rich materials with integrated CO 2 utilization, comprising: comminuting and leaching Al-rich materials in concentrated HCI; separating unreacted material from metal chloride solution; separating Al 3+ from solution by crystallization of AlCl 3 ·6H 2 O; calcination of AlCl 3 ·6H 2 O with HCl recovery; precipitation of metal carbonates from CO 2 ; regeneration of HCl and extractive amines; the Al 3+ separation the facilitated by increasing HCl concentration; the calcination being performed in two steps, one in the range 400 and 600°C to generate a HCl-rich gas and one above 600°C to produce Al 2 O 3 ; for precipitating metal carbonates, mixing the metal chloride solution with an organic solution containing a selected amine and contacting the mixture with a CO 2 -containing gas, thereby also extracting HCl by formation of an ammonium chloride salt complex; processing thermally or chemically the organic solution to regenerate the amine for recirculation.

    Abstract translation: 一种具有一体化二氧化碳利用的富铝材料生产氧化铝和碳酸盐的方法,包括:将浓缩HCl中的富Al材料粉碎和浸出; 从金属氯化物溶液中分离出未反应的物质; 通过AlCl3·6H2O的结晶从溶液中分离出Al3 +; 用HCl回收煅烧AlCl3·6H2O; 二氧化碳沉淀金属碳酸盐; HCl和萃取胺的再生; 通过增加HCl浓度促进Al3 +分离; 煅烧分两步进行,一个在400和600℃范围内,产生富含HCl的气体,一个高于600℃,生成Al2O3; 用于沉淀金属碳酸盐,将金属氯化物溶液与含有选择的胺的有机溶液混合并将该混合物与含CO 2的气体接触,从而也通过形成氯化铵盐络合物来提取HCl; 加热或化学处理有机溶液以再生胺用于再循环。