公开(公告)号:WO2023067498A1
公开(公告)日:2023-04-27
申请号:PCT/IB2022/059998
申请日:2022-10-18
申请人: POMETON SPA
摘要: A plant (1') for obtaining metal powders, preferentially iron powder from metal oxide powders, preferentially from iron oxide powders is described. The plant (1') comprising at least one furnace (24) having a treatment chamber (28) rotatable around a first rotation axis (C) and configured to contain the metal oxide powders, to be transformed into metal powders, a first actuator device configured to induce a rotation of the treatment chamber (28) around the first rotation axis (C), a plurality of grinding bodies (29) arranged in the treatment chamber (28), a heating device configured to heat, in use, an internal space (29) of the treatment chamber (28) to a temperature of at least 900°C, preferentially at least 1000°C, and a conditioning device configured to introduce, in use, hydrogen and/or maintain a desired concentration of hydrogen in the treatment chamber (28).
-
2.
公开(公告)号:WO2023062130A1
公开(公告)日:2023-04-20
申请号:PCT/EP2022/078517
申请日:2022-10-13
发明人: SAEUBERLICH, Tino , EXNER, Jürgen , WARNECKE, Knut , OELMANN, Harald , MEESE-MARKTSCHEFFEL, Juliane
摘要: Die vorliegende Erfindung betrifft ein Verfahren zur Herstellung eines Wolframmetall-Pulvers mit einer spezifischen BET-Oberfläche von größer 8 m²/g und ein mittels dieses Verfahrens erhältliches Wolframmetall-Pulver.
-
公开(公告)号:WO2022108488A1
公开(公告)日:2022-05-27
申请号:PCT/RU2021/050366
申请日:2021-11-01
摘要: Способ получения высокодисперсных железосодержащих порошков из техногенных отходов станций водоподготовки подземных вод включает диспергирование осадка промывных вод воздействием, обеспечивающим эквивалентный диаметр частиц не более 100 микрон и не менее чем 90% частиц от общего числа частиц; обезвоживание осадка промывных вод до относительной влажности не более 90%; загрузку или поточную подачу осадка промывных вод в реакционную камеру или реактор; восстановление соединений железа, содержащихся в осадке промывных вод в реакционной камере или реакторе в газовой среде, имеющей восстановительный потенциал и состоящий не менее чем на 95% из смеси монооксида и диоксида углерода при температуре от 300 до 900°С; сепарацию частиц целевого продукта - соединений железа, имеющих ферромагнитные свойства, от компонентов сырьевой смеси; охлаждение до 90°С и менее для снижения химической активности получаемых железосодержащих порошков с целью предотвращения преждевременного окисления при контакте с окисляющими веществами, в том числе с кислородом воздуха.
-
公开(公告)号:WO2021106008A1
公开(公告)日:2021-06-03
申请号:PCT/IN2020/050517
申请日:2020-06-11
申请人: DHOKEY, Narendra , SHINDE, Sameer
发明人: DHOKEY, Narendra , SHINDE, Sameer
摘要: A countercurrent reactor for powder metallurgy processes, said reactor comprising a rotary kiln (300) with variable angle, said rotary kiln (300) being provided on a bed (301) configured with a movable mechanism (302), at its second end (304), in order to provide said variable angle to said rotary kiln (300); thereby making flow of input powder, from its first end (306), to be gravity fed in order to achieve controlled angled flow rate for said input powder.
-
公开(公告)号:WO2019009136A1
公开(公告)日:2019-01-10
申请号:PCT/JP2018/024121
申请日:2018-06-26
申请人: 東邦チタニウム株式会社
摘要: 積層セラミックコンデンサの内部電極の薄層化に伴うコンデンサの容量低下を改善し得る、内部電極の導電ペーストに好適な金属粉末を提供する。金属粉末は、金属粒子が連結してなる連結粒子のうち、アスペクト比が1.2以上であり、円形度が0.675以下であり、長径が金属粉末の個数50%径の3倍以上である連結粒子が上記金属粉末に含まれる割合が、個数基準で500ppm以下である。
-
公开(公告)号:WO2018051106A1
公开(公告)日:2018-03-22
申请号:PCT/GB2017/052725
申请日:2017-09-14
申请人: METALYSIS LIMITED
发明人: MELLOR, Ian , DOUGHTY, Greg
CPC分类号: B22F9/20 , B22F1/025 , B22F3/1055 , B22F9/026 , B22F9/18 , B22F9/22 , B22F2009/245 , B22F2202/15 , B22F2998/10 , B22F2999/00 , C22C32/0031 , C22C32/0047 , C22C32/0052 , C22C32/0084 , C22C2001/1089 , Y02P10/295 , B22F3/1039 , B22F2201/01 , B22F3/16 , B22F3/02
摘要: Method of Producing a Composite Material A method of forming a composite material comprising a matrix phase and a reinforcement phase distributed within the matrix phasecomprises the step of growing a plurality of precursor particles comprising a matrix precursor material and a reinforcement precursor material using a fluidised-bed spray granulation process, thereby forming a precursor powder (190).The matrix precursor material comprisesa reducible compound comprising a first metal and oxygen. The precursor powder is reduced under conditions in which oxygen is removed from the matrix precursor material.The matrix phase of the composite comprises the first metal, and the reinforcement phase of the composite either consists of the reinforcement precursor material or derives from a reaction of the reinforcement precursor material.A precursor powder (190) and a composite material are also provided. (Figure4)
摘要翻译: 制造复合材料的方法形成包含基体相和分布在基体相内的增强相的复合材料的方法包括生长多个前体颗粒的步骤,所述前体颗粒包含基体前体材料和 使用流化床喷雾造粒工艺制备增强前体材料,从而形成前体粉末(190)。所述基体前体材料包含含有第一金属和氧的可还原化合物。 在从基体前体材料中除去氧的条件下,前体粉末被还原。复合材料的基体相包含第一金属,并且复合材料的增强相或者由增强材料前体材料组成或者来源于 增强前体材料。还提供前体粉末(190)和复合材料。 (图4) P>
-
公开(公告)号:WO2018012458A1
公开(公告)日:2018-01-18
申请号:PCT/JP2017/025136
申请日:2017-07-10
申请人: DOWAエレクトロニクス株式会社
摘要: 【課題】複素比透磁率のμ'が大きく、かつ十分に小さなtanδを有する、鉄粉を提供する。 【解決手段】3価の鉄イオンとリン含有イオンを含む酸性の水溶液をアルカリ水溶液で中和して水和酸化物の沈殿物のスラリーを得る工程、もしくは、3価の鉄イオンを含む酸性の水溶液をアルカリ水溶液で中和して得られる水和酸化物の沈殿物を含むスラリーにリン含有イオンを添加する工程の後、得られたスラリーにシラン化合物を添加して水和酸化物の沈殿物にシラン化合物の加水分解生成物を被覆し、その被覆後の水和酸化物の沈殿物を固液分離して回収し、回収した沈殿物を加熱してシリコン酸化物を被覆した鉄粒子を得た後、シリコン酸化物被覆の一部または全てを溶解除去する。
摘要翻译: 要解决的问题:提供复相对磁导率μ'大且足够小的tanδ的铁粉。 三价步骤酸性含有铁离子和含磷离子的水溶液被中和用碱水溶液,得到的水合氧化物的沉淀物,或含酸性3价铁离子的浆液 加入含磷离子以含有通过中和用碱的水溶液的水溶液得到的水合氧化物的沉淀物的浆料的步骤之后,水合氧化物的沉淀物通过添加硅烷化合物到所得浆液 ,涂布硅烷化合物的水解产物,通过固液分离回收涂布后的水合氧化物沉淀物,加热回收的沉淀物,并获得涂覆有氧化硅的铁颗粒 ,部分或全部氧化硅涂层被溶解掉。 p>
-
公开(公告)号:WO2017111334A1
公开(公告)日:2017-06-29
申请号:PCT/KR2016/013892
申请日:2016-11-29
申请人: 영남대학교 산학협력단
IPC分类号: C01B21/072 , B22F9/22
CPC分类号: B22F9/22 , C01B21/072
摘要: 본 발명은 질화알루미늄의 저온 합성 방법에 관한 것으로, 보다 상세하게는 0.5 내지 8 중량%의 아연 분말, 0.01 내지 2 중량%의 마그네슘 분말, 0.01 내지 1 중량%의 실리콘 분말, 0.01 내지 1 중량%의 구리 분말 및 잔량의 알루미늄 분말을 포함하는 혼합분말을 유기결합제와 가압혼련하여 만든 피드스탁 과립 또는 이것으로 만들어지는 성형체를 상압의 질소가스분위기 하에서 가열탈지하여 다공질체를 만들고 이어 알루미늄 분말의 급격한 질화반응을 유발시키는 것을 특징으로 하는 질화알루미늄 합성방법에 관한 것이며, 추가로 리튬, 칼슘, 인, 가돌리움, 철, 니켈, 코발트, 망간, 은, 크롬, 지르코늄, 스트론튬, 몰리브데늄, 텅스텐 및 이들의 합금 혹은 Al 2 O 3 , SiO 2 , ZrO 2 , CaO, Y 2 O 3 , TiC, TiN, B 4 C, SiC, Si 3 N 4 , TiB 2 , h-BN, c-BN, 다이어몬드, 탄소나노튜브 및 그래핀으로 이루어진 군에서 선택된 하나 이상의 무기물을 상기 알루미늄 혼합분말에 더 첨가하여 질소가스분위기하에서 소결함으로써 질화알루미늄 함량이 높은 복합상 물질을 합성하는 방법에 관한 것이다.
摘要翻译:
本发明涉及氮化铝的低温合成法,更具体而言,0.5〜8%重量的锌粉末,0.01〜2%(重量)的镁粉末的,0.01至1重量%的硅 加热混合粉末的模制产品,包括粉末,0.01至铜粉末和按重量计由原料颗粒或它制成的1%的铝粉末的剩余量通过捏合有机粘合剂,并在脱脂常压下在氮气气氛中的压力和多孔材料 创建随后涉及的氮化铝的合成方法,包括:使铝粉末,额外锂,钙,磷,红景天日光浴室,铁,镍,钴,锰,银,铬,锆,锶的快速氮化反应的步骤, Sub 2,SiO 2,ZrO 2,CaO ,Y 2 O 3 O 3,TiC,TiN,B 3, 硅<子> 3 子>名词<子> 4 子>,的TiB <子> 2 子>,的h-BN,C-BN,金刚石,碳纳米管,并且是选自下组的销 涉及选择以通过在氮气气氛下进行烧结合成具有氮化铝的含量高的复合材料的方法,一种或多种矿物,被进一步添加到铝粉末混合物。 p>
-
公开(公告)号:WO2016004219A1
公开(公告)日:2016-01-07
申请号:PCT/US2015/038855
申请日:2015-07-01
发明人: MEDHEKAR, Vinay
CPC分类号: B01J31/185 , B01J23/755 , B01J31/1845 , B01J31/26 , B01J35/023 , B01J35/026 , B01J35/1009 , B01J37/04 , B01J37/14 , B01J37/16 , B01J37/18 , B01J2231/322 , B01J2531/847 , B22F9/22 , B22F2999/00 , B22F2201/013 , B22F2201/02
摘要: Methods are described herein that involve rotating or gently mixing nickel(II)-containing particles in a reaction vessel while heating the particles and flowing a reducing atmosphere through the reaction vessel for a time sufficient to generate free-flowing nickel metal (Ni(0)) from the nickel(II)-containing particles.
摘要翻译: 本文描述的方法包括在加热颗粒并使还原气氛通过反应容器流动足以产生自由流动的镍金属(Ni(0))的时间的同时在反应容器中旋转或轻轻混合含镍(II)的颗粒, )来自含镍(II)的颗粒。
-
公开(公告)号:WO2015156080A1
公开(公告)日:2015-10-15
申请号:PCT/JP2015/057325
申请日:2015-03-12
申请人: 東邦チタニウム株式会社
摘要: 積層セラミックコンデンサの製造工程において優れた焼結特性を有し、積層セラミックコンデンサの電極層と誘電体層の間の剥離や電極層のクラックといった欠陥の発生を防止することができるニッケル粉末を提供する。ニッケル粉末は1.0~5.0質量%の硫黄を含有し、個数50%径を0.09μm以下とする。
摘要翻译: 提供一种在层压陶瓷电容器的制造工艺中具有优异的烧结特性的镍粉末,并且能够防止层压陶瓷电容器中的缺陷发生,例如电极层中的裂纹和电极层与电介质层之间的分离。 镍粉含有1.0-5.0质量%的硫,其中50%的粒子具有小于或等于0.09μm的尺寸。
-
-
-
-
-
-
-
-
-