公开(公告)号:WO2022031481A1
公开(公告)日:2022-02-10
申请号:PCT/US2021/043368
申请日:2021-07-28
申请人: MILLIKEN & COMPANY
发明人: DOTSON, Darin , XU, Xiaoyou , FORRISTER, Walter
IPC分类号: B29C48/00 , B29C49/00 , B29C55/00 , B29C55/28 , C08L23/06 , B29C48/0018 , B29C48/022 , B29C48/10 , B29K2023/06 , B29L2023/001 , C08F110/02 , C08J2323/06 , C08J2423/06 , C08J5/18 , C08K2201/014 , C08K5/098 , C08L2201/14 , C08L2203/16 , C08L2203/30 , C08L2205/025 , C08L2205/03 , C08L2205/24 , C08L2310/00
摘要: A thermoplastic polymer composition comprises a polyethylene polymer composition and a salt of bicyclo[2.2.1]heptane-2,3-dicarboxylic acid. The polyethylene polymer composition can have a Melt Relaxation Index of 2 or greater. A method for molding a thermoplastic polymer composition comprises the steps of (a) providing an apparatus comprising a die with an annular orifice, a means for blowing pressurized fluid into a tube exiting the die orifice, and a means for drawing and collecting the tube; (b) providing the thermoplastic polymer composition described above; (c) heating the thermoplastic polymer composition to melt the thermoplastic polymer composition; (d) extruding the molten thermoplastic polymer composition through the die to form a tube; (e) blowing a pressurized fluid into the tube to inflate the tube while simultaneously drawing it; (f) allowing the film to cool; and (g) collecting the film.
-
公开(公告)号:WO2021257530A1
公开(公告)日:2021-12-23
申请号:PCT/US2021/037372
申请日:2021-06-15
IPC分类号: C08J7/048 , C08J7/046 , C08J7/04 , C08J5/18 , C09D133/00 , B29C70/544 , C08L101/00 , C08L2201/14 , C08L2203/16 , C09D5/00
摘要: The present disclosure relates to a multifunctional film for a vacuum bag that may include a flexible barrier film that may include a textured surface. The multifunctional film may further include a release coating overlying the textured surface of the flexible barrier film. The multifunctional film may further have an oxygen (O2) permeability of not greater than about 1100 cc/(m2-day-atm) and a stability rating of not greater than about 90%, where the stability rating is defined as the maximum percent decrease in elongation at break as measured using ASTM D882 after being exposed to a temperature of 200 °C for 12 hours.
-
公开(公告)号:WO2022031480A1
公开(公告)日:2022-02-10
申请号:PCT/US2021/043367
申请日:2021-07-28
申请人: MILLIKEN & COMPANY
发明人: DOTSON, Darin , XU, Xiaoyou , FORRISTER, Walter
IPC分类号: C08L23/06 , B29C48/00 , B29C49/00 , B29C55/00 , B29C55/28 , B29C2948/92704 , B29C48/0017 , B29C48/022 , B29C48/09 , B29C49/0005 , B29C49/04 , B29K2023/06 , C08K2003/267 , C08K3/26 , C08K5/098 , C08L2201/14 , C08L2203/30 , C08L2205/025 , C08L2310/00
摘要: A thermoplastic polymer composition comprises a polyethylene polymer composition and a salt of bicyclo[2.2.1]heptane-2,3-dicarboxylic acid. The polyethylene polymer composition can have a Melt Relaxation Ratio of 1.5 or greater. A method for molding a thermoplastic polymer composition comprises the steps of (a) providing an apparatus comprising a die and a mold cavity; (b) providing the thermoplastic polymer composition described above; (c) heating the thermoplastic polymer composition to melt the thermoplastic polymer composition; (d) extruding the molten thermoplastic polymer composition through the die to form a parison; (e) capturing the parison in the mold cavity; (f) blowing a pressurized fluid into the parison to inflate the parison and conform it to the interior surface of the mold cavity; (g) allowing the molded article to cool so that the molded article retains its shape; and (h) removing the molded article from the mold cavity.
-
-