Abstract:
A semiconductor structure can include two or more epitaxial oxide materials with different properties, such as compositions, crystal symmetries, or bandgaps. The semiconductor structures can comprise one or more epitaxial oxide layers formed on a compatible substrate with in-plane lattice parameters and atomic positions that provide a suitable template for the growth of the epitaxial oxide materials. One or more of the epitaxial oxide materials can be strained. One or more of the epitaxial oxide materials can be doped n- or p-type. The semiconductor structure can comprise a superlattice with epitaxial oxide materials. The semiconductor structure can comprise a chirp layer with epitaxial oxide materials. The semiconductor structures can be a portion of a semiconductor device, such as an optoelectronic device, a light emitting diode, a laser diode, a photodetector, a solar cell, a high-power diode, a high-power transistor, a transducer, or a high electron mobility transistor.
Abstract:
The invention relates to an optical element (133) for transmitting radiation in wavelengths of less than 250 nm, especially of 193 nm, consisting of a material containing magnesium-aluminium spinel. In the optical element (133), the ratio (V) of the aluminium part in the magnesium-aluminium spinel to the magnesium part in the magnesium-aluminium spinel varies by less than 200 ppm, preferably less than 100 ppm, especially preferably less than 50 ppm, and/or is between 2.0 and 2.2, preferably between 2.02 and 2.10, especially preferably between 2.04 and 2.08. The invention also relates to a projection objective and a projection illumination system comprising such an optical element, and to a production method for a blank (1) for producing the optical element (133).
Abstract:
A method of forming a metal gallate spinel structure that includes mixing a divalent metal-containing salt and a gallium-containing salt in solution with fermentative or thermophilic bacteria. In the process, the bacteria nucleate metal gallate spinel nano-objects from the divalent metal-containing salt and the gallium-containing salt without requiring reduction of a metal in the solution. The metal gallate spinel structures, as well as light-emitting structures in which they are incorporated, are also described.
Abstract:
A method for preparing a suspension of LDH particles comprises the steps of preparing LDH precipitates by coprecipitation to form a mixture of LDH precipitates and solution; separating the LDH precipitates from the solution; washing the LDH precipitates to remove residual ions; mixing the LDH precipitates with water; and subjecting the mixture of LDH particles and water from step (d) to a hydrothermal treatment step by heating to a temperature of from greater than 80 °C to 150 °C for a period of about 1 hour to about 144 hours to form a well dispersed suspension of LDH particles in water.
Abstract:
Single crystal spinel boules, wafers, substrates and active devices including same are disclosed. In one embodiment, such articles reduced mechanical stress and/or strain represented by improved yield rates.
Abstract:
Methods for preparation of surfactant-free ultra-small spinel ternary metal oxide nanoparticles are provided. A method comprises dissolving first and second metal salts in deionized water in a specific mole ratio to form a solution comprising two different metal ions, applying a coprecipitation method and adding an alkaline solution to the solution to form a colloidal suspension, wherein a colloid of the colloidal suspension is a metal hydroxide, adjusting the amount and the addition rate of the alkaline solution to form a specific structure of metal hydroxide precipitate; washing and drying the metal hydroxide to form a structured metal hydroxide powder, and applying a calcination method to the structured metal hydroxide powder to form a surfactant-free spinel-type (AB 2 O 4 ) ternary metal oxide, wherein A and B each respectively comprise a metal element.
Abstract:
Die Erfindung bezieht sich auf das Gebiet der Keramik und betrifft transparente Komposit-Scheiben für Sicherheitsanwendungen, die üblicherweise aus mehreren Lagen von ggf. untereinander durch ein Verbindungsmittel verbundener Keramik-, Glas- und Kunststoff-Platten aufgebaut sind und eine erhöhte Belastbarkeit aufweisen. Die Aufgabe der Erfindung besteht in der Angabe einer transparenten Komposit- Scheibe für Sicherheitsanwendungen, welche die bisherigen Transmissions- und Qualitätsnachteile transparenter polykristalliner Keramiken ebenso vermeidet wie die Nachteile in der Schutzwirkung, wie sie Al 2 O 3 -Einkristalle im Vergleich mit feinkristallinen transparenten Al 2 O 3 - oder Spinell-Sinterkeramiken zeigen. Gelöst wird die Aufgabe durch eine transparente Komposit-Scheibe für Sicherheitsanwendungen, wobei der Komposit aus mehreren Lagen besteht, die hintereinander angeordnet sind, und mindestens eine Lage eine Platte oder mosaik- oder serienmäßig angeordnete Platten aus einkristallinem Magnesium-Aluminat-Spinell sind.
Abstract:
Die Erfindung betrifft ein optisches Element (133) zur Transmission von Strahlung bei Wellenlängen von weniger als 250 nm, insbesondere bei 193 nm, aus einem Magnesium-Aluminium-Spinell enthaltenden Material, wobei im Volumen des optischen Elements (133) das Verhältnis (V) des Aluminium-Anteils im Magnesium-Aluminium- Spinell zum Magnesium-Anteil im Magnesium-Aluminium-Spinell um weniger als 200 ppm, bevorzugt um weniger als 100 ppm, besonders bevorzugt um weniger als 50 ppm variiert und/oder im Bereich zwischen 2,0 und 2,2, bevorzugt im Bereich zwischen 2,02 und 2,10, besonders bevorzugt im Bereich zwischen 2,04 und 2,08 liegt. Die Erfindung betrifft weiterhin ein Projektionsobjektiv und eine Projektionsbelichtungsanlage mit einem solchen optischen Element, sowie ein Herstellungsverfahren für einen Rohling (1) zur Herstellung des optischen Elements (133).