PROCESS FOR THE PREPARATION OF A FIBER, A FIBER AND A YARN MADE FROM SUCH A FIBER
    8.
    发明公开
    PROCESS FOR THE PREPARATION OF A FIBER, A FIBER AND A YARN MADE FROM SUCH A FIBER 有权
    方法用于从这种纤维的纤维,纤维和纱线

    公开(公告)号:EP3011086A1

    公开(公告)日:2016-04-27

    申请号:EP14737041.5

    申请日:2014-06-20

    IPC分类号: D01F6/00 D01F6/62

    摘要: A fiber comprising polyethylene-2,5-furan-dicarboxylate, is prepared by melt spinning in a process wherein a molten composition comprising polyethylene-2,5-furan-dicarboxylate having an intrinsic viscosity of at least 0.55 dl/g, determined in dichloroacetic acid at 25° C., is passed through one or more spinning openings to yield molten threads; wherein the molten threads are cooled to below the melting temperature of the composition to yield spun fibers; and wherein the spun fibers are drawn to a linear density in the range of 0.05 to 2.0 tex per fiber. The invention also proves a fiber comprising polyethylene-2,5-furan-dicarboxylate having a linear density of 0.05 to 2.0 tex, wherein the polyethylene-2,5-furan-dicarboxylate has an intrinsic viscosity of at least 0.45 dl/g, determined in dichloroacetic acid at 25° C.

    摘要翻译: 包括聚乙烯 - 2,5-呋喃二羧酸酯的纤维,其是通过熔融纺丝的方法制备worin一个熔融的组合物,其包含具有在至少0点55分升/克的特性粘度,在确定性开采双氯聚2,5-呋喃二羧酸酯 酸在25℃下,通过一个或更多个纺纱孔传递到产生熔融的线; worin熔融线程冷却至低于该组合物,得到纺丝纤维的熔化温度; 和worin纺成纤维被吸引到在每根纤维0:05到2.0特的范围内的线性密度。 因此,本发明证明了一个纤维包括具有0:05的线密度到2.0特的聚乙烯 - 2,5-呋喃二羧酸酯,worin聚乙烯-2,5-呋喃二羧酸酯具有至少00:45分升/克的特性粘度,确定性开采 在在25℃下二氯乙酸