Fluorosilicone rubber composition
    111.
    发明公开
    Fluorosilicone rubber composition 有权
    Fluorsilikon - 古米-Zusammensetzung

    公开(公告)号:EP2883903A1

    公开(公告)日:2015-06-17

    申请号:EP14196011.2

    申请日:2014-12-03

    CPC classification number: C08K3/36 C08K5/14 C08K2201/006 C08L83/08

    Abstract: A fluorosilicone rubber composition is provided comprising (A) a fluorosilicone gum having an aliphatic unsaturated monovalent hydrocarbon group content of 0.03-1 mol% based on the total of monovalent hydrocarbon groups and a residual alkali metal content of up to 20 ppm, (B) reinforcing silica having a specific surface area of 50-100 m 2 /g, and (C) an organic peroxide catalyst. The composition is molded into silicone rubber parts which are improved in compression set even after immersion in ε-caprolactam.

    Abstract translation: 提供氟硅酮橡胶组合物,其包含(A)基于一价烃基和残余碱金属含量高达20ppm的脂族不饱和单价烃基含量为0.03-1摩尔%的氟硅酮胶,(B) 比表面积为50〜100m 2 / g的增强二氧化硅,(C)有机过氧化物催化剂。 该组合物被模塑成硅橡胶部件,即使在浸入μ-己内酰胺之后其压缩永久变形。

    RUBBER COMPOSITION FOR TIRE, VULCANIZED RUBBER COMPOSITION FOR TIRE, AND TIRES USING SAME
    113.
    发明公开
    RUBBER COMPOSITION FOR TIRE, VULCANIZED RUBBER COMPOSITION FOR TIRE, AND TIRES USING SAME 审中-公开
    橡胶组合物轮胎,硫化橡胶组合物轮胎和轮胎

    公开(公告)号:EP2803699A1

    公开(公告)日:2014-11-19

    申请号:EP13735767.9

    申请日:2013-01-10

    Abstract: An object of the present invention is to provide a rubber composition for a tire, capable of achieving both good rolling resistance properties and good wear resistance in a sufficiently compatible manner when the rubber composition is applied to a component member of a tire. Specifically, the present invention provides a rubber composition comprising a rubber composition and hydrated silica, wherein "CTAB" (m 2 /g) as specific surface area by cetyltrimethylammonium bromide adsorption and "IB" as ink bottle-shaped micropore index, of the hydrated silica, satisfy a specific relationship and "weight loss on ignition" as weight loss when the hydrate silicate is heated at 750 °C for 3 hours and "weight loss on heating" as weight loss when the hydrate silicate is heated at 105 °C for 2 hours satisfy a specific relationship.

    Abstract translation: 本发明的一个目的是提供一种用于轮胎的橡胶组合物,能够在充分地当橡胶组合物被施加到轮胎的组成构件以兼容的方式实现良好的滚动阻力性质都和良好的耐磨性的。 具体而言,本发明提供了一种橡胶组合物,包含一种橡胶组合物和水合二氧化硅,worin“CTAB”(米2 /克)由十六烷基三甲基溴吸附和“IB”作为墨瓶状细孔指数水合的,因为比表面积 二氧化硅,满足当当水合物硅酸盐在105℃下加热水合物硅酸盐在750℃下加热3小时和“加热减量”作为失重特定关系和“灼烧重量损失”作为失重 2小时满足特定的关系。

    FLUORINE RUBBER COMPOSITION
    116.
    发明公开
    FLUORINE RUBBER COMPOSITION 有权
    氟橡胶组合物

    公开(公告)号:EP2682426A1

    公开(公告)日:2014-01-08

    申请号:EP12767251.7

    申请日:2012-04-02

    Abstract: Disclosed is a fluororubber composition comprising 100 parts by weight of a peroxide-crosslinkable tetrafluoroethylene-vinylidene fluoride-hexafluoropropene ternary copolymer rubber having a fluorine content of 64 wt.% or more, (A) 5 to 90 parts by weight of carbon black having a specific surface area of 5 to 20 m 2 /g, (B) 5 to 40 parts by weight of a fine bituminous powder, (C) at least one of 1 to 30 parts by weight of hydrophilicity-imparted talc and 1 to 20 parts by weight of hydrophilicity-imparted clay, and (D) 0.5 to 6 parts by weight of an organic peroxide; the fluororubber composition being used as a molding material for fuel oil sealing materials to be in contact with fuel oil. The fluororubber composition provides a sealing materials having excellent metal corrosion resistance, without compounding an acid acceptor comprising a metal oxide.

    Abstract translation: 公开了一种氟橡胶组合物,其包含100重量份的氟含量为64重量%或更高的过氧化物可交联的四氟乙烯 - 偏二氟乙烯 - 六氟丙烯三元共聚物橡胶,(A)5至90重量份的具有 (B)5至40重量份的细沥青粉末,(C)至少一种1-30重量份的亲水性赋予的滑石和1-20重量份的比表面积 (D)0.5至6重量份的有机过氧化物; 该氟橡胶组合物用作与燃料油接触的燃料油密封材料的模塑材料。 氟橡胶组合物提供具有优异金属耐腐蚀性的密封材料,而不配合包含金属氧化物的酸受体。