GLOSSY PILLING-RESISTANT ACRYLIC FIBER, METHOD FOR PRODUCING SAME, AND SPUN YARN AND KNITTED FABRIC INCLUDING SAID ACRYLIC FIBER
    2.
    发明公开
    GLOSSY PILLING-RESISTANT ACRYLIC FIBER, METHOD FOR PRODUCING SAME, AND SPUN YARN AND KNITTED FABRIC INCLUDING SAID ACRYLIC FIBER 审中-公开
    光泽抗压腈纶纤维,其生产方法及包括所述丙烯酸纤维在内的棉纱和针织织物

    公开(公告)号:EP3187629A1

    公开(公告)日:2017-07-05

    申请号:EP15837071.8

    申请日:2015-08-25

    IPC分类号: D01F6/18

    摘要: The present invention provides: an acrylic fiber having a fineness of 0.5 to 3.5 dtex and having excellent gloss, pilling resistance, and texture; a method for producing said acrylic fiber; and a spun yarn and a knitted fabric containing said acrylic fiber. Provided is an acrylic fiber having a filament fineness of 0.5 to 3.5 dtex, wherein the product K of the value of knot strength (cN/dtex) and the value of knot elongation (%) is from 8 to 30 inclusive, and the number of recesses having a depth of 0.1 µm or greater is 10 or fewer. In this method for producing said acrylic fiber, an acrylonitrile-based copolymer containing 92 to 96.8 mass% of an acrylonitrile unit, 2 to 6 mass% of a vinyl-based monomer unit, and 0.2 to 2.0 mass% of a sulfonic acid group-containing vinyl monomer unit is dissolved in an organic solvent, to prepare a spinning dope. A coagulated fiber bundle is formed by discharging the spinning dope from discharge holes into a coagulation bath having a solvent concentration of 40 to 60 mass% and a temperature of 35 to 50 °C. The coagulated fiber bundle is drawn in hot water at a draw ratio of 2 to 3.8 times, an oil agent is applied, the fiber bundle is dried, and then the fiber bundle is drawn under dry heat at a draw ratio of 1.2 to 3 times.
    The product S of said draw ratio in hot water and said draw ratio under dry heat is from 4 to 6 times. Further, the fiber bundle is subjected to a thermal relaxation treatment.

    摘要翻译: 本发明提供:纤度为0.5〜3.5分特,且具有优异的光泽,耐起球性和质感的丙烯酸类纤维, 一种生产所述丙烯酸纤维的方法; 以及包含所述丙烯酸纤维的细纱和针织物。 本发明提供细度为0.5〜3.5分特的丙烯酸系纤维,其中,结节强度(cN / dtex)和结节伸长率(%)的值为8以上且30以下, 深度为0.1μm以上的凹部为10个以下。 在该制造上述丙烯酸系纤维的方法中,使用丙烯腈系单体92〜96.8质量%,乙烯系单体单元2〜6质量%,磺酸基单体0.2〜2.0质量% 将含乙烯基单体单元溶解在有机溶剂中,制备纺丝原液。 将纺丝原液从排出孔排出到溶剂浓度为40〜60质量%,温度为35〜50℃的凝固浴中,形成凝固纤维束。 将凝固的纤维束以2〜3.8倍的拉伸倍率在热水中拉伸,涂布油剂,将纤维束干燥后,以1.2〜3倍的拉伸倍率在干热下拉伸纤维束 。 所述热水拉伸比S和所述干热拉伸比S乘以4至6倍。 此外,纤维束经受热松弛处理。

    HOLLOW FIBER MEMBRANE AND HOLLOW FIBER MEMBRANE MODULE
    3.
    发明公开
    HOLLOW FIBER MEMBRANE AND HOLLOW FIBER MEMBRANE MODULE 审中-公开
    中空纤维膜和空心纤维膜组件

    公开(公告)号:EP3187249A1

    公开(公告)日:2017-07-05

    申请号:EP15836260.8

    申请日:2015-08-21

    摘要: The invention provides a hollow fiber membrane exhibits favorable gas permeation performance and excellent heat resistance and in which the generation of pinholes are suppressed, and a hollow fiber membrane module using the same. The hollow fiber membrane having a gas permeable nonporous layer; and a porous supporting layer to support the nonporous layer formed of a thermoplastic elastomer having a DSC melting peak temperature of 130°C or higher and a rupture elongation prescribed in ISO 37 (2010) of 300% or more. The nonporous layer is formed of a composition containing a styrene-based thermoplastic elastomer (I) containing at least either of an ABA type styrene-based thermoplastic elastomer (α) having a polystyrene portion (A) and a poly-conjugated diene portion (B) or a hydrogenated product (αh) of the ABA type styrene-based thermoplastic elastomer (α) and a polyolefin (II), wherein the poly-conjugated diene portion (B) contains at least either of a 1,2-bonding unit or a 3,4-bonding unit, wherein a total amount of the 1,2-bonding unit and the 3,4-bonding unit is 50% by mole or more with respect to a total amount of the entire units constituting the poly-conjugated diene portion (B).

    摘要翻译: 本发明提供一种中空纤维膜和具有该中空纤维膜膜的中空纤维膜组件,该中空纤维膜呈现良好的气体渗透性能和优异的耐热性,并且其中抑制了针孔的产生。 该中空纤维膜具有气体可渗透的无孔层; 以及多孔性支撑层,用于支撑由DSC熔融峰值温度为130℃以上且ISO37(2010)中规定的断裂伸长率为300%以上的热塑性弹性体形成的无孔层。 无孔层由含有苯乙烯系热塑性弹性体(I)的组合物形成,所述苯乙烯系热塑性弹性体(I)含有具有聚苯乙烯部分(A)和聚共轭二烯部分(B)的ABA型苯乙烯系热塑性弹性体(α) )或ABA型苯乙烯类热塑性弹性体(α)和聚烯烃(II)的氢化物(αh),其中,聚共轭二烯部分(B)含有1,2-键合单元或 3,4-键合单元,其中1,2-键合单元和3,4-键合单元的总量相对于构成聚共轭物的全部单元的总量为50摩尔%以上 二烯部分(B)。

    ACRYLIC FIBERS, METHOD FOR MANUFACTURING SAME, AND SPUN YARN AND KNITTED FABRIC USING SAID FIBERS
    6.
    发明公开
    ACRYLIC FIBERS, METHOD FOR MANUFACTURING SAME, AND SPUN YARN AND KNITTED FABRIC USING SAID FIBERS 审中-公开
    丙烯酸纤维,其制造方法及纺纱和针织面料所述纤维

    公开(公告)号:EP3138940A1

    公开(公告)日:2017-03-08

    申请号:EP15786320.0

    申请日:2015-04-28

    IPC分类号: D01F8/08 D02J1/22

    摘要: Provided are: acrylic fibers having 2-7% boiling water shrinkage and formed by the side-by-side conjugation of a copolymer A, which contains 5-10 mass% of an unsaturated monomer that can form a copolymer with acrylonitrile units, and a copolymer B, which contains 2-5 mass% of unsaturated monomer units that can form a copolymer with acrylonitrile units and 0.2-1.5 mass% of sulfonic acid group-containing monomer units; a method for manufacturing said fibers; a spun yarn containing said fibers; and a knitted fabric obtained from said spun yarn. The single fiber fineness of the heat-treated acrylic fibers is 1.7-6.6 dtex, the bulkiness is at least 380 cm3/g, the percentage of crimp is at least 15%, and the product (DKSDKE) of the knot strength (cN/dtex) and the knot elongation (%) is 10-25. The acrylic fibers have excellent crimp characteristics and anti-pilling properties.

    摘要翻译: 本发明提供:具有2-7%的沸水收缩率的丙烯酸纤维和由侧由端缀合的共聚物A的,其中含有5-10%的不饱和单体的质量也可以形成与丙烯腈单元的共聚物形成,并且 共聚物B,其含有2-5%的不饱和单体单元的质量也可形成具有丙烯腈单元和含磺酸基的单体单元的0.2-1.5质量%的共聚物; 用于制造所述纤维的方法; 细纱含有所述纤维; 和从所述获得的针织物细纱。 经热处理的丙烯酸类纤维的单纤维纤度是分特1.7-6.6,膨松度是至少380立方厘米/ g时,卷曲的百分比是至少15%,该产品的结节强度(DKSDKE)(CN / 分特)和结节伸长(%)为10-25。 所述丙烯酸类纤维具有优异的卷曲特性和抗起球性能。

    ACRYLIC RESIN COMPOSITION, METHOD FOR PRODUCING SAME, AND ACRYLIC RESIN FILM
    7.
    发明公开
    ACRYLIC RESIN COMPOSITION, METHOD FOR PRODUCING SAME, AND ACRYLIC RESIN FILM 审中-公开
    丙烯酸树脂组合物,其制备方法和丙烯酸树脂膜

    公开(公告)号:EP3135725A1

    公开(公告)日:2017-03-01

    申请号:EP15761765.5

    申请日:2015-03-10

    发明人: ABE, Junichi

    摘要: The purpose of the present invention is to provide an acrylic resin composition that is a raw material for an acrylic resin film which has an excellent appearance and in which occurrence of blocking is suppressed. The present invention is an acrylic resin composition that comprising an acrylic polymer (A), an anti-blocking agent (B), and a non-crosslinked acrylic polymer (C). The non-crosslinked acrylic polymer (C) is a polymer of a monomer component including 50% to 100% by mass of methyl methacrylate (c1), the polymer having a reduced viscosity of 0.2 to 2 L/g.

    摘要翻译: 本发明的目的在于提供一种丙烯酸类树脂组合物,该丙烯酸类树脂组合物是具有优异外观并且抑制了发生粘连的丙烯酸树脂膜的原料。 本发明是包含丙烯酸类聚合物(A),防粘连剂(B)和非交联型丙烯酸类聚合物(C)的丙烯酸类树脂组合物。 非交联型丙烯酸类聚合物(C)是含有50〜100质量%的甲基丙烯酸甲酯(c1),比浓粘度为0.2〜2L / g的单体成分的聚合物。

    RESIN COMPOSITION AND MOLDED BODY FORMED FROM RESIN COMPOSITION
    10.
    发明公开
    RESIN COMPOSITION AND MOLDED BODY FORMED FROM RESIN COMPOSITION 审中-公开
    HARZZUSAMMENSETZUNG UNDFORMKÖRPERAUS DER HARZZUSAMMENSETZUNG

    公开(公告)号:EP3124547A1

    公开(公告)日:2017-02-01

    申请号:EP15770052.7

    申请日:2015-03-18

    摘要: A resin composition which contains from 5% by mass to 65% by mass (inclusive) of a polymer (X) described below and from 35% by mass to 95% by mass (inclusive) of a polymer (Y) described below. Alternatively, a resin composition which contains more than 65% by mass but 85% by mass or less of a polymer (X) described below and 15% by mass or more but less than 35% by mass of a polymer (Y) described below, wherein a domain (y1) described below or a domain (y2) described below comprises a macromonomer unit. Polymer (X): a vinylidene fluoride resin Polymer (Y): a copolymer having a domain (y1) that is compatible with the polymer (X) and a domain (y2) that is incompatible with the polymer (X)

    摘要翻译: 含有下述聚合物(X)5质量%〜65质量%(以下)和下述35质量%〜95质量%(以下)的聚合物(Y)的树脂组合物。 或者,含有下述聚合物(X)的含量超过65质量%但为85质量%以下且15质量%以上且小于35质量%的下述聚合物(Y)的树脂组合物 其中下述的域(y1)或下述的域(y2)包含大分子单体。 聚合物(X):偏二氟乙烯树脂聚合物(Y):具有与聚合物(X)相容的结构域(y1)和与聚合物(X)不相容的结构域(y2)的共聚物