Compressor coating
    4.
    发明公开
    Compressor coating 有权
    Verdichterbeschichtung

    公开(公告)号:EP1281863A3

    公开(公告)日:2004-01-28

    申请号:EP02017303.5

    申请日:2002-08-01

    IPC分类号: F04B27/08 F04B27/10

    摘要: A swash plate (10) is operably connected through a lug plate (11) and a hinge mechanism (12) to a drive shaft (9), and slidably retained on an end part of each piston (8). through a pair of front and rear shoes (15a, 15b). A rotational motion of the swash plate (10) following rotation of the drive shaft (9) is converted through the shoes (15a, 15b) into a reciprocating motion of each piston (8). A thermoplastic polyimide coating (17) is formed on the swash plate (10) and the shoes (15a, 15b) as sliding components of a compressor (C). The thermoplastic polyimide coating (17) may contain a solid lubricant. For the solid lubricant, for example, polytetrafluoroethylene is used. Thus, it is possible to obtain a compressor, which includes the sliding components having improved sliding characteristics, and is manufactured relatively easily.

    Compressor
    6.
    发明公开
    Compressor 有权
    压缩机

    公开(公告)号:EP1647670A1

    公开(公告)日:2006-04-19

    申请号:EP05025453.1

    申请日:2004-06-17

    IPC分类号: F01B3/00 F04B27/10

    摘要: A compressor has a swash plate and shoes. Surfaces of the swash plate slides on flat surfaces of the shoes. A sliding film is formed on each of the swash plate surfaces. The sliding films are formed of a polyamide-imide resin that contains at least solid lubricant. The polyamide-amide resin has a tensile strength at room temperature of 200 MPa. The isocyanate component, which is a crude material of the polyamide-imide resin, contains 5 % to 90 % by mol of 3,3'-dimethylbiphenyl-4,4'-diisocyanate. The number average molecular weight of the polyamide-imide resin is no less than 20,000. When a base portion of the swash plate is made of an aluminum-based metal, the sliding films are formed on the base portion with middle layers made of anodized aluminium in between.

    摘要翻译: 压缩机有一个斜盘和鞋子。 斜盘的表面在鞋的平坦表面上滑动。 滑动膜形成在每个斜盘表面上。 滑动膜由至少含有固体润滑剂的聚酰胺酰亚胺树脂形成。 聚酰胺酰胺树脂在室温下的拉伸强度为200MPa。 作为聚酰胺酰亚胺树脂的原料的异氰酸酯成分含有5摩尔%〜90摩尔%的3,3'-二甲基联苯-4,4'-二异氰酸酯。 聚酰胺酰亚胺树脂的数均分子量不小于20,000。 当斜盘的基座部分由铝基金属制成时,滑动膜在基座部分上形成,其间具有由阳极氧化铝制成的中间层。