摘要:
The invention relates to a particulate powder, said powder having a median circularity of greater than 0.87 wt % and less than 9.0 wt % of particles having a size greater than 100 μm. The powder and at least 80 wt % of the particles have a chemical composition such that, in wt % on the basis of the oxides and for a total of 100%: Cr 2 O 3 + Al 2 O 3 + ZrO 2 + MgO + Fe 2 O 3 + SiO 2 + TiO 2 ≥ 90%; Cr 2 O 3 + Al 2 O 3 + MgO ≥ 60%; Cr 2 O 3 ≥ 9%; 20% ≥ SiO 2 ≥ 0,5%; and other oxides: ≤ 10%. The invention can be used for a glass furnace.
摘要:
Process for manufacturing a product, comprising the following successive steps: a) mixing raw materials to form a starting feedstock, b) melting the starting feedstock so as to form a molten liquid, c) solidifying the molten liquid so as to obtain a fused product comprising crystals linked by a glassy phase, and d) crystallization heat treatment of the glassy phase of said fused product, in which the composition of the starting feedstock is adapted in order to manufacture a product having the following chemical composition, as weight percentages based on the oxides, and for a total of 100%: 40% ≤ (ZrO 2 + HfO 2 ) ≤ 94%, 6% 2 2 O 3 , 0% ≤ Al 2 O 3 , 2% ≤ SiO 2 , 0% ≤ MgO, 0% ≤ TiO 2 , and other oxides ≤ 1%. Use of the product obtained as a grinding agent, an agent for dispersing in a wet medium, a surface treatment agent, a supporting agent or a heat-exchange agent.
摘要:
The invention relates to a device selected from among a glass furnace and a channel for dispensing the glass comprising a block and/or a coating made of a sintered material obtained by sintering a particular mixture comprising a chromium oxide content, indicated as "Cr T ", of between 10% and 82%. The die fraction is such that 0.39.(Cr T )+24 M T )+52, Cr M denoting the chromium oxide content by weight of the die fraction in wt % on the basis of the oxides of the die, and the aggregate is such that x II ≥ 97%, x III ≥ 70%, and x IV ≤ x III - 70%, Cr G denoting the chromium oxide content by weight of one grain in wt % on the basis of the oxides of said grain. x II denotes the amount, in wt % on the basis of the aggregate, of grains having the following conditions (II): if 10% ≤ Cr T ≤ 30%, then Cr G ≤ 0.018.(Cr T ) 2 - 0.390.(Cr T )+58.8; if 30% ≤ Cr T ≤ 60%, then Cr G ≤ 1.22.( Cr T )+26.7; and if 60% T ≤ 82%, then Cr G ≤ 100. X III denotes the amount, in wt % on the basis of the aggregate, of grains having the following conditions (III): if 10% ≤ Cr T ≤ 30%, then 0.018.(Cr T ) 2 - 0.390.(Cr T )+9.10 ≤ Cr G ≤ 0.18.(Cr T ) 2 - 0.390.(Cr T )+25.10; if 30% T ≤ 60%, then 1.17.(Cr T ) - 21.5 ≤ Cr G ≤ 1.17. (Cr T ) - 5.5; and if 60% T ≤ 82%, then 1.17.(Cr T ) - 21.5 ≤ Cr G ≤ 1.67. (Cr T ) - 35.5. x IV denotes the amount, in wt % on the basis of the aggregate, of grains having the following conditions (IV): if 10% ≤ Cr T ≤ 30%, then 0.018.(Cr T ) 2 - 0.390.(Cr T )+9.10 > Cr G ; if 30% T ≤ 60%, then 1.17.(Cr T ) - 21.5 > Cr G ; and if 60% T ≤ 82%, then 1.17.(Cr T ) - 21.5 > Cr G . The invention can be used for a glass furnace.
摘要翻译:本发明涉及一种颗粒粉末,所述粉末具有大于0.87重量%且小于9.0重量%的具有大于100μm尺寸的颗粒的中值圆形度。 该粉末和至少80重量%的颗粒具有以氧化物计的重量%的化学组成,总计为100%:Cr 2 O 3 + Al 2 O 3 + ZrO 2 + MgO + Fe 2 O 3 + SiO 2 + TiO 2≥90%。 的Cr2O3 +氧化铝+ MgO的≧60%; 的Cr2O3≧9%; 20%的SiO 2≧≧0.5%; 和其他氧化物:≦̸ 10%。 本发明可用于玻璃熔炉。
摘要:
The invention relates to a sintered particle having a chemical analysis, in weight percent, of: ZrO 2 partially stabilized with CeO 2 and Y 2 O 3 : the remainder up to 100%; Al 2 O 3 : 10-60%; additive selected from CaO, a manganese oxide, La 2 O 3 , SrO, BaO, and the mixtures thereof: 0.2-6%, the CaO content being lower than 2%; impurities: 2 and Y 2 O 3 , present with a molar content in molar percent on the basis of the sum of ZrO 2 , CeO 2 and Y 2 O 3 , of: CeO 2 : 6-11 mol %; and Y 2 O 3 : 0.5-2 mol %, the particle being produced by sintering at a sintering temperature higher than 1300°C, the sintering temperature being lower than 1400°C if the additive is CaO or if the CeO 2 molar content is between 10 and 11%.