摘要:
The invention relates to a process and apparatus for blending immiscible polymers, whereby at least two extruders screws, each comprise at least one melting zone and three to eight mixing zones, whereby the melting zone is a first mixing zone, whereby further the length of at least one mixing zone is between 4 and 15 times the diameter of the screw and the length of each of the other mixing zones is between 1 and 10 times the diameter of the screw, whereby further the combined length of the mixing zones of the screw is between 15 and 37 % of the length of the screw.
摘要:
The present invention relates to a process for the manufacturing of composite materials from natural fibers and thermoplastic polymers. Examples of fibers are wood fibers originating from pulping processes known as refiner pulp (RMP), thermomechanical pulp (TMP) or chemi-thermomechanical pulp (CTMP), but the process can also be applied to other kinds of natural fiber containing raw materials. In the process according to the present invention, fibers are introduced from the blowline or the housing of a refiner into a flash tube dryer, separated from humid air in a cyclone, introduced into a compounder and mixed with at least one thermoplastic polymer and the product is subsequently pelletized. The process according to the present invention is advantageously run as a continuous process.
摘要:
A first mask layer (13) and a second mask layer (12) are transferred and imparted to a target object (20) using a fine-pattern-forming film (I) provided with a cover film (10) having a nanoscale concavo-convex structure (11) formed on one surface thereof, a second mask layer (12) provided in a recess of the concavo-convex structure (11), and a first mask layer (13) provided so as to cover the concavo-convex structure (11) and the second mask layer (12). A surface of a fine-pattern-forming film (II) to which the first mask layer (13) is provided is pressed toward a surface of the target object (20), energy rays are irradiated to the first mask layer (13), and the cover film (10) is then separated from the second mask layer (12) and the first mask layer (13). Pressing and energy ray irradiation are each performed independently. The target object is etched using the second mask layer (12) and the first mask layer (13).
摘要:
An ophthalmic lens operable to protect the eye from harmful ultraviolet and high energy visible wavelengths of light and methods for producing the same.
摘要:
There is provided a resin composition for a modeling material 4a, used for shaping a modeling material 4 by a manufacturing method for light curing molding using an ink-jet scheme, comprising (A) an ethylenic unsaturated monomer as a photocuring component, (B) a photopolymerization initiator, and (C) a surface adjusting agent, wherein the resin composition for a modeling material has surface tension Mt of 26.0 to 33.0 mN/m, and the resin composition for a modeling material has surface tension Mst represented by the following (i) expression of 33.0 mN/m or more, and this resin composition for a modeling material 4a can afford a light cured article having the good dimensional accuracy.
摘要:
A functional polymeric cutting edge structure and methods for the manufacturing cutting edge structures using polymeric materials are provided. A razor blade for use in a razor cartridge or a blade box for assembly in a razor cartridge frame may be formed using the present invention.
摘要:
A method of blow molding a glossy article having at least one layer of thermoplastic material. The method comprises the steps of feeding a parison of said thermoplastic material into a mold having an inner surface with at least a portion of SPI finish standard selected from the group consisting of A-1, A-2, A-3, B-1, B-2 and B-3 mold and a first temperature of greater than 55° C.; blowing the parison against the inner surface of the mold to form the article; and subsequently lowering the temperature of the mold to a second temperature of between 10° C. to 55° C. before release of the molded article. The cycle time of the mold (tct) is less than 250 seconds.
摘要:
The present disclosure provides a process of preparing linear polypropylene foam, comprising the following steps: (a) preparing a specimen comprising at least one linear polypropylene; and at least one nucleating agent selected from the group consisting of alpha nucleating agents and beta nucleating agents; (b) deforming the specimen under a deforming pressure and at a deforming temperature for a period of time; and (c) subjecting the deformed specimen obtained in the step (b) to a foaming process to obtain the linear polypropylene foam. The present disclosure further provides a specimen after PIF treatment and a linear polypropylene foam prepared by the above process.