摘要:
Polyparaxylylene (PPX) polymers that can be expanded into porous articles that have a node and fibril microstructure are provided. The fibrils contain PPX polymer chains oriented with the fibril axis. The PPX polymer may contain one or more comonomer. PPX polymer articles may be formed by applying PPX to a substrate by vapor deposition. The nominal thickness of the PPX polymer film is less than about 50 microns. The PPX polymer film may be removed from the substrate to form a free-standing PPX polymer film, which may then be stretched into a porous article. Alternatively, a PPX polymer article can be formed by lubricating PPX polymer powder, heating the lubricated powder, and calendering or ram extruding to produce a preform that can subsequently be stretched into a porous article. The heating and expansion temperatures are from about 80°C to about 220°C or from about 220°C to about 290°C or from about 290°C to about 450°C.
摘要:
A composition which can be used as an organic water/oxygen barrier material, an OLED display device and manufacturing method thereof are disclosed. The composition includes: 15-25 wt % of parylene, 15-25 wt % of polyvinyl chloride, 5-15 wt % of acetone, 5-15 wt % of trichloroethylene, 10-20 wt % of polyvinyl acetate, 5-15 wt % of polyvinyl alcohol, 0-5 wt % of SiO2 nanoparticles, and 8-12 wt % of an organic solvent, wherein all weight percent values are based on the total weight of the composition. When a water/oxygen barrier layer fabricated by the composition is disposed between a luminescent layer of OLED and a light extraction layer, water vapor and oxygen gas can be prevented from entering the OLED luminescent layer, thereby prolonging the service life of the OLED luminescent layer.
摘要:
Polyparaxylylene (PPX) polymers that can be expanded into porous articles that have a node and fibril microstructure are provided. The fibrils contain PPX polymer chains oriented with the fibril axis. The PPX polymer may contain one or more comonomer. PPX polymer articles may be formed by applying PPX to a substrate by vapor deposition. The nominal thickness of the PPX polymer film is less than about 50 microns. The PPX polymer film may be removed from the substrate to form a free-standing PPX polymer film, which may then be stretched into a porous article. Alternatively, a PPX polymer article can be formed by lubricating PPX polymer powder, heating the lubricated powder, and calendering or ram extruding to produce a preform that can subsequently be stretched into a porous article. The heating and expansion temperatures are from about 80°C to about 220°C or from about 220°C to about 290°C or from about 290°C to about 450°C.
摘要:
The present disclosure relates, in part, to Parylene based conformal coating compositions having improved properties, e.g., improved heat transfer and durability characteristics, as well as a methods and apparatus to coat objects with these compositions, and objects coated with these compositions. In some aspects, coating compositions comprising Parylene and boron nitride are disclosed. The disclosure also includes objects (e.g., electronic equipment, textiles, etc.) having a conformal coating comprising a Parylene compound and boron nitride.
摘要:
There is described a reservoir means which means is provided with a moisture resistant coating, the reservoir means is especially adapted to contain a medicament. There is also described a medicament delivery device which comprises a medicament reservoir, a medicament delivery passage and a metering member characterised in that the device includes a surface or surfaces provided with a moisture resistant coating. The device is especially an inhaler, e.g. a dry powder inhaler. A method of treating a respiratory disorder is also described which comprises administering of a therapeutically effective amount of a pharmaceutically active agent to a patient suffering from such a disorder.
摘要:
Polyparaxylylene (PPX) polymer films that can be expanded into porous articles that have a node and fibril microstructure are provided. The fibrils contain PPX polymer chains oriented with the fibril axis. The PPX polymer may contain one or more comonomer. PPX polymer articles may be formed by applying PPX to one or both sides of a substrate, such as by vapor deposition. The nominal thickness of the PPX polymer film(s) is less than about 50 microns. The PPX polymer film(s) may be removed from the substrate to form a free-standing PPX polymer film(s), which may then be stretched into a porous article.
摘要:
A method of sealing pores of an oxidation layer of a work-piece that includes the porous oxidation layer disposed on a substrate. The method includes impregnating the pores with a polymerizable gas and polymerizing the gas. In some embodiments, the gas is derived from a paracyclophane, typically heated at low pressure.