SELF-ETCHING CEMENTITIOUS SUBSTRATE COATING COMPOSITION

    公开(公告)号:EP4074680A1

    公开(公告)日:2022-10-19

    申请号:EP21168884.1

    申请日:2021-04-16

    Abstract: Described is a method for producing a coating with an aqueous coating composition AC, the method comprising the following steps: a) applying the aqueous coating composition AC to a cementitious substrate; b) curing the applied aqueous coating composition AC; wherein the aqueous coating composition AC comprises at least one amino-functional vinyl copolymer VC and at least one epoxy silane ES and the coating composition has a pH of 3 - 6.5 and the weight ratio between amino-functional vinyl copolymer VC and epoxy silane ES (VC/ES) is from 1.0 - 9.5. Since the composition displays self-etching properties on concrete surfaces, cementitious substrates do not have to be mechanically or chemically pretreated before the composition is applied.

    Building board and method for producing building board
    9.
    发明公开
    Building board and method for producing building board 审中-公开
    建筑板材和生产建筑板材的方法

    公开(公告)号:EP2781495A2

    公开(公告)日:2014-09-24

    申请号:EP13195252.5

    申请日:2013-12-02

    Abstract: A building board includes an inorganic board having a surface covered by an insulating coating film containing a coating film forming material and organic hollow particles, wherein the organic hollow particles have an average particle size in the range of 5 to 50 µm and an average hollow ratio of 80% or more, and the insulating coating film contains 0.01 to 5.0 parts by mass of the organic hollow particles per 100 parts by mass of solid content thereof, and has an average thickness of 5 to 500 µm. The method for producing a building board includes: applying, onto a surface of an inorganic board, an insulating coating material containing a coating film forming material and organic hollow particles; and drying the insulating coating material to form an insulating coating film.

    Abstract translation: 建筑板材包括具有被包含涂膜形成材料的绝缘涂膜和有机中空粒子覆盖的表面的无机板,其中有机中空粒子的平均粒径为5〜50μm,平均中空率 为80%以上,并且绝缘涂膜包含每100质量份固体含量为0.01至5.0质量份有机中空颗粒,并具有5​​至500μm的平均厚度。 制造建筑板的方法包括:将包含涂膜形成材料和有机中空颗粒的绝缘涂层材料涂覆到无机板的表面上; 并干燥绝缘涂层材料以形成绝缘涂层膜。

Patent Agency Ranking