公开(公告)号:JP2008007676A
公开(公告)日:2008-01-17
申请号:JP2006180951
申请日:2006-06-30
Applicant: Polyplastics Co , ポリプラスチックス株式会社
Inventor: HASE HIROYUKI
IPC: C08L59/04 , C08K5/13 , C08K5/20 , C08K5/24 , C08K5/3432 , C08K5/3475 , C08K5/3477
CPC classification number: C08K5/005 , C08K2201/014 , C08L59/00
Abstract: PROBLEM TO BE SOLVED: To provide a polyacetal resin composition which has excellent processability and stability and is excellent in weather (light) resistance, from whose molded articles the generation of formaldehyde is remarkably reduced, and from which the oozing of compounded components is prevented. SOLUTION: This polyacetal resin composition comprises (A) a polyacetal copolymer having a hemiformal terminal group content of ≤1.0 mmol/kg, a formyl terminal group content of ≤2.0 mmol/kg, and an unstable terminal group content of ≤0.5 wt.%, (B) a hindered phenolic antioxidant, (C) at least one compound selected from a guanamine compound (c-1) and a hydrazide compound (c-2), (D) a hindered amine stabilizer wherein the nitrogen of the piperidine derivative having a sterically hindered group is tertiary, and (E) a UV light absorbent, in specific compounding amounts and in a specific compounding ratio. COPYRIGHT: (C)2008,JPO&INPIT
Abstract translation: 解决问题的方案为了提供加工性和稳定性优异且耐候性(耐光性优异)的聚缩醛树脂组合物,其模塑制品中甲醛的产生明显降低,并且复合组分的渗出 被阻止 解决方案:该聚缩醛树脂组合物包含(A)半缩醛末端基含量≤1.0mmol/ kg,甲酰基末端基含量≤2.0mmol/ kg,不稳定末端基含量≤0.5的聚缩醛共聚物 (C)至少一种选自胍胺化合物(c-1)和酰肼化合物(c-2)的化合物,(D)受阻胺稳定剂,其中氮 具有空间位阻基团的哌啶衍生物为叔,和(E)紫外线吸收剂,具体配合量和特定配混比。 版权所有(C)2008,JPO&INPIT
-
公开(公告)号:JP3987068B2
公开(公告)日:2007-10-03
申请号:JP2004508167
申请日:2003-05-20
Inventor: ファルーン,スティーヴン・ビー , フィリップス,マシュー・ディー , ローズ,リチャード・エス
IPC: C08L75/04 , C08G18/00 , C08G18/48 , C08G101/00 , C08K5/49 , C08K5/523 , C08K5/5313
CPC classification number: C08G18/48 , C08G2101/0008 , C08G2101/005 , C08G2101/0083 , C08K5/49 , C08K2201/014 , C08L75/04
-
93.
公开(公告)号:JP2007512409A
公开(公告)日:2007-05-17
申请号:JP2006541105
申请日:2004-11-25
Applicant: デュスロ エイエス
Inventor: ヴィエラ アンドルスコヴァ , ヤン ウーラル , ヤロスラフ ホラク , ペーター レホッキー
IPC: C09K15/18 , C07B61/00 , C07C209/60 , C07C211/55 , C08K5/00 , C08K5/18 , C08L101/00
CPC classification number: C08K5/18 , C08K2201/014
Abstract: 65〜98質量%のジオクチルジフェニルアミン、29質量%以下のモノオクチルジフェニルアミン、5質量%以下のオクチルブチルジフェニルアミン、1.5質量%以下のトリオクチルジフェニルアミン及び1質量%以下のジフェニルアミンを含むオクチル化ジフェニルアミンの抗酸化組成物を、酸性触媒の存在下、ジイソブチレンによるジフェニルアミンのアルキル化によって調製する。 それらは、単独で又は抗分解系及びそれに基づく物質の成分としてポリマー材料、潤滑剤及び油の有効な安定剤として使用され得る。
-
公开(公告)号:JP2006510919A
公开(公告)日:2006-03-30
申请号:JP2005502422
申请日:2003-12-04
Applicant: ランクセス・ドイチユラント・ゲゼルシヤフト・ミツト・ベシユレンクテル・ハフツング
Inventor: カピタノブ,コンスタンテイン・アウトノモビチ , キルシユ,ユルゲン , ゴトシヤルク,ペーター−アレクサンダー , コプ,リヒヤルト , コルシユノブ,アレクサンダー・イワノビチ , サブキン,ジエナデイ・グリゴリービチ , ツアンダー,クラウス , ナサロバ,エレナ・サベリーブナ , ニキテイン,ウラジミル・ミハイロビチ , プドライナー,ハインツ , ベルデン,ブルクハルト , マダー,クラウス , ユンゲルマン,ハルデイ , ヨアヒミ,デトレフ , ライツ,エドガー , リシヤコブ,イゴル・レオニドビチ
CPC classification number: G21F1/10 , C08K3/08 , C08K2201/014 , G21Y2002/201 , G21Y2004/10
Abstract: 本発明は、a)ガドリニウムを少なくとも26重量%およびb)バリウム、インジウム、錫、ランタン、モリブデン、ニオブ、タンタル、ジルコニウムおよびタングステンを包含する群の1種以上の元素、合金および/または化合物を含有する混合物に関する。 本発明は、また、前記混合物の製造方法、前記混合物を放射線を遮蔽する目的および放射線を遮蔽する重合体材料を製造する目的で用いること、放射線を遮蔽するゴム、熱可塑性プラスチックおよびポリウレタンを製造する方法、放射線を遮蔽する重合体材料で構成させた製品に加えて前記材料で構成させた製品を製造する方法にも関する。
-
公开(公告)号:JP2006508228A
公开(公告)日:2006-03-09
申请号:JP2004556938
申请日:2003-04-14
Applicant: ジンウック ハ , ユジンテックトゥウェンティワン カンパニー リミテッド
IPC: C09D133/00 , C08K3/00 , C08K3/22 , C08K3/38 , C09D5/18 , C09D7/12 , C09D133/06 , C09D163/00 , C09D167/08 , C09D175/04 , H01B7/295
CPC classification number: H01B7/295 , C08K3/016 , C08K3/22 , C08K3/38 , C08K2201/014 , C09D5/18 , C08L33/06 , C08L75/04
Abstract: 全体コーティング組成物に対して、10〜50重量%の水溶性樹脂、アクリル系樹脂またはウレタン系樹脂、10〜30重量%の難燃剤、8〜20重量%の難燃補助剤、30〜45重量%の希釈剤、および0.1〜0.5重量%の添加剤を含む、難燃性コーティング組成物を開示する。 本発明によると、火災の発生時、コーティング層に含有された不燃性材料により燃焼が遅延されるだけでなく、有害ガスの発生が最小化されるので、火災を初期に鎮圧し得る時間を確保することができ、人名被害を最小化することができる。
-
公开(公告)号:JP2006057091A
公开(公告)日:2006-03-02
申请号:JP2005235928
申请日:2005-08-16
Applicant: Clariant Gmbh , クラリアント・ゲゼルシヤフト・ミト・ベシユレンクテル・ハフツング
Inventor: THEWES VOLKER , HENNEMANN ACHIM
IPC: C09D201/00 , C09D5/18 , C09D7/12 , C09D163/00 , C09K21/04 , C09K21/12 , C09K21/14
CPC classification number: C08K5/0066 , C08K5/5313 , C08K2201/014 , C09D5/185
Abstract: PROBLEM TO BE SOLVED: To provide a fire-resisting coating capable of forming a heat insulating layer, based on substances each changed into a foam layer and carbonized, in case of a fire, and a film-forming binder, a blowing agent, a commonly-used auxiliary agent, and an additive.
SOLUTION: This fire-resisting coating forms the heat insulating layer, wherein the fire-resisting coating contains a flame retardant mixture containing a phosphorus-based/nitrogen-based flame retardant, and a phosphinic acid salt expressed by general formula (I) (R
1 and R
2 are identical to or different from each other and are each a 1-6C linear or branched alkyl or an aryl; M is Mg, Ca, Al, Sb, Sn, Ge, Ti, Zn, Fe, Zr, Ce, Bi, Sr, Mn, Li, Na, K or a protonated nitrogen base; and m is 1 to 4) and/or a diphosphinic acid salt expressed by general formula (II) (R
3 is a 1-10C linear or branched alkylene, a 6-10C arylene, a 6-10C alkylarylene or a 6-10C arylalkylenene; n is 1 to 4; and x is 1 to 4) and/or a polymer thereof.
COPYRIGHT: (C)2006,JPO&NCIPIAbstract translation: 要解决的问题:为了提供能够形成绝热层的耐火涂层,其基于在发生火灾的情况下变成泡沫层并碳化的物质和成膜粘合剂,吹塑 助剂,常用助剂和添加剂。 该耐火涂层形成绝热层,其中耐火涂层含有含有磷系/氮系阻燃剂的阻燃剂混合物和由通式(I)表示的次膦酸盐 )(R
1 SP>和R 2 SP>彼此相同或不同,分别为1-6C直链或支链烷基或芳基; M为Mg,Ca, Al,Sb,Sn,Ge,Ti,Zn,Fe,Zr,Ce,Bi,Sr,Mn,Li,Na,K或质子化氮碱; m为1〜4)和/或二膦酸盐 通式(II)(R 3)是1-10C直链或支链亚烷基,6-10C亚芳基,6-10C烷基亚芳基或6-10C芳基亚烷基烯; n为1至4; 和x为1至4)和/或其聚合物。 版权所有(C)2006,JPO&NCIPI -
公开(公告)号:JP2005344113A
公开(公告)日:2005-12-15
申请号:JP2005161631
申请日:2005-06-01
Applicant: Clariant Gmbh , クラリアント・ゲゼルシヤフト・ミト・ベシユレンクテル・ハフツング
Inventor: BAUER HARALD , HOEROLD SEBASTIAN , NASS BERND , SICKEN MARTIN
IPC: C09K21/12 , C07F9/30 , C08K5/00 , C08K5/53 , C08K5/5313 , C08K5/5377 , C08L21/00 , C08L101/00 , C09K21/02 , C09K21/04 , C09K21/06 , C09K21/08 , C09K21/10 , C09K21/14 , D01F1/10 , D01F6/90 , D01F6/92
CPC classification number: C08K5/5313 , C08K2201/014 , C08L21/00
Abstract: PROBLEM TO BE SOLVED: To provide a pressing granulated fire retardant composition having a heightened phosphorus content. SOLUTION: The pressing granulated fire retardant composition contains a phosphinic acid salt represented by formula (1) and/or a diphosphinic acid salt represented by formula (2) and/or a polymer thereof, and a fusible zinc phosphinate. (In the formulas, R 1 and R 2 are the same or different, and each a linear or branched 1-6C alkyl or an aryl; R 3 is a linear or branched 1-10C alkylene, a 6-10C arylene, a 6-10C alkylarylene or a 6-10C arylalkylene; M is Mg, Ca, Al, Sb, Sn, Ge, Ti, Fe, Zr, Ce, Bi, Sr, Mn, Li, Na, K and/or a protonated nitrogen base; m is 1-4; n is 1-4; and x is 1-4). The method for producing the pressing granulated fire retardant, and the method for using the composition are also provided. COPYRIGHT: (C)2006,JPO&NCIPI
Abstract translation: 待解决的问题:提供具有提高的磷含量的压制颗粒状阻燃剂组合物。 压制颗粒状阻燃组合物含有式(1)表示的次膦酸盐和/或式(2)表示的二次膦酸盐和/或其聚合物和可熔融次膦酸锌。 (式中,R 1和R 2相同或不同,并且各自为直链或支链的1-6C烷基或芳基; R
3 SP> / SP>是直链或支链1-10C亚烷基,6-10C亚芳基,6-10C烷基亚芳基或6-10C芳基亚烷基; M是Mg,Ca,Al,Sb,Sn,Ge,Ti,Fe,Zr ,Ce,Bi,Sr,Mn,Li,Na,K和/或质子化氮碱; m为1-4; n为1-4; x为1-4)。 还提供了压制粒状阻燃剂的制造方法以及使用该组合物的方法。 版权所有(C)2006,JPO&NCIPI -
98.
-
公开(公告)号:JPWO2003035749A1
公开(公告)日:2005-02-10
申请号:JP2003538259
申请日:2002-09-04
Applicant: 第一工業製薬株式会社
CPC classification number: C08K5/03 , C08K3/2279 , C08K2201/014 , C08L25/02
Abstract: 本発明は、スチレン系樹脂(A)中に分散された、(B)すべての臭素原子が芳香環へ結合している融点200℃ないし260℃の含臭素芳香環化合物、(C)2,3−ジブロモプロピル基を有する含臭素有機化合物、および任意に(D)三酸化アンチモンを含んでいる難燃性スチレン系樹脂組成物に関する。
-
公开(公告)号:JP2004537629A
公开(公告)日:2004-12-16
申请号:JP2003519151
申请日:2002-08-07
Applicant: ヘンケル コーポレイションHenkel Corporation
Inventor: アンソニー エイ. ガロー、
IPC: C08J5/00 , C08G59/62 , C08K3/18 , C08K3/22 , C08K3/24 , C08K3/36 , C08K5/49 , C08L25/04 , C08L63/00 , C09K21/02 , H01B3/40 , H01L21/56 , H01L23/29 , H01L23/31 , H05K3/28
CPC classification number: C08K3/22 , C04B2235/3256 , C04B2235/3258 , C04B2235/3284 , C04B2235/3418 , C04B2235/424 , C04B2235/48 , C04B2235/483 , C08K3/24 , C08K3/36 , C08K2201/014 , H01L23/293 , H01L2924/0002 , H05K3/285 , Y10T428/31511 , C08L63/00 , H01L2924/00
Abstract: 【課題】ハロゲン、リン、およびアンチモンを実質的に含まない難燃性成形組成物を開示する。 また、集積回路の様な電子デバイスを被覆するために、これらの難燃性成形組成物を使用することを開示する。
【解決手段】難燃性成形組成物は、エポキシ樹脂;三酸化タングステンの様な、耐火金属を含む第一の遷移金属酸化物;およびモリブデン酸カルシウムの様な、VIA族元素のオキシアニオン及びIIA族元素のカチオンを含む第二の遷移金属酸化物を含む。
-
-
-
-
-
-
-
-
-