公开(公告)号:JP4847339B2
公开(公告)日:2011-12-28
申请号:JP2006543159
申请日:2005-10-25
Applicant: 日本碍子株式会社
CPC classification number: C04B35/195 , C04B35/62665 , C04B35/63 , C04B35/632 , C04B38/0006 , C04B38/08 , C04B2111/00793 , C04B2235/3206 , C04B2235/3217 , C04B2235/3218 , C04B2235/3222 , C04B2235/3418 , C04B2235/3445 , C04B2235/3463 , C04B2235/349 , C04B2235/449 , C04B2235/5436 , C04B2235/5445 , C04B2235/9607 , Y10T428/24149
-
公开(公告)号:JPWO2008099844A1
公开(公告)日:2010-05-27
申请号:JP2008558099
申请日:2008-02-13
Applicant: 日本碍子株式会社
CPC classification number: C04B37/005 , B01D46/2448 , B01D46/2451 , B01D46/2459 , B01D46/2466 , B01D2046/2433 , B01D2046/2496 , B01D2279/30 , C04B28/24 , C04B35/565 , C04B35/6316 , C04B35/806 , C04B38/0019 , C04B2111/00413 , C04B2235/3418 , C04B2235/3427 , C04B2235/349 , C04B2235/5228 , C04B2237/083 , C04B2237/365 , C04B2237/52 , C04B2237/68 , F01N3/0222 , F01N2330/60 , C04B14/104 , C04B14/20 , C04B14/324 , C04B14/4656 , C04B20/008 , C04B22/148 , C04B38/007 , C04B38/0645 , C04B2103/0091 , C04B2103/0094 , C04B24/06
Abstract: ディーゼル車の排気ガス浄化用フィルタとして使用されるハニカム構造体には、溜まったカーボン微粒子を燃焼させて除去するという再生処理を行うことが必要である。この際に局所的な高温化が避けられないため、大きな熱応力が発生し易く、亀裂が発生しやすいという問題が存在した。接合層12に低気孔率部分と高気孔率部分を備え、その位置を制御することで、接合部が破壊した際の亀裂の進展位置を高気孔率部分に誘導し、亀裂を高気孔率部分で屈曲させることで、接合層12の破断を起こりにくくし、亀裂の進展を制御可能な接合体とその製造方法を見出した。
-
公开(公告)号:JPWO2008088013A1
公开(公告)日:2010-05-13
申请号:JP2008554076
申请日:2008-01-17
Applicant: 日本碍子株式会社
CPC classification number: C04B35/806 , B28B1/002 , B28B11/243 , C04B28/24 , C04B35/565 , C04B37/005 , C04B38/0006 , C04B38/0019 , C04B2111/00793 , C04B2235/3418 , C04B2235/3427 , C04B2235/349 , C04B2235/5228 , C04B2235/606 , C04B2235/9607 , C04B2237/083 , C04B2237/365 , F01N3/2828 , F26B21/006 , C04B38/0054 , C04B38/0074 , C04B14/104 , C04B14/324 , C04B2103/42 , C04B14/4656
Abstract: 接合材層によって一体的に接合された複数のハニカムセグメントの接合組織にばらつきが生じて特性がばらつくことを低減するハニカムセグメント接合体の乾燥方法を提供する。隔壁により仕切られ軸方向に貫通する複数のセルを有するハニカムセグメント10を接合材により複数互いの接合面で一体的に接合し、接合材が硬化する前に、一体化されたハニカムセグメント接合体1の両端面8を同時に加熱して乾燥させ、その後、全体を加熱して乾燥する。ハニカムセグメント接合体1の全体の水分量の1%以上が飛散するまで、両端面8を乾燥するとよい。
-
公开(公告)号:JP4426524B2
公开(公告)日:2010-03-03
申请号:JP2005503540
申请日:2004-03-10
Applicant: 日本碍子株式会社
Inventor: 崇弘 冨田
IPC: C04B38/00 , C04B35/14 , C04B35/18 , C04B35/195 , C04B35/20 , C04B35/46 , C04B35/622
CPC classification number: C04B38/0051 , C04B38/0074
-
公开(公告)号:JP4307781B2
公开(公告)日:2009-08-05
申请号:JP2002061989
申请日:2002-03-07
Applicant: 日本碍子株式会社
IPC: B01D39/00 , C04B38/00 , B01D39/20 , B01D53/86 , B01J27/224 , B01J32/00 , B01J35/04 , C04B35/565
CPC classification number: C04B38/0038 , C04B35/565 , C04B35/6316 , C04B35/6365 , C04B38/0006 , C04B2235/3206 , C04B2235/3208 , C04B2235/3213 , C04B2235/3427 , C04B2235/3481 , C04B2235/3826 , C04B2235/428 , C04B2235/5436 , C04B2235/6021 , C04B2235/6582 , C04B2235/668 , C04B2235/728 , C04B2235/77 , C04B2235/80 , C04B2235/96 , C04B2235/9607 , C04B35/63 , C04B38/0009 , C04B38/0051 , C04B35/65
Abstract: A silicon carbide-based porous material containing silicon carbide particles (1) as an aggregate and metallic silicon (2), wherein the average pore diameter of the silicon carbide-based porous material is at least 0.25 time the average particle diameter of the silicon carbide particles (1), or the contact angle between the silicon carbide particles (1) and the metallic silicon (2) is acute, or a large number of secondary texture particles each formed by contact of at least four silicon carbide particles (1) with one metallic silicon (2) are bonded to each other to form a porous structure. This silicon carbide-based porous material can be sintered, in its production, at a relatively low firing temperature and, therefore, can be provided at a low production cost, at a high yield and at a low product cost.
-
-
公开(公告)号:JPWO2007069674A1
公开(公告)日:2009-05-28
申请号:JP2007550217
申请日:2006-12-14
Applicant: 日本碍子株式会社
CPC classification number: B01D46/2448 , B01D46/0001 , B01D46/2429 , B01D46/2444 , B01D46/2459 , B01D2046/2496 , B01D2265/04 , C04B35/10 , C04B35/185 , C04B35/195 , C04B35/478 , C04B35/563 , C04B35/565 , C04B35/581 , C04B35/584 , C04B35/597 , C04B37/005 , C04B38/0019 , C04B2111/00793 , C04B2237/06 , C04B2237/062 , C04B2237/068 , C04B2237/365 , Y10T428/24149 , C04B38/0074
Abstract: 硬化後の接合材層のヤング率が被接合物の20%以上であり、且つ硬化後の平均線熱膨張係数が被接合物の70%以下である接合材である。この接合材は、発生する熱応力によるハニカムセグメントの変形を接合層で抑制することができ、クラック等の欠陥の発生を低減することができる排ガス用の捕集フィルタ、中でも、ディーゼルエンジンの排ガス中の粒子状物質(パティキュレート)等を捕集するディーゼルパティキュレートフィルタ(DPF)の作製時に好適に用いることができる。
-
公开(公告)号:JPWO2005095302A1
公开(公告)日:2008-07-31
申请号:JP2006511672
申请日:2005-03-29
Applicant: 日本碍子株式会社
IPC: C04B35/63 , C04B35/622
CPC classification number: C04B35/63
Abstract: セラミックス形成材料を含有する成形原料を混練することによって得られるセラミックス坏土であって、成形原料として、セラミックス形成材料に加えて、層状複水酸化物を、セラミックス形成材料との合計に対して0.5〜50質量%の割合で含有させるとともに、NGK粘土硬度計にて測定した硬度を4〜18mmとする。
-
公开(公告)号:JPWO2006046542A1
公开(公告)日:2008-05-22
申请号:JP2006543159
申请日:2005-10-25
Applicant: 日本碍子株式会社
CPC classification number: C04B35/195 , C04B35/62665 , C04B35/63 , C04B35/632 , C04B38/0006 , C04B38/08 , C04B2111/00793 , C04B2235/3206 , C04B2235/3217 , C04B2235/3218 , C04B2235/3222 , C04B2235/3418 , C04B2235/3445 , C04B2235/3463 , C04B2235/349 , C04B2235/449 , C04B2235/5436 , C04B2235/5445 , C04B2235/9607 , Y10T428/24149
Abstract: コージェライト形成材料からなる成形用調合物と有機バインダとを含有する坏土をハニカム形状に成形してハニカム成形体を作製し、ハニカム成形体を焼成してハニカム構造体を得るハニカム構造体の製造方法であって、成形用調合物が、少なくともタルク(第1のマグネシウム含有物質)を含む2種以上のマグネシウム含有物質を含有し、マグネシウム含有物質の中で、タルク以外のマグネシウム含有物質(第2のマグネシウム含有物質)の平均粒子径が4μm以下であるハニカム構造体の製造方法。坏土中の有機物の含有量が少なくても、良好に成形されたハニカム構造体を得ることが可能なハニカム構造体の製造方法及びハニカム構造体を提供する。
-
公开(公告)号:JPWO2005097703A1
公开(公告)日:2008-02-28
申请号:JP2006511975
申请日:2005-03-18
Applicant: 日本碍子株式会社
IPC: C04B38/00 , B01D39/00 , B01D39/20 , B01J35/04 , B01J37/04 , B01J37/08 , B28B3/20 , C04B35/195 , C04B35/622
CPC classification number: B29D99/0089 , C04B35/195 , C04B35/6263 , C04B38/0006 , C04B2235/3201 , C04B2235/3208 , C04B2235/3217 , C04B2235/3218 , C04B2235/3418 , C04B2235/3445 , C04B2235/349 , C04B2235/96 , C04B2235/9607 , Y10T428/24149 , C04B35/6303
Abstract: コーディエライト形成材料及び有機バインダを含有する成形原料を混練、成形して、ハニカム形状の成形体(ハニカム成形体)を作製し、作製されたハニカム成形体を焼成して、コーディエライトを主成分とするハニカム形状の構造体(ハニカム構造体)を得るハニカム構造体の製造方法であって、成形原料として、コーディエライト形成材料及び有機バインダに加えて、層電荷(X)が0.2
-
-
-
-
-
-
-
-
-