Fluororesin composition for coating and product using the same
    61.
    发明专利
    Fluororesin composition for coating and product using the same 审中-公开
    用于涂料的氟菊酯组合物和使用该组合物的产品

    公开(公告)号:JP2009024145A

    公开(公告)日:2009-02-05

    申请号:JP2007191771

    申请日:2007-07-24

    Abstract: PROBLEM TO BE SOLVED: To provide a fluororesin composition for coating, which can be applied at a construction site and from which a heat-ray shielding film excellent in transparency, chemical resistance and weather resistance can be formed.
    SOLUTION: The fluororesin composition for coating contains a fluororesin (A) having 30-200 mg-KOH/g hydroxyl value and heat-ray shielding inorganic fine particles (B) having 1-200 nm average particle diameter.
    COPYRIGHT: (C)2009,JPO&INPIT

    Abstract translation: 要解决的问题:提供可以施工在施工现场的涂料用氟树脂组合物,由此可以形成透明性,耐化学性和耐候性优异的热射线屏蔽膜。 解决方案:用于涂料的氟树脂组合物含有具有30-200mg-KOH / g羟基值的氟树脂(A)和具有1-200nm平均粒径的热射线屏蔽无机细颗粒(B)。 版权所有(C)2009,JPO&INPIT

    Fluororesin-based thermosetting powder coating composition exhibiting excellent stain resistance
    63.
    发明专利
    Fluororesin-based thermosetting powder coating composition exhibiting excellent stain resistance 审中-公开
    基于荧光素的热固化粉末涂料组合物展示出优异的耐污性

    公开(公告)号:JP2008266361A

    公开(公告)日:2008-11-06

    申请号:JP2007107017

    申请日:2007-04-16

    Abstract: PROBLEM TO BE SOLVED: To provide a fluororesin-based thermosetting powder coating composition exhibiting excellent stain resistance.
    SOLUTION: The fluororesin-based thermosetting powder coating composition exhibiting excellent stain resistance comprises 100 pts.wt. of a resin composition comprised of (a) 65-95 wt.% of a crosslinkable reactive group-bearing fluororesin having a fluorine content of 10-30 wt.% and a glass transition temperature of 30-85°C and (b) 5-35 wt.% a curing agent capable of reacting with the crosslinkable reactive group of the fluororesin to form a crosslink, and incorporated therewith, (c) 0.1-10.0 pts.wt. of an alkyl silicate mixture as a hydrophilizing agent comprised of 45-79 wt.% of an alkyl polysilicate compound, 5-20 wt.% of a tetraalkoxysilane compound and 1-50 wt.% of a linear alcohol.
    COPYRIGHT: (C)2009,JPO&INPIT

    Abstract translation: 要解决的问题:提供具有优异耐污性的氟树脂类热固性粉末涂料组合物。

    解决方案:耐污染性优异的氟树脂类热固性粉末涂料组合物包含100重量份 的树脂组合物包含(a)含氟量为10〜30重量%,玻璃化转变温度为30〜85℃的交联性反应性基团的氟树脂为65〜95重量%,(b)为5〜 -35重量%的能够与氟树脂的可交联反应性基团反应以形成交联的固化剂,并且与其结合,(c)0.1-10.0重量份 的烷基硅酸盐混合物作为亲水剂,其由45-79重量%的烷基聚硅酸盐化合物,5-20重量%的四烷氧基硅烷化合物和1-50重量%的直链醇组成。 版权所有(C)2009,JPO&INPIT

    Coated substrate having coating film comprising hollow silicone particulate and fluorine resin
    65.
    发明专利
    Coated substrate having coating film comprising hollow silicone particulate and fluorine resin 审中-公开
    具有包覆中空硅胶颗粒和氟树脂的涂层膜的涂层基材

    公开(公告)号:JP2008201908A

    公开(公告)日:2008-09-04

    申请号:JP2007039813

    申请日:2007-02-20

    Abstract: PROBLEM TO BE SOLVED: To provide a transparent coated substrate exerting a low reflectance and a high film strength by providing a coated film comprising a hollow silicone particulate and a fluorine resin for forming the coating film, provided that the hollow silicone particulate has a high porosity and a low reflectance, shows a high productivity, is hardly breakable and has a narrow particle size distribution and a particle size of ≤1 μm, and the fluorine resin for forming the coating film has a low reflectance.
    SOLUTION: The transparent substrate having a low reflectance and a high film strength is obtained by providing the coating film comprising the hollow silicone particulate and the fluorine resin for forming the coating film. Here, the hollow silicone particulate is obtained by removing an organic polymer particle and/or an organic solvent from a core-shell particle, provided that the core-shell particle is obtained by coating a particle comprising the organic polymer particle and/or the organic solvent with a particular silicone compound.
    COPYRIGHT: (C)2008,JPO&INPIT

    Abstract translation: 要解决的问题:通过提供一种包含中空硅氧烷颗粒和用于形成涂膜的氟树脂的涂膜,提供具有低反射率和高膜强度的透明涂层基材,只要中空硅氧烷颗粒具有 高孔隙率,低反射率,高生产率,难以破裂,粒径分布窄,粒径≤1μm,形成涂膜用氟树脂反射率低。 解决方案:通过提供包含中空硅氧烷颗粒和用于形成涂膜的氟树脂的涂膜,获得具有低反射率和高膜强度的透明基板。 这里,中空硅氧烷颗粒是通过从核 - 壳颗粒中除去有机聚合物颗粒和/或有机溶剂而获得的,条件是核 - 壳颗粒是通过将包含有机聚合物颗粒和/或有机聚合物颗粒的颗粒 溶剂与特定的硅氧烷化合物。 版权所有(C)2008,JPO&INPIT

    Powder coating, coating film layer, coating method and coated article
    66.
    发明专利
    Powder coating, coating film layer, coating method and coated article 审中-公开
    粉末涂料,涂膜,涂料方法和涂料

    公开(公告)号:JP2007321114A

    公开(公告)日:2007-12-13

    申请号:JP2006155538

    申请日:2006-06-05

    Inventor: OOTA KAZUNOBU

    Abstract: PROBLEM TO BE SOLVED: To obtain a powder coating that provides photocatalytic performance by photocatalytic activity even in a condition having little ultraviolet irradiation or almost no ultraviolet irradiation and develops photocatalytic activity especially indoors so as to exhibit photocatalytic performance and a coating film layer, to provide a coating method and to obtain a coated article. SOLUTION: The powder coating obtains photocatalytic performance by photocatalytic activity of a photocatalytic crystal 1 with a visible light even in a condition having little ultraviolet irradiation or almost no ultraviolet irradiation by development of the photocatalytic activity of the photocatalytic crystal 1 mixed in a coating matrix 2 with a visible light at a wavelength of ≥380 nm and develops the photocatalytic activity of the photocatalytic crystal 1 by making good use of a visible light derived from a light of fluorescent light, etc., existing indoors even in a house hardly having ultraviolet irradiation so as to exhibit photocatalytic performance. COPYRIGHT: (C)2008,JPO&INPIT

    Abstract translation: 要解决的问题:为了获得即使在紫外线辐射少或几乎没有紫外线照射的条件下也能通过光催化活性提供光催化性能的粉末涂料,特别是在室内显影光催化活性以显示光催化性能和涂膜层 ,以提供涂布方法并获得涂布制品。 解决方案:即使在少量紫外线照射的条件下也可以通过光催化结晶1的光催化活性获得光催化性能,或者几乎不发生通过混合在光催化结晶1中的光催化活性的紫外线照射 涂层基体2具有波长≥380nm的可见光,并且通过充分利用由室内甚至室内甚至室内的荧光等引起的可见光,从而显现出光催化性结晶1的光催化活性 具有紫外线照射以显示光催化性能。 版权所有(C)2008,JPO&INPIT

    Optical film, polarizing plate and image display device
    67.
    发明专利
    Optical film, polarizing plate and image display device 有权
    光学膜,偏光板和图像显示装置

    公开(公告)号:JP2007298974A

    公开(公告)日:2007-11-15

    申请号:JP2007097467

    申请日:2007-04-03

    Abstract: PROBLEM TO BE SOLVED: To provide an optical film having a low reflectance and excellent in at least one of abrasion resistance and magic wiping durability. SOLUTION: The optical film has a layer provided by applying a coating composition as an outermost layer above a support, wherein the coating composition contains (A) a fluorine-containing compound having a fluorine content of ≥40% and (B) a particle having a particle size of 5-120 nm, and the outermost layer has a refractive index of 1.20-1.38. COPYRIGHT: (C)2008,JPO&INPIT

    Abstract translation: 要解决的问题:提供具有低反射率和优异的耐磨性和魔法擦拭耐久性中的至少一个的光学膜。 解决方案:光学膜具有通过将涂料组合物涂布在载体上方的最外层而提供的层,其中涂料组合物含有(A)氟含量≥40%的含氟化合物和(B) 粒径为5-120nm的粒子,最外层的折射率为1.20〜1.38。 版权所有(C)2008,JPO&INPIT

    Photocatalytic body and set of paint composition for forming the same
    68.
    发明专利
    Photocatalytic body and set of paint composition for forming the same 有权
    光化学体系及其形成组合物

    公开(公告)号:JP2007289955A

    公开(公告)日:2007-11-08

    申请号:JP2007138855

    申请日:2007-05-25

    Abstract: PROBLEM TO BE SOLVED: To provide a photocatalytic body which photocatalytic particles strongly adhere over a long period of time without losing ability with extremely little degradation and deterioration of the binder caused by the photocatalytic particles. SOLUTION: A photocatalytic body keeps a first layer containing a persistent binder overlying a substrate, but no photocatalytic particles, and the first layer is costed or sprayed with a mixture of the persistent binder and the photocatalytic particles and dried at an ambient temperature of 200°C to provide a second layer. The volume of photocatalytic particles as a volume standard against a total amount of the photocatalytic particles and the persistent binder of the second layer is; (1) 5-40%, if the persistent binder is cement and/or gypsum, (2) 20-98%, if the persistent binder is not cement and/or gypsum. COPYRIGHT: (C)2008,JPO&INPIT

    Abstract translation: 要解决的问题:为了提供光催化剂颗粒在长时间内强烈粘附而不丧失能力的光催化体,极少的降解和由光催化剂颗粒引起的粘合剂的劣化。 解决方案:光催化体将包含持久性粘合剂的第一层保持在基材上,但没有光催化颗粒,并且第一层被成本化或用持久性粘合剂和光催化颗粒的混合物喷涂并在环境温度下干燥 为200℃,以提供第二层。 相对于光催化颗粒和第二层的持久性粘合剂的总量的光催化颗粒的体积标准为体积; (1)如果持久性粘合剂是水泥和/或石膏,则为5-40%,(2)如果持久性粘合剂不是水泥和/或石膏,则为20-98%。 版权所有(C)2008,JPO&INPIT

    Coating material, method for producing the same and optical article
    69.
    发明专利
    Coating material, method for producing the same and optical article 审中-公开
    涂料,其制造方法和光学制品

    公开(公告)号:JP2007182511A

    公开(公告)日:2007-07-19

    申请号:JP2006002168

    申请日:2006-01-10

    Abstract: PROBLEM TO BE SOLVED: To provide a coating material having high surface hardness, excellent in scratch resistance and having low refractive index and to provide a method for producing the coating material and to provide an optical article using the coating material. SOLUTION: The coating material comprises (A) a compound having a perfluoro group, (B) silica microparticles having 40-100 nm average particle diameter and having voids in the inside and (C) porous silica microparticles having 5-30 nm average particle diameter. In the coating material, refractive index of a film obtained after coating is ≤1.365. COPYRIGHT: (C)2007,JPO&INPIT

    Abstract translation: 要解决的问题:提供具有高表面硬度,优异的耐刮擦性和低折射率的涂料,并提供一种制备涂料的方法,并提供使用这种涂料的光学制品。 解决方案:涂层材料包括(A)具有全氟基团的化合物,(B)具有40-100nm平均粒径并且在内部具有空隙的二氧化硅微粒和(C)具有5-30nm的多孔二氧化硅微粒 平均粒径。 在涂料中,涂布后获得的膜的折射率≤1.365。 版权所有(C)2007,JPO&INPIT

    Precoated metal sheet and its manufacturing method
    70.
    发明专利
    Precoated metal sheet and its manufacturing method 有权
    预制金属板及其制造方法

    公开(公告)号:JP2007098864A

    公开(公告)日:2007-04-19

    申请号:JP2005294109

    申请日:2005-10-06

    Inventor: HATTORI NOBUO

    Abstract: PROBLEM TO BE SOLVED: To provide a precoated metal sheet having excellent formability and an excellent appearance, and also having characteristics in which an adhesive material is hardly adhere thereto even in the case of using the adhesive material together, and soil and oil are hardly adhere, even if the precoated metal sheet is contacted with an optical disk or the like, its surface is hardly injured, and to provide its manufacturing method. SOLUTION: A pre-coated metal sheet 1 provided with a metal plate 2 and a resin film 3 comprised of a fluororesin matrix layer 4 in which urethane beads 5 are dispersed is constituted. In this case, the content of the urethane bead 5 is ≥5 mass% and ≤50 mass%, its mean particle diameter is not lower than 1.1 times and not higher than 5 times of the mean thickness of the fluororesin matrix layer 4, when the concentration of fluorine in the resin film 3 is calculated according to a formula: A(%)=äF/(F+C+O+N)}×100, the concentration is not lower than 15% on the utmost top face of the film and not higher than 15% at the inside of the film. Wherein A is the concentration proportion of fluorine; F is a fluorine mass%; C is a carbon mass%; O is an oxygen mass%; and N is a nitrogen mass%. COPYRIGHT: (C)2007,JPO&INPIT

    Abstract translation: 要解决的问题:提供具有优异成形性和优异外观的预涂金属片,并且即使在使用粘合剂材料的情况下也具有难以粘附粘合剂的特性,以及土壤和油 即使预涂金属片与光盘等接触,其表面几乎不受伤,也提供其制造方法。 解决方案:设置有金属板2的预涂金属板1和由其中分散有聚氨酯珠5的氟树脂基质层4组成的树脂膜3。 在这种情况下,聚氨酯珠粒5的含量为≥5质量%且≤50质量%,其平均粒径不低于氟树脂基质层4的平均厚度的1.1倍且不高于5倍,当 根据以下公式计算树脂膜3中的氟浓度:A(%)=äF/(F + C + O + N)}×100,在最上面的浓度不低于15% 电影里面不超过15%。 其中A是氟的浓度比例; F为氟质量% C为碳质量% O是氧质量%; N为氮质量%。 版权所有(C)2007,JPO&INPIT