公开(公告)号:JP2006226287A
公开(公告)日:2006-08-31
申请号:JP2006034702
申请日:2006-02-13
发明人: SHIRK RYAN C , SANOCKI STEPHEN M , PEISERT JOSEPH C , LANGER ROGER L , HORNBACK LOYD R III , HARDING IAN R
IPC分类号: F01N3/24 , B01D53/86 , B01D53/94 , B01J33/00 , D04H1/70 , D06M11/79 , F01N3/26 , F01N3/28 , F01N13/14
摘要: PROBLEM TO BE SOLVED: To provide an insulating member suitable for insulating an end cone body of a pollution control device. SOLUTION: An insulating end cone body 60 is suitable for insulting the end cone body of the pollution control device. The insulating end cone body 60 includes a cone-shaped foam or non-foam insulating material containing inorganic fiber suitable for insulating the end cone body of the pollution control device, and a shape-retaining element which is in intimate contact with the insulating material and which contains a binder to maintain the insulating material in a self-supporting cone shape. COPYRIGHT: (C)2006,JPO&NCIPI
-
公开(公告)号:JP2005260261A
公开(公告)日:2005-09-22
申请号:JP2005120129
申请日:2005-04-18
发明人: BRUXVOORT WESLEY J , CULLER SCOTT R , HO KWOK-LUN , KAISAKI DAVID A , KESSEL CARL R , KLUN THOMAS P , KRANZ HEATHER K , MESSNER ROBERT P , WEBB RICHARD J , WILLIAMS JULIA P
IPC分类号: B24B1/00 , B24B7/22 , B24B21/04 , B24B37/04 , B24B53/007 , B24B53/017 , B24D3/00 , B24D3/02 , B24D3/28 , B24D11/00 , H01L21/304 , H01L21/3105
CPC分类号: B24B53/017 , B24B7/228 , B24B21/04 , B24B37/042 , B24D3/28 , B24D11/00 , H01L21/31053
摘要: PROBLEM TO BE SOLVED: To provide a semiconductor wafer having a more "flat" and/or more "even" and/or more "unrough" surface than a surface wafer before processing, by modifying the surface of the semiconductor wafer. SOLUTION: A method of modifying the surface of a semiconductor wafer 34 comprises the steps of (a) bringing a plurality of abrasive particles and a binder into contact with a fixed article 39 to be polished having a three-dimensionally processed polished surface including a predetermined pattern shape; and of (b) modifying the surface of the wafer by relatively moving the wafer and the fixed article to be polished. COPYRIGHT: (C)2005,JPO&NCIPI
摘要翻译: 要解决的问题:通过修改半导体晶片的表面,提供在处理之前具有比表面晶片更“平坦”和/或更多的“平坦”和/或更“不通”表面的半导体晶片。 解决方案:修改半导体晶片34的表面的方法包括以下步骤:(a)使多个研磨颗粒和粘合剂与待研磨的固定制品39接触,所述固定制品39具有三维处理的抛光表面 包括预定图案形状; 和(b)通过相对移动待抛光的晶片和固定物品来改变晶片的表面。 版权所有(C)2005,JPO&NCIPI
-
公开(公告)号:JP2005111475A
公开(公告)日:2005-04-28
申请号:JP2004320818
申请日:2004-11-04
发明人: HUELSMAN GARY L , KOLB WILLIAM B
IPC分类号: B05C9/14 , B05D3/02 , B05D5/12 , F26B3/20 , F26B7/00 , F26B13/10 , F26B25/00 , G11B5/84 , G11B5/842 , G11B5/845
CPC分类号: F26B25/006 , F26B3/20 , F26B7/002 , F26B13/10 , F26B13/105 , G11B5/84 , G11B5/842 , G11B5/845
摘要: PROBLEM TO BE SOLVED: To provide a method and an apparatus for efficiently drying coating on a coated substrate.
SOLUTION: The method and the apparatus (10) for drying the substrate (16) uses a condensing surface (22) located near the substrate on the side of the substrate being dried. The liquid from the substrate is evaporated and then condensed on the condensing surface (22). The condensed liquid is moved thereon using at least capillary force. The coated substrate is subjected to a magnetic field between the condensing surface and the coated substrate created in advance at a location outside a space between the condensing surface and the coated substrate to orient magnetic particles on the coated substrate.
COPYRIGHT: (C)2005,JPO&NCIPI摘要翻译: 要解决的问题:提供一种用于在涂覆的基材上有效干燥涂层的方法和装置。 解决方案:用于干燥基板(16)的方法和装置(10)使用位于待干燥的基板侧的基板附近的冷凝表面(22)。 将来自基板的液体蒸发,然后在冷凝表面(22)上冷凝。 冷凝的液体至少使用毛细管力在其上移动。 涂覆的基板在冷凝表面和涂覆的基板之间在冷凝表面和涂覆的基板之间的空间外的位置处预先形成磁场,以使涂覆的基板上的磁性颗粒定向。 版权所有(C)2005,JPO&NCIPI
-
公开(公告)号:JP2004315236A
公开(公告)日:2004-11-11
申请号:JP2004125748
申请日:2004-04-21
CPC分类号: B65H1/00 , B42D5/005 , B65C11/00 , B65D83/0894 , B65H2402/41 , B65H2402/411 , B65H2701/1934
摘要: PROBLEM TO BE SOLVED: To provide a new improved holding means to which a dispenser is mounted to place the same on a specific place such as the back or wrist of a user's hand, or a vertical or horizontal surface.
SOLUTION: This dispenser 20 is used for taking out soft sheets one by one from a sheet stack coated with an adhesive agent, and comprises a first housing part 35 and a second housing part 36. The first housing part 35 comprises a bottom wall 23, an end wall, a side wall and a first upper side wall part 28, and the second housing part comprises a second upper side wall part 29 mounted on the first housing part 35. The second upper side wall part 29 has an opening part between the end parts to discharge the sheet, the second upper side wall part 29 is formed apart from the first upper side wall part 28, and the stack can be put in a cavity part.
COPYRIGHT: (C)2005,JPO&NCIPI-
公开(公告)号:JP2004148500A
公开(公告)日:2004-05-27
申请号:JP2003404522
申请日:2003-12-03
CPC分类号: B24D11/005 , B29C39/148 , B29K2105/16
摘要: PROBLEM TO BE SOLVED: To provide a method for manufacturing abrasive products.
SOLUTION: The method includs the steps of:(a) providing a backing material having a front surface; (b) providing a manufacturing tool having a contacting surface and an radiation energy transmission;(c) coating a mixed material including several abrasive particles and a binder precursor on the contacting surface of the manufacturing tool;(d) making contact the mixed material, that is applied on the contacting surface of the manufacturing tool, on the front surface of the backing material so as to wet the surface of the backing material with this mixed material;(e) providing a structure material formed for handling after at least partially curing the binder precursor by transmitting radiation energy through the manufacturing tool;(f) separating the structure material formed for handling from the manufacturing tool.
COPYRIGHT: (C)2004,JPO摘要翻译: 要解决的问题:提供一种制造磨料产品的方法。 解决方案:该方法包括以下步骤:(a)提供具有前表面的背衬材料; (b)提供具有接触表面和辐射能量传递的制造工具;(c)在制造工具的接触表面上涂覆包括若干磨料颗粒和粘合剂前体的混合材料;(d)使混合材料接触, 其被施加在制造工具的接触表面上,在背衬材料的前表面上,以便用该混合材料润湿背衬材料的表面;(e)提供形成用于在至少部分固化后处理的结构材料 通过将辐射能量传递通过制造工具;(f)将形成的用于处理的结构材料与制造工具分离。 版权所有(C)2004,JPO
-
公开(公告)号:JP2003238686A
公开(公告)日:2003-08-27
申请号:JP2003002885
申请日:2003-01-09
发明人: MAZUREK MIECZYSLAW H , KANTNER STEVEN S , LEIHR CHARLES M , BOGAERT YVAN A , GALKIEWICZ ROBERT K , SHERMAN AUDREY A
IPC分类号: C07F7/08 , C07F7/12 , C07F7/18 , C08F290/00 , C08F299/08 , C08G77/20 , C08G77/26 , C08G77/28 , C08G77/388 , C09J5/00 , C09J5/06 , C09J7/02 , C09J155/00 , C09J183/00 , C09J183/02 , C09J183/07 , C09J183/08
摘要: PROBLEM TO BE SOLVED: To provide a reaction terminator for a silicone compound which can be quickly, perfectly, and reliably cured with a radiation even when it has a high molecular weight. SOLUTION: A terminator being a fluorosilane compound represented by formula (1) is reacted with a solution of a living polymer siloxanolate in a nonhydroxy solvent to form a siloxane macromonomer represented by formula (2). COPYRIGHT: (C)2003,JPO
-
公开(公告)号:JP2003176466A
公开(公告)日:2003-06-24
申请号:JP2002365116
申请日:2002-12-17
发明人: SHIZUKUDA HARUO , KODA NOBORU
IPC分类号: C09J7/02 , C09J183/04 , C09J201/00
摘要: PROBLEM TO BE SOLVED: To provide a double-sided self-adhesive tape having good punchability, heat resistance, and dimensional stability, and capable of being equipped with a silicone self-adhesive agent. SOLUTION: This multilayered foamed pressure-sensitive self-adhesive tape is formed by laminating a foamed pressure-sensitive adhesive layer, a transparent flexible film, a transparent self-adhesive or transparent adhesive layer, and a transparent release agent in this order. Further, the multilayered foamed pressure-sensitive self-adhesive tape is formed by laminating a self-adhesive, a foamed base material, the transparent flexible film, the transparent self-adhesive or transparent adhesive layer, and the transparent release agent in this order. COPYRIGHT: (C)2003,JPO
-
公开(公告)号:JP2002370176A
公开(公告)日:2002-12-24
申请号:JP2002169993
申请日:2002-06-11
发明人: BARRY JOHN L , BELL DONALD R , CHESLEY JASON A , MELBYE WILLIAM L , RUDE HAROLD E , SHEFEIELD WILLIAM F , SLAMA DAVID F , STEPHENS ALAN N
CPC分类号: B29C43/222 , A44B18/0003 , A44B18/0049 , A44B18/0053 , B24D9/085 , B24D11/00 , B29C43/46 , B29C55/06 , B29C59/025 , B29C2043/461 , B29L2031/729
摘要: PROBLEM TO BE SOLVED: To realize durability sufficient for embodiment by solving a problem wherein fiber falls off from a cut loop part and sticks to a painting surface when cutting an abrasive, and a problem wherein the loop part is damaged by a polishing surface when stacking the abrasive. SOLUTION: A loop engaging means 442 engaging with projecting hook stems 446 is arranged on the support member 412 side of a backup pad, and a plurality of hook stems 446 engageably and disengageably engaging with this loop engaging means 442 are arranged on the abrasive 444 side. Respective loops for constituting the loop engaging means 442 are composed of one or two or more filaments. Tensile strength of the respective filaments is set larger than 60 g, and the loop height is set to 0.25 to 6.25 mm.
摘要翻译: 要解决的问题:通过解决当切割磨料时纤维从切割环部分脱落并粘附到涂漆表面的问题,实现足够的耐久性,以及当堆叠时环路部分被抛光表面损坏的问题 磨料。 解决方案:与支撑杆446接合的环接合装置442设置在支撑垫的支撑构件412侧,并且与该环接合装置442接合和脱离接合的多个钩杆446布置在磨料444侧 。 用于构成环接合装置442的各个环由一个或两个或更多个长丝组成。 各个长丝的拉伸强度设定为大于60g,并且将环高度设定为0.25〜6.25mm。
-
公开(公告)号:JP2002155124A
公开(公告)日:2002-05-28
申请号:JP2001275190
申请日:2001-09-11
发明人: HAIDOS JOHN C , ARUDI RAVINDRA L , ROTTO NELSON T
IPC分类号: C08F12/12 , C08F12/00 , C08G18/38 , C08G18/81 , C08K5/521 , C08L71/02 , C08L75/14 , C09D5/00 , C09D5/23 , C09D171/00 , C09D171/12 , C09D175/08 , C09D175/14 , G11B5/70 , G11B5/702 , G11B5/73 , G11B5/735
摘要: PROBLEM TO BE SOLVED: To provide a dispersion used particularly for a magnetic layer provided on a non-magnetic support, optionally for a back side coating. SOLUTION: At least one of the magnetic layer and the optional back side coating contains a polymer binder obtained from a reaction product containing a free-radical generator and a radiation-curable polymer. The radiation-curable polymer contains α-methylstyrene parts represented by formula (I) on its side chains.
-
公开(公告)号:JP2002138078A
公开(公告)日:2002-05-14
申请号:JP2001204928
申请日:2001-07-05
IPC分类号: B01F17/00 , B01F17/38 , B01F17/52 , C07C17/00 , C07C17/25 , C07C19/08 , C07C19/10 , C07C19/14 , C07C19/16 , C07C31/40 , C07C51/285 , C07C53/21 , C07C69/653 , C07C303/24 , C07C303/32 , C07C305/06 , C07C309/13 , C07C309/14 , C07C309/15 , C07C309/17 , C07C319/02 , C07C319/14 , C07C319/18 , C07C323/03 , C07C323/12 , C07C323/14 , C07C323/50 , C07C323/52 , C07C323/60 , C07D303/08 , C08G18/08 , C08G18/09 , C08G18/28 , C08G18/80 , C08G63/682 , C08J7/04 , C08L101/00 , C09K3/00 , C09K3/18 , C11D1/04 , C11D1/10 , C11D1/14 , D06M13/02 , D06M13/224 , D06M13/236 , D06M13/244 , D06M13/248 , D06M13/252 , D06M13/265 , D06M13/272 , D06M13/282 , D06M13/292 , D06M13/298 , D06M13/322 , D06M13/372 , D06M13/398 , D06M13/402 , D06M13/408 , D06M13/425 , D06M13/428 , D06M13/46 , D06M13/463 , D06M13/467
摘要: PROBLEM TO BE SOLVED: To obtain an excellent surfactant composition comprising mixtures of the polymers containing perfluoroalkyl groups. SOLUTION: The surfactant composition is obtained by addition or polymerization, subsequently by subjecting to treatment with thiol, an amine, and the like, of the monomer unit represented by the formula Rfsb-Z (wherein Rf is a perfluroalkyl group; (s) is a linear chain; (b) is a branched chain; and Z is a double bond, a polymerizing group such as an epoxy group, or the like).
-
-
-
-
-
-
-
-
-