Steering column
    3.
    发明专利
    Steering column 有权
    驾驶杆

    公开(公告)号:JP2014139074A

    公开(公告)日:2014-07-31

    申请号:JP2014022148

    申请日:2014-02-07

    摘要: PROBLEM TO BE SOLVED: To provide a structure capable of securing strength while making thickness of a hollow circular tubular steering column thinner partially.SOLUTION: By performing drawing processing on a front end of an iron-based cylindrical member 19, an inner diameter of a front end surface is made smaller than that of a part positioned on the inner diameter side of a part forming a rear end surface of a body part 18. In addition, a part near the front end in the cylindrical member 19 is inserted into an insertion hole 25 opening toward an outer surface 24 of a mold 23, the part near the front end is projected toward inside of the mold 23. Molten metal of light alloy is fed into the mold 23, so as to mold the body part 18. After taken out from the mold 23, a cutting process is performed to an inner diameter part of a front end inner peripheral edge projecting toward an inner part of a radial direction in the cylindrical member 19 and the body part 18 so as to make an inner diameter of at least the part near the front end in the cylindrical member 19 equal to or more than that of the body part 18.

    摘要翻译: 要解决的问题:提供能够确保强度的结构,同时使空心圆形管状转向柱的厚度部分变薄。解决方案:通过在铁基圆柱形构件19的前端执行拉伸加工, 前端面比形成本体部18的后端面的部分的内径侧的部分小。此外,将圆筒部件19的前端附近的部分插入到插入部 孔25朝向模具23的外表面24开口,靠近前端的部分朝向模具23的内侧突出。轻合金的熔融金属被供给到模具23中,以模制主体部分18.之后 从模具23取出,对圆筒部件19和主体部18的向径向内侧突出的前端内周缘的内径部进行切削加工,以形成内径 至少在圆柱形构件19中的前端附近的部分等于或大于主体部分18的部分。

    Method of manufacturing aluminum base composite material matter
    7.
    发明专利
    Method of manufacturing aluminum base composite material matter 有权
    制备铝基复合材料的方法

    公开(公告)号:JP2011136370A

    公开(公告)日:2011-07-14

    申请号:JP2010255021

    申请日:2010-11-15

    IPC分类号: B22D19/14 B22D19/00

    摘要: PROBLEM TO BE SOLVED: To provide a method of manufacturing an aluminum base composite material matter. SOLUTION: This method of manufacturing the aluminum base composite material matter includes: a first step where a semi-solid-like aluminum base material is formed; a second step where a semi-solid-like mixture is obtained by adding reinforcing nano-particles to the semi-solid-like aluminum base material; a third step where the semi-solid-like mixture is made into a liquid state by heating; a fourth step where the mixture in the liquid state is processed ultrasonically; and a fifth step where the aluminum base composite material matter is obtained by cooling the mixture in the liquid state. COPYRIGHT: (C)2011,JPO&INPIT

    摘要翻译: 要解决的问题:提供一种制造铝基复合材料的方法。 解决方案:该铝基复合材料的制造方法包括:形成半固体状的铝基材的第一工序; 第二步,通过在半固体状铝基材中添加增强纳米粒子而获得半固体状混合物; 通过加热将半固体状混合物制成液态的第三步骤; 第四步骤,其中处于液态的混合物被超声处理; 以及第五步骤,其中通过将液体状态的混合物冷却来获得铝基复合材料。 版权所有(C)2011,JPO&INPIT

    Method for manufacturing aluminum composite material
    10.
    发明专利
    Method for manufacturing aluminum composite material 审中-公开
    制造铝复合材料的方法

    公开(公告)号:JP2006326630A

    公开(公告)日:2006-12-07

    申请号:JP2005152934

    申请日:2005-05-25

    IPC分类号: B22D19/00 B22D18/02 B22D27/09

    摘要: PROBLEM TO BE SOLVED: To provide a method for manufacturing an aluminum composite material which is formed by casting a ferrous sintered body having high adhesiveness with aluminum.
    SOLUTION: The method for manufacturing the aluminum composite material comprises a preforming step of forming and sintering ferrous powder so as to obtain a preformed body of a porous ferrous sintered material having 50% to 70% of the ferrous powder by an occupied volume percentage, and a composite material forming step of placing the preformed body, which is preheated at a preheating temperature of 300°C to 400°C in a vacuum, an inert gas atmosphere, a reducing gas atmosphere, or a mixed gas atmosphere of the inert gas and the reducing gas, in a casting mold held at a temperature of 200°C to 400°C, and then press-impregnating the preformed body with a molten aluminum or aluminum alloy to cast it by a two step pressing method comprising a first pressing step and a second pressing step.
    COPYRIGHT: (C)2007,JPO&INPIT

    摘要翻译: 解决的问题:提供一种铝复合材料的制造方法,该铝复合材料通过铸造与铝具有高粘合性的铁质烧结体而形成。 解决方案:制造铝复合材料的方法包括:形成和烧结铁质粉末的预成形步骤,以获得具有50%至70%的含铁粉末的多孔铁质烧结材料的预制体,占据体积 百分比,以及复合材料形成步骤,将在预热温度为300℃至400℃的预热体在真空中,惰性气体气氛,还原气体气氛或混合气体气氛中放置的预成型体 惰性气体和还原气体,在保持在200℃至400℃的温度下的铸模中,然后用熔融的铝或铝合金将预成形体压制浸渍,通过两步压制方法将其浇铸,包括 第一按压步骤和第二按压步骤。 版权所有(C)2007,JPO&INPIT