Abstract:
The present invention relates to a process for drying particulate polymers, comprising the steps of: a) providing a particulate polymer comprising from 60 wt % to 90 wt % of at least one solvent based on the total weight of particulate polymer and solvent, b) mechanically predrying the particulate polymer to a content of the at least one solvent of from 20 wt % to 50 wt % based on the total weight of particulate polymer and solvent, wherein the mechanical predrying in step b) is carried out with a roller press, and c) end-drying the particulate polymer to a content of the at least one solvent of from 0 wt % to 15 wt % based on the total weight of particulate polymer and solvent, wherein the particulate polymer is a polymer comprising repeating units of formulae I, II and/or III The present invention further relates to a process for working up particulate polymers.
Abstract:
A process for producing a melamine-formaldehyde foam by heating and foaming an aqueous mixture M using microwave radiation, said mixture M comprising at least one melamine-formal-dehyde precondensate, at least one curative, at least one surfactant, at least one blowing agent and at least one linear polymer with a number average molecular weight Mn in the range from 500 to 10.000 g/mol and at least two functional groups selected from OH, NH2 or COOH as well as a melamine-formaldehyde foam obtainable by this process and its use.
Abstract:
Process for producing polyarylene ether beads from a polyarylene ether solution, comprising the steps of i) dividing the polyarylene ether solution into droplets, ii) transferring the droplets into a precipitation bath to form polyarylene ether beads in the precipitation bath which (A) comprises at least one aprotic solvent (component (1)) and at least one protic solvent (component (2)), (B) has a temperature of 0° C. to Tc, where the critical temperature Tc in [° C.] can be determined by the numerical equation Tc=(99−c)/0.61 in which c is the concentration of component (1) in the precipitation bath in [% by weight] and (C) has component (1) in concentrations of 5% by weight to cc, where the critical concentration cc in [% by weight] can be determined by the numerical equation cc=99−0.61*T in which T is the temperature in the precipitation bath in [° C], where the percentages by weight are each based on the sum of the percentages by weight of component (1) and of component (2) in the precipitation bath.
Abstract:
Process for producing polyarylene ether beads from a polyarylene ether solution, comprising the steps of i) dividing the polyarylene ether solution into droplets, ii) transferring the droplets into a precipitation bath to form polyarylene ether beads in the precipitation bath which (A) comprises at least one aprotic solvent (component (1)) and at least one protic solvent (component (2)), (B) has a temperature of 0° C. to Tc, where the critical temperature Tc in [° C.] can be determined by the numerical equation Tc=(77−c)/0.58 in which c is the concentration of component (1) in the precipitation bath in [% by weight] and (C) has component (1) in concentrations of 5% by weight to cc, where the critical concentration cc in [% by weight] can be determined by the numerical equation cc=77−0.58*T in which T is the temperature in the precipitation bath in [° C.], where the percentages by weight are each based on the sum of the percentages by weight of component (1) and of component (2) in the precipitation bath.
Abstract:
The invention relates to a process for producing polyarylene ether beads from a polyarylene ether solution, comprising the steps of i) dividing the polyarylene ether solution in a division apparatus which is made to vibrate with a frequency of 10 to 1400 Hz to obtain droplets, ii) transferring the droplets into a precipitation bath to form polyarylene ether beads in the precipitation bath which (A) comprises at least one aprotic solvent (component (1)) and at least one protic solvent (component (2)), (B) has a temperature of 0° C. to Tc, where the critical temperature Tc in [° C.] can be determined by the numerical equation Tc=(77−c)/0.58 in which c is the concentration of component (1) in the precipitation bath in [% by weight] and (C) has component (1) in concentrations of 5% by weight to cc, where the critical concentration cc in [% by weight] can be determined by the numerical equation cc=77−0.58*T in which T is the temperature in the precipitation bath in [° C.], where the percentages by weight are each based on the sum of the percentages by weight of component (1) and of component (2) in the precipitation bath.
Abstract:
The present invention relates to a polymerizable lactam composition comprising at least one polymerizable lactam and at least one polaryl sulfone. The present invention further relates to a method of using the polymerizable lactam composition in the manufacture of polyamides and/or polyamide moldings.