CHLOROPRENE POLYMER COMPOSITION, DIP-MOLDED ARTICLE, AND METHOD FOR PRODUCING SAID COMPOSITION AND ARTICLE

    公开(公告)号:US20240034862A1

    公开(公告)日:2024-02-01

    申请号:US18256692

    申请日:2021-10-01

    CPC classification number: C08L9/00 C08J5/02

    Abstract: A method for producing a chloroprene polymer composition containing a chloroprene polymer, the method including: a polymerization step of polymerizing a monomer containing chloroprene at a polymerization rate of 20% or more to obtain a polymer composition containing a chloroprene polymer; and a mixing step of mixing the polymer composition with a rosin containing at least one conjugate resin acid component selected from the group consisting of abietic acid, neoabietic acid, palustric acid, levopimaric acid, and salts thereof, in which a mixed amount of the rosin in the mixing step is more than 0 parts by mass and 23 parts by mass or less with respect to 100 parts by mass of solid content of the polymer composition.

    CHLOROPRENE-BASED BLOCK COPOLYMER, LATEX, LATEX COMPOSITION, AND RUBBER COMPOSITION

    公开(公告)号:US20230074040A1

    公开(公告)日:2023-03-09

    申请号:US17788994

    申请日:2021-03-22

    Abstract: A chloroprene-based block copolymer, a latex, a latex composition, and a rubber composition that can produce a product with excellent tensile properties and flexibility without the use of a vulcanizing agent or a vulcanizing accelerator having a chloroprene-based block copolymer, contains 5 to 30% by mass of a polymer block (A) and 70 to 95% by mass of a chloroprene-based polymer block (B), wherein the polymer block (A) is derived from a monomer, when the monomer is polymerized alone, a polymer with a glass transition temperature of 80° C. or higher can be obtained and the chloroprene-based polymer block (B) includes a chloroprene monomer unit and a polyfunctional monomer unit.

    CHLOROPRENE-BASED BLOCK COPOLYMER, LATEX, LATEX COMPOSITION, AND RUBBER COMPOSITION

    公开(公告)号:US20230055361A1

    公开(公告)日:2023-02-23

    申请号:US17788958

    申请日:2021-03-22

    Abstract: A chloroprene-based block copolymer, a latex, a latex composition, and a rubber composition that can produce a product with excellent flexibility and tensile properties without the use of a vulcanizing agent or a vulcanizing accelerator. A chloroprene-based block copolymer, includes 5 to 30% by mass of a polymer block (A) and 70 to 95% by mass of a chloroprene-based polymer block (B), wherein: the polymer block (A) is derived from a monomer; when the monomer is polymerized alone, a polymer with a glass transition temperature of 80° C. or higher can be obtained; the chloroprene-based polymer block (B) includes a chloroprene monomer; and the chloroprene-based block copolymer has a toluene insoluble content of 20 to 100% by mass with respect to 100% by mass of the chloroprene-based block copolymer.

    CHLOROPRENE-BASED BLOCK COPOLYMER LATEX

    公开(公告)号:US20230050436A1

    公开(公告)日:2023-02-16

    申请号:US17788950

    申请日:2021-03-22

    Abstract: A chloroprene-based block copolymer latex, including a chloroprene-based block copolymer, wherein: the chloroprene-based block copolymer contains 5 to 30% by mass of a polymer block (A) and 70 to 95% by mass of a chloroprene-based polymer block (B); the polymer block (A) is derived from a monomer; when the monomer is polymerized alone, a polymer with a glass transition temperature of 80° C. or higher can be obtained; the chloroprene-based polymer block (B) includes a chloroprene monomer unit; and when the chloroprene-based block copolymer latex is molded by immersion molding to obtain a film and then the film is heat-treated at 130° C. for 30 minutes, a tensile strength at break measured in accordance with JIS K6251 of the film is 17 MPa or more is provided.

    DIP-MOLDED ARTICLE
    7.
    发明申请

    公开(公告)号:US20230025987A1

    公开(公告)日:2023-01-26

    申请号:US17788782

    申请日:2021-03-22

    Abstract: An immersion-molded body, wherein: the immersion-molded body is obtained using a latex; the latex comprises a chloroprene-based block copolymer; the chloroprene-based block copolymer contains 5 to 30% by mass of a polymer block (A) and 70 to 95% by mass of a chloroprene-based polymer block (B); the polymer block (A) is derived from a monomer; when the monomer is polymerized alone, a polymer with a glass transition temperature of 80° C. or higher can be obtained; the chloroprene-based polymer block (B) includes a chloroprene monomer unit; and when the immersion-molded body is heat-treated at 130° C. for 30 minutes, a tensile strength at break of the heat-treated immersion-molded body measured in accordance with JIS K6251 is 17 MPa or more.