摘要:
[Object] To provide a wire-harness use composite wire having a further improved corrosion resistance, while having excellent conductivity and strength. [Solving means] A wire-harness use composite wire comprising a first element wire which comprises 0.01-0.25 mass % C, 0.01-0.25 mass % N, 0.5-4.0 mass % Mn, 16-20 mass % Cr, 8.0-14.0 mass % Ni, and the balance of Fe and impurities and satisfies that a C+N content is in the range of 0.15 mass %≦C+N≦0.30 mass %, and a second element wire comprising at least one material selected from the group consisting of copper, copper alloy, aluminum, and aluminum alloy, the first element wire and the second element wire being twisted together.
摘要翻译:提供具有进一步改善的耐腐蚀性的线束使用复合线,同时具有优异的导电性和强度。 [解决方案]一种线束用复合线,其包括第一元素线,其包含0.01-0.25质量%的C,0.01-0.25质量%的N,0.5-4.0质量%的Mn,16-20质量%的Cr,8.0-14.0质量% %Ni,余量为Fe和杂质,并且满足C + N含量在0.15质量%<= C + N <= 0.30质量%的范围内,并且第二元素丝包括至少一种选自 由铜,铜合金,铝和铝合金组成的组,第一元件线和第二元素线被扭曲在一起。
摘要:
A high-strength steel wire for heat-resistant springs has both excellent high-temperature tensile strength and excellent high-temperature sag resistance at a temperature as high as 350 to 500° C., particularly at 400° C. or so (these properties are needed for spring materials). The steel wire contains (a) 0.01 to 0.08 wt % C, 0.18 to 0.25 wt % N, 0.5 to 4.0 wt % Mn, 16 to 20 wt % Cr, and 8.0 to 10.5 wt % Ni, (b) at least one constituent selected from the group consisting of 0.1 to 3.0 wt % Mo, 0.1 to 2.0 wt % Nb, 0.1 to 2.0 wt % Ti and 0.3 to 2.0 wt % Si, and (c) mainly Fe and unavoidable impurities both of which constitute the remainder. The steel wire has (a) a tensile strength of at least 1,300 N/mm2 and less than 2,000 N/mm2 before being treated with low-temperature annealing, and (b) a maximum crystal-grain diameter of less than 12 μm in the γ phase (austenite) in a transverse cross section of the wire.
摘要翻译:用于耐热弹簧的高强度钢丝线在350至500℃的温度下,特别是在400℃左右,具有优异的高温拉伸强度和优异的耐高温下垂性(这些性能 需要弹簧材料)。 钢丝包含(a)0.01〜0.08重量%的C,0.18〜0.25重量%的N,0.5〜4.0重量%的Mn,16〜20重量%的Cr和8.0〜10.5重量%的Ni,(b) 选自由0.1至3.0重量%的Mo,0.1至2.0重量%的Nb,0.1至2.0重量%的Ti和0.3至2.0重量%的Si组成的组,以及(c)主要为构成剩余部分的Fe和不可避免的杂质。 钢丝在用低温退火处理之前具有(a)至少1300N / mm 2以上且小于2000N / mm 2的拉伸强度,以及 (b)线的横截面中γ相(奥氏体)中的最大晶粒直径小于12μm。
摘要:
There are provided a lightweight insulated electric wire capable of reducing influences of external magnetic fields while having an excellent conductivity and an excellent strength and an automobile wire harness using the same insulated electric wire. There is provided a signal electric wire including a conductor portion consisting of one or more first wires and one or more second wires, which are stranded together. The first wires are constituted by metal wires made from at least one type of metal selected from a group consisting of copper, copper alloy, aluminum and aluminum alloy. The second wires are constituted by metal wires different from the first wires and have a relative permeability of 4.0 or less. By setting the relative permeability of the constituent wires of the conductor portion to 4.0 or less, it is possible to suppress temperature rises caused by eddy current loses due to external magnetic fields, thus alleviating degradation of the insulation layer and poor insulation.
摘要:
An Ni-based or Ni—Co-based heat-resistant alloy wire excellent in resistance to sag at high temperatures ranging from 600 to 700° C., which excellent resistance is most suitable for spring materials. The heat-resistant alloy wire contains (a) 0.01 to 0.40 wt % C, 5.0 to 25.0 wt % Cr, and 0.2 to 8.0 wt % Al; (b) at least one constituent selected from the group consisting of 1.0 to 18.0 wt % Mo, 0.5 to 15.0 wt % W, 0.5 to 5.0 wt % Nb, 1,0 to 10.0 wt % Ta, 0.1 to 5.0 wt % Ti and 0.001 to 0.05 wt % B; (c) at least one constituent selected from the group consisting of 3.0 to 20.0 wt % Fe and 1.0 to 30.0 wt % Co; and (d) the remaining constituent consisting mainly of Ni and unavoidable impurities. The wire has (a) a tensile strength not less than 1,400 N/mm2 and less than 1,800 N/mm2, (b) an average crystal-grain diameter not less than 5 &mgr;m and less than 50 &mgr;m in a cross section, and (c) a crystal-grain aspect ratio (a major-axis/minor-axis ratio) of 1.2 to 10 in a longitudinal section.
摘要:
A wire-harness use composite wire comprising a first element wire which comprises 0.01-0.25 mass % C, 0.01-0.25 mass % N, 0.5-4.0 mass % Mn, 16-20 mass % Cr,8.0-14.0 mass % Ni, and the balance of Fe and impurities and satisfies that a C+N content is in the range of 0.15 mass %≦C+N≦0.30 mass %, and a second element wire comprising at least one material selected from the group consisting of copper, copper alloy, aluminum, and aluminum alloy, the first element wire and the second element wire being twisted together.
摘要翻译:一种线束用复合线,其包括第一元素线,其包含0.01-0.25质量%的C,0.01-0.25质量%的N,0.5-4.0质量%的Mn,16-20质量%的Cr,8.0-14.0质量%的Ni和 Fe和杂质的余量,并且满足C + N含量在0.15质量%<= C + N <= 0.30质量%的范围内,并且第二元素线包括选自由铜组成的组中的至少一种材料 铜合金,铝和铝合金,将第一元件线和第二元件线绞合在一起。
摘要:
Provided is a high-strength stainless steel spring exhibiting a good workability and having a high load characteristic. Thus, the high-strength stainless steel spring of the invention has an chemical component containing 0.04 to 0.08% by mass of C, 0.15 to 0.22% by mass of N, 0.3 to 2.0% by mass of Si, 0.5 to 3.0% by mass of Mn, 16 to 20% by mass of Cr, 8.0 to 10.5% by mass of Ni, 0.5 to 3.0% by mass of Mo, and the balance of Fe and inevitable impurities, and when the average diameter of the coil is represented by D and further the diameter of the steel wire is represented by d in the case that cross sections of the stainless steel wire are in a complete round form or the value obtained by subtracting the average coil diameter from the outer diameter of the coil is represented by d′ in the case that the cross sections of the stainless steel wire are in a form other than the complete round form, the spring has a spring index D/d or D/d′ of 2 to 6.
摘要:
Provided is a high-strength stainless steel spring exhibiting a good workability and having a high load characteristic. Thus, the high-strength stainless steel spring of the invention has an chemical component containing 0.04 to 0.08% by mass of C, 0.15 to 0.22% by mass of N, 0.3 to 2.0% by mass of Si, 0.5 to 3.0% by mass of Mn, 16 to 20% by mass of Cr, 8.0 to 10.5% by mass of Ni, 0.5 to 3.0% by mass of Mo, and the balance of Fe and inevitable impurities, and when the average diameter of the coil is represented by D and further the diameter of the steel wire is represented by d in the case that cross sections of the stainless steel wire are in a complete round form or the value obtained by subtracting the average coil diameter from the outer diameter of the coil is represented by d′ in the case that the cross sections of the stainless steel wire are in a form other than the complete round form, the spring has a spring index D/d or D/d′ of 2 to 6.
摘要:
A lightweight insulated electric wire and an automobile wire harness using the same insulated electric wire where the insulated electric wire has a conductor portion including one or more first wires and one or more second wires, which are stranded together. The first wires are constituted by metal wires made from at least one type of metal selected from copper, copper alloy, aluminum and aluminum alloy. The second wires are constituted by metal wires different from the first wires and have a relative permeability of 4.0 or less.
摘要:
There is provided a stainless steel wire having both excellent corrosion resistance and an excellent fatigue strength while being fabricable with high productivity. A stainless steel wire consists of 0.01 to 0.25 mass % C, 0.01 to 0.25 mass % N, 0.4 to 4.0 mass % Mn, 16 to 25 mass % Cr, 8.0 to 14.0% Ni and the balance Fe with impurities, wherein the C+N content satisfies 0.15 mass % ≦C+N ≦0.35 mass %. The stainless steel wire contains 15 vol. % martensite phase induced by a drawing and the balance austenite phase and has a texture which causes the austenite phase to exhibit diffraction intensities satisfying both I(200)/I(111)≧2.0 and I(220)/I(111)≧3.0 by X-ray diffraction in the longitudinal direction of the steel wire.
摘要翻译:提供了具有优异的耐腐蚀性和优异的疲劳强度的不锈钢丝,同时可高生产率地制造。 不锈钢丝由0.01〜0.25质量%的N,0.01〜0.25质量%的N,0.4〜4.0质量%的Mn,16〜25质量%的Cr,8.0〜14.0%的Ni,余量的Fe与杂质组成,其中C + N含量满足0.15质量%<= C + N <= 0.35质量%。 不锈钢丝包含15卷。 通过拉伸和平衡奥氏体相诱导的马氏体相,并且具有使奥氏体相呈现满足I(200)/ I(111)> = 2.0和I(220)/ I(111)>的衍射强度的织构。 = 3.0,通过X线衍射在钢丝的纵向上。
摘要:
A steel wire of pearlite structure containing 0.8-1.0 mass % of C and 0.8-1.5 mass % of Si is disclosed. In the cross section of the steel wire the average hardness in a region up to 100 &mgr;m from the surface thereof is at least 50 higher that that in a deeper region based on micro-Vickers hardness. The steel wire is manufactured by working a wire rod having the abovementioned chemical composition through shaving, patenting and drawing processes, then strain-relief annealing the resultant wire, and thereafter subjecting the thus annealed wire to a short peening process. The steel wire can be produced through a drawing process without applying a quenching and tempering process, and are superior in heat resistance and fatigue strength.