摘要:
A metal-bonding adhesive composition consisting essentially of 95 - 60% by weight, based on the total composition, of an aliphatic homopolyamide and 5 - 40% by weight, based on the total composition, of an aliphatic copolyamide, said homopolyamide being a crystalline homopolyamide having up to 14 amide groups per 100 carbon atoms, and said copolyamide consisting of 90 - 70% by weight of (1) a polyamide having up to 14 amide groups per 100 carbon atoms and 10 - 30% by weight of (2) at least one polyamide whose recurring units are different from those of said polyamide (1), and a metallic can body composed of a metal blank, both side end portions of which are bonded by the side-lap-seam interposed by a layer of said adhesive composition.
摘要:
An adhesive composition for bonding together metal sheets in an extremely short time, which is an intimate mixture of (I) nylon 66, nylon 6, nylon 610, nylon 11 or nylon 12 and (II) a semicrystalline copolyamide such as a copolyamide of hexamethylene diammonium adipate, hexamethylene diammonium sebacate and 6-amino-caproic acid, in a ratio by weight of (I):(II) from 99:1 to 90:10.
摘要:
A hardened surface layer is formed in the region of inner and outer surfaces of a hollow material having a central through hole, then the hollow material is hot-forged into a hollow gear-like forged body by a forging die having a first die element with a piercing punch entering into the central through hole of the hollow material from one side thereof and having a second die element with a piercing punch entering into the central through hole of the hollow material from another side thereof. The forging die forms teeth of the gear on the outer side of the hollow material while producing an annular flash in the central through hole of the hollow material between the piercing punches. A distance between the piercing punches in a closed condition of the forging die defines a thickness of the annular flash which is 0.3 mm or more and no greater than 1.3 times (130%) of a depth of the hardened surface layer. After that, the annular flash is removed from the forged body, and thermal refining is implemented to the forged body by quenching and tempering.