Abstract:
This semiconductor wafer surface protection film has a substrate layer A, an adhesive absorption layer B, and adhesive surface layer C, in the stated order. The adhesive absorption layer B comprises an adhesive composition containing a thermoset resin b1, said adhesive absorption layer B having a minimum value G′bmin of the storage elastic modulus G′b in the range of 25° C. to less than 250° C. of 0.001 MPa to less than 0.1 MPa, a storage elastic modulus G′b250 at 250° C. of 0.005 MPa or above, and a temperature at which G′bmin is exhibited of 50-150° C. The adhesive surface layer C has a minimum value G′cmin of the storage elastic modulus G′c in the range of 25° C. to less than 250° C. of 0.03 MPa.
Abstract:
An adhesive resin composition of the present invention includes an expandable sticky polymer having a structure derived from a Meldrum's acid derivative, or a Meldrum's acid derivative represented by the following general formula (1) and an adhesive resin.
Abstract:
An adhesive resin composition includes an expandable sticky polymer having a structure derived from a Meldrum's acid derivative, or a Meldrum's acid derivative represented by the following general formula (1) and an adhesive resin.
Abstract:
Provided is a method of producing an electronic device, including a step of preparing a structure which includes an electronic component having a circuit forming surface, and an adhesive laminated film which includes a base material layer, an unevenness-absorptive resin layer, and an adhesive resin layer in this order and in which the adhesive resin layer is attached to the circuit forming surface of the electronic component such that the circuit forming surface is protected; and a step of forming an electromagnetic wave-shielding layer on the electronic component in a state of being attached to the adhesive laminated film.