公开(公告)号:US20230294347A1
公开(公告)日:2023-09-21
申请号:US18324120
申请日:2023-05-25
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Wen-Cheng YANG , TE-CHAO LIAO , HAO-SHENG CHEN , Chien-Chih LIN
CPC classification number: B29C48/19 , B29C48/40 , B29B7/14 , C08J3/22 , B32B27/08 , B32B27/20 , B32B27/36 , B29K2067/00
Abstract: A method for producing a polyester film is provided. The method includes a resin alloy master batch preparation step and a film forming step. The resin alloy master batch preparation step includes melting and kneading a high temperature resistant resin material and a polyester resin material with a twin-screw granulator, and then forming a plurality of resin alloy master batches. In the resin alloy master batch preparation step, a twin-screw temperature of the twin-screw granulator is between 250° C. and 320° C., and a twin-screw rotation speed of the twin-screw granulator is between 300 rpm and 800 rpm. The film forming step includes melting and extruding the resin alloy master batches with to form a polyester film. The polyester film includes a heat resistant layer formed of the plurality of resin alloy master batches so that the heat resistant layer includes the high temperature resistant resin material and the polyester resin material.
-
公开(公告)号:US20200216661A1
公开(公告)日:2020-07-09
申请号:US16238661
申请日:2019-01-03
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao LIAO , Wen-Cheng YANG , Chun-Che TSAO , Chia-Yen HSIAO , Chih-Feng WANG
Abstract: A white polyester film, having a specific weight of 0.6-1.2, being a three-layered structure containing two outer layers (A) having a combined thickness taking up 2% to 30% of an overall thickness of the film and a middle layer (B), and having air-bubble cells in both the outer layers (A) and the middle layer (B), has the outer layers (A) formed from a polyester resin and inorganic particles; and has the middle layer (B) having a heat distortion temperature above 120° C. and a melt flow index (MI) of 0.2-1 g/10 min (at 230° C., with a load of 2.16 kg) via crosslinking modified with 0.1-3 PHR of phrperoxide, and inorganic particles.
-
公开(公告)号:US20210253809A1
公开(公告)日:2021-08-19
申请号:US17034279
申请日:2020-09-28
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao LIAO , Wen-Cheng YANG , Wen-Jui CHENG , Chia-Yen HSIAO
Abstract: A low shrinkage low oligomer polyester film and a method for manufacturing the same are provided. The method includes forming at least one polyester composition into an unstretched polyester thick film and stretching the unstretched polyester thick film in a machine direction (MD) and a transverse direction (TD) at a stretch ratio of two to six times. The polyester composition includes 94% to 99.974% by weight of a polyester resin, 0.01% to 1% by weight of a primary antioxidant, 0.01% to 1% by weight of a secondary antioxidant, 0.003% to 2% by weight of a nucleating agent, and 0.003% to 2% by weight of a flow aid. The polyester resin has an intrinsic viscosity between 0.60 dl/g and 0.80 dl/g.
-
-