公开(公告)号:US20160067686A1
公开(公告)日:2016-03-10
申请号:US14786209
申请日:2014-04-22
Applicant: SHELL OIL COMPANY
Inventor: Ali AZGHAY , Marcello Stefano RIGUTTO
CPC classification number: B01J27/19 , B01J37/0213 , B01J37/0236 , B01J37/20 , C10G45/08
Abstract: The invention provides a process for preparing a sulphided catalyst comprising the steps of (a) treating a catalyst carrier with one or more Group VIB metal components, one or more Group VIII metal components and a glycolic acid ethoxylate ether compound according to the formula (I) R—(CH2)x—CH2—O—[—(CH2)2—O—]m—CH2—COOH (I) wherein R is a hydrocarbyl group containing of from 5 to 20 carbon atoms, x is in the range of from 1 to 15, and m is in the range of from 1 to 10, and wherein the molar ratio of compound (I) to the Group VIB and Group VIII metal content is at least 0.01:1 to 1:0.01; (b) drying the treated catalyst carrier at a temperature of at most 200° C. to form a dried impregnated carrier; and (c) sulphiding the dried impregnated carrier to obtain a sulphided catalyst.
Abstract translation: 本发明提供了一种制备硫化催化剂的方法,包括以下步骤:(a)用一种或多种VIB族金属组分,一种或多种VIII族金属组分和根据式(I)的乙醇酸乙氧基化醚化合物处理催化剂载体 )R-(CH 2)x -CH 2 -O - [ - (CH 2)2 -O-] m -CH 2 -COOH(I)其中R是含有5至20个碳原子的烃基,x在 为1〜15,m为1〜10,化合物(I)与VIB族和Ⅷ族金属含量的摩尔比为0.01:1〜1:0.01以上。 (b)在至多200℃的温度下干燥经处理的催化剂载体以形成干燥的浸渍载体; 和(c)硫化干燥的浸渍载体以获得硫化催化剂。
-
2.
公开(公告)号:US20160045910A1
公开(公告)日:2016-02-18
申请号:US14779673
申请日:2014-03-28
Applicant: SHELL OIL COMPANY
Inventor: Ali AZGHAY , Patricia Johanna Anne Maria GILTAY , Marcello Stefano RIGUTTO , Arend Jan VAN WELSENES , Ferry WINTER
CPC classification number: B01J38/62 , B01J23/882 , B01J23/94 , B01J27/0515 , B01J37/20 , B01J38/12 , B01J38/48 , C10G45/08 , C10G65/00 , C10G2300/70
Abstract: The invention provides a process for rejuvenation of a used hydrotreating catalyst comprising at least 8% wt of coke and one or more non-noble Group VIII and/or Group VIb metals, which process comprises the steps of: (i) removing coke from the used hydrotreating catalyst; and (ii) treating the catalyst obtained in step (i) with of from 2 to 60% wt of gluconic acid, based on weight of dry catalyst.
Abstract translation: 本发明提供了一种使用的加氢处理催化剂的再生方法,其包含至少8重量%的焦炭和一种或多种非贵金属VIII族和/或VIb族金属,该方法包括以下步骤:(i) 使用加氢处理催化剂; 和(ii)以干燥催化剂的重量,用2-60重量%的葡萄糖酸处理步骤(ⅰ)中获得的催化剂。
-
公开(公告)号:US20160271594A1
公开(公告)日:2016-09-22
申请号:US15033926
申请日:2014-11-04
Applicant: SHELL OIL COMPANY
Inventor: Ferry WINTER , Jen Arend VAN WELSENES , Marcello Stefano RIGUTTO , Patricia Johanna Anne Maria GILTAY , Johannes Jacobus Maria VAN VLAANDEREN , Ali AZGHAY
CPC classification number: B01J27/19 , B01J21/04 , B01J23/883 , B01J31/0202 , B01J31/04 , B01J35/0006 , B01J35/0026 , B01J35/026 , B01J35/1019 , B01J35/1061 , B01J37/0018 , B01J37/0201 , B01J37/0203 , B01J37/0205 , B01J37/0207 , B01J37/0215 , B01J37/0236 , B01J37/024 , B01J37/08 , B01J37/086 , B01J37/088 , B01J37/20 , B01J37/28 , B01J2523/00 , C10G45/08 , B01J2523/31 , B01J2523/51 , B01J2523/68 , B01J2523/845 , B01J2523/847
Abstract: Process for preparing a hydrotreating catalyst comprising of from 5 wt % to 50 wt % of molybdenum, of from 0.5 wt % to 20 wt % of cobalt, and of from 0 to 5 wt % of phosphorus, all based on total dry weight of catalyst, which process comprises (a) treating a nickel containing carrier with molybdenum, cobalt and of from 1 to 60% wt of gluconic acid, based on weight of carrier, and optionally phosphorus, (b) optionally drying the treated carrier at a temperature of from 40 to 200° C., and (c) calcining the treated and optionally dried carrier at a temperature of from 200 to 650° C. to obtain the calcined treated carrier.
Abstract translation: 制备加氢处理催化剂的方法,所述加氢处理催化剂包含5重量%至50重量%的钼,0.5重量%至20重量%的钴和0至5重量%的磷,均基于催化剂的总干重 ,该方法包括(a)基于载体的重量和任选的磷,用钼,钴和1至60重量%的葡萄糖酸处理含镍载体,(b)任选地在经处理的载体的温度 40℃至200℃,和(c)在200至650℃的温度下煅烧经处理和任选干燥的载体以获得经煅烧处理的载体。
-
公开(公告)号:US20160264879A1
公开(公告)日:2016-09-15
申请号:US15033927
申请日:2014-11-04
Applicant: SHELL OIL COMPANY
Inventor: Ferry WINTER , Jan Arend VAN WELSENES , Marcello Stefano RIGUTTO , Patricia Johanna Anne Maria GILTAY , Johannes Jacobus Maria VAN VLAANDEREN , Ali AZGHAY
CPC classification number: B01J27/19 , B01J21/04 , B01J23/883 , B01J31/0202 , B01J31/04 , B01J35/0006 , B01J35/0026 , B01J35/026 , B01J35/1019 , B01J35/1061 , B01J37/0018 , B01J37/0201 , B01J37/0203 , B01J37/0205 , B01J37/0207 , B01J37/0215 , B01J37/0236 , B01J37/024 , B01J37/08 , B01J37/086 , B01J37/088 , B01J37/20 , B01J37/28 , B01J2523/00 , C10G45/08 , B01J2523/31 , B01J2523/51 , B01J2523/68 , B01J2523/845 , B01J2523/847
Abstract: Process for preparing a hydrotreating catalyst comprising of from 5 wt % to 50 wt % of molybdenum, of from 0.5 wt % to 20 wt % of nickel and of from 0 to 5 wt % of phosphorus, all based on total dry weight of catalyst, which process comprises (a) treating alumina carrier with molybdenum and nickel and of from 1 to 60% wt of gluconic acid, based on weight of carrier, and op tionally phosphorus, (b) optionally drying the treated carrier at a temperature of from 40 to 200° C., and (c) calcining the treated and optionally dried carrier at a temperature of from 200 to 650° C. to obtain the calcined treated carrier.
Abstract translation: 制备加氢处理催化剂的方法,其包含5重量%至50重量%的钼,0.5重量%至20重量%的镍和0至5重量%的磷,均基于催化剂的总干重, 该方法包括(a)以钼和镍为原料处理氧化铝载体,以及基于载体的重量计,1至60重量%的葡萄糖酸,和磷酸作用,(b)任选地在40℃的温度下干燥经处理的载体 至200℃,和(c)在200-650℃的温度下煅烧经处理和任选干燥的载体以获得经煅烧处理的载体。
-
-
-