Abstract:
A substrate comprising a surface at least a portion of which is covered with an epilame agent, comprising at least one compound in the form of a copolymer comprising units M and units N, associated by covalent bonds via their main chains, where M is
N is
where R1 and R2, which may be identical or different, are H, a C1-C10 alkyl group, a C2-C10 alkenyl group; X and Y, which may be identical or different, are spacer arms consisting of a heteroatom or a linear or branched hydrocarbon chain containing at least one heteroatom and comprising at least one carbon atom; A, which may be identical or different, forms an anchoring group to the substrate; L, which may be identical or different, is a halogenated ether group according to formula (I)
where Q is a halogen atom; P, which may be identical or different, is a C1-C10 alkyl group or a C2-C10 alkenyl group comprising at least one halogen atom and being linear or branched; p is chosen between 1 and 4; and n is chosen between 1 and 20.
Abstract:
The present invention concerns an epilame-coated product including a substrate on which an epilame is deposited, characterized in that the product further includes an adhesion layer located between the substrate and having chemical affinity with said epilame.
Abstract:
The disclosure relates to a substrate comprising a surface at least part of which is coated with an epilamization agent, the epilamization agent including at least one compound in the form of a block copolymer comprising at least one block of M units linked by covalent bonds by their main chains, and at least one block of N units linked by covalent bonds by their main chains, the blocks being connected to each other by covalent bonds by their main chains in linear sequences, where M is a and N is
Abstract:
The invention relates to a method for epilamization of at least one portion of a substrate surface comprising the steps of: a) preparing an epilame agent b) optionally, preparing the substrate surface c) placing the substrate and the epilame agent in a chamber at ambient pressure d) introducing CO2 into the hermetically sealed chamber at a pressure comprised between 25 bar and 74 bar and at a temperature comprised between 10° C. and 80° C. for a duration comprised between 1 minute and 30 minutes, e) reducing the pressure in the chamber, and f) removing the epilamized substrate from the chamber.
Abstract:
A substrate including a surface, at least one part of which is coated with an epilamization agent including at least one compound in the form of a statistical copolymer comprising M units, N units and optionally at least one P unit, linked by covalent bonds by their main chains and randomly distributed, where M is N is P is