EXTENSIBLE ARTIFICIAL LEATHER AND METHOD FOR MAKING THE SAME
    92.
    发明申请
    EXTENSIBLE ARTIFICIAL LEATHER AND METHOD FOR MAKING THE SAME 有权
    可伸缩人造革及其制造方法

    公开(公告)号:US20080145613A1

    公开(公告)日:2008-06-19

    申请号:US11618960

    申请日:2007-01-02

    IPC分类号: D06N3/00 B05D5/00

    摘要: A method is provided for making extensible artificial leather. In the method, a substrate is supported on in-extensible woven cloth and locating the substrate firmly on a coating machine. Foamy highly solid-containing water-based polyurethane resin is coated on the substrate for forming a middle layer with tiny open cells. The middle layer is dried and the woven cloth is removed from the substrate. A superficial layer of polyurethane is attached to the middle layer in a dry process so that the extensible artificial leather is made with excellent strength against peeling, abrasion and dissolution.

    摘要翻译: 提供了制造可延展人造革的方法。 在该方法中,将基板支撑在可伸长的织布上并将基板牢固地定位在涂布机上。 将泡沫高固体含水的聚氨酯树脂涂覆在基材上,形成具有微小开孔的中间层。 中间层被干燥,织物从基材上除去。 在干燥过程中,中间层附着有表面的聚氨酯层,使得可伸长的人造革被制成具有优异的剥离,磨损和溶解强度。

    Method for Making Macromolecular Laminate
    93.
    发明申请
    Method for Making Macromolecular Laminate 审中-公开
    制备高分子层压板的方法

    公开(公告)号:US20080095945A1

    公开(公告)日:2008-04-24

    申请号:US11956857

    申请日:2007-12-14

    IPC分类号: B05D3/12

    CPC分类号: C08L75/04

    摘要: A method for making a macromolecular laminate is disclosed. Firstly, a high solid-content polyurethane resin is prepared. The high solid-content polyurethane resin has a solid content higher than 80% by weight and a viscosity from 20000 to 60000 cps/30° C. The high solid-content polyurethane resin is liquid at the room temperature. The high solid-content polyurethane resin is mixed with additives to form a first type of polyurethane resin compound with a solid content higher than 50% by weight and a viscosity from 20000 to 60000 cps/30° C. The first type of polyurethane resin compound is liquid at room temperature and has a pot life of at least three hours at room temperature. The first type of polyurethane resin compound is coated on a releasing paper to make a main layer. Then, the releasing paper is removed from the main layer to make a laminate.

    摘要翻译: 公开了制备高分子层压体的方法。 首先,制备高固含量聚氨酯树脂。 高固含量聚氨酯树脂的固含量高于80重量%,粘度为20000至60000cps / 30℃。高固含量聚氨酯树脂在室温下为液体。 将高固含量的聚氨酯树脂与添加剂混合以形成固体含量高于50重量%,粘度为20000至60000cps / 30℃的第一种聚氨酯树脂化合物。第一种类型的聚氨酯树脂化合物 在室温下为液体,在室温下具有至少3小时的适用期。 将第一种类型的聚氨酯树脂化合物涂覆在脱模纸上以制成主层。 然后,将脱模纸从主层移除以制成层压体。

    Luminary material and method for manufacturing the same
    94.
    发明授权
    Luminary material and method for manufacturing the same 失效
    照明材料及其制造方法

    公开(公告)号:US07361418B2

    公开(公告)日:2008-04-22

    申请号:US11444354

    申请日:2006-06-01

    IPC分类号: B32B9/00 B32B19/00

    摘要: The present invention relates to a luminary material comprising a substrate; a luminary layer formed on a surface of the substrate; and a surface layer comprising a first portion and a second portion, wherein the first portion allows stronger light to be emitted from the luminary layer than the second portion. The luminary material according to the invention exhibits various colors, patterns and/or textures formed on the surface. Therefore, the luminary material is qualified as a decorative material in the light. A method for manufacturing the luminary material is also provided.

    摘要翻译: 本发明涉及一种包含基底的发光材料; 形成在所述基板的表面上的发光层; 以及包括第一部分和第二部分的表面层,其中所述第一部分允许比所述第二部分从所述发光体层发射更强的光。 根据本发明的发光材料表现出形成在表面上的各种颜色,图案和/或纹理。 因此,灯光材料在光线中被认为是装饰材料。 还提供了用于制造照明材料的方法。

    METHOD OF PRODUCING ARTIFICIAL LEATHER AND ARTIFICIAL LEATHER
    95.
    发明申请
    METHOD OF PRODUCING ARTIFICIAL LEATHER AND ARTIFICIAL LEATHER 审中-公开
    生产人造革和人造革的方法

    公开(公告)号:US20080066848A1

    公开(公告)日:2008-03-20

    申请号:US11943656

    申请日:2007-11-21

    IPC分类号: D06N3/00 B32B5/20

    摘要: The present invention relates to a method of producing artificial leather, comprising steps of: (a) providing a substrate; (b) providing a foamed polyurethane dispersion, wherein the polyurethane dispersion has a solid content of about 40% to about 60% and a void content of about 0.01% to about 80%; (c) coating the substrate with a layer of the foamed polyurethane dispersion; and (d) drying the substrate and the layer of the foamed polyurethane dispersion for obtaining the artificial leather. Artificial leather is also provided in the present invention.

    摘要翻译: 本发明涉及一种生产人造革的方法,包括以下步骤:(a)提供基材; (b)提供泡沫聚氨酯分散体,其中聚氨酯分散体具有约40%至约60%的固体含量和约0.01%至约80%的空隙含量; (c)用一层泡沫聚氨酯分散体涂覆基材; 和(d)干燥基材和泡沫聚氨酯分散体层以获得人造革。 本发明也提供人造皮革。

    Sheet for mounting polishing workpiece and method for making the same

    公开(公告)号:US07316605B1

    公开(公告)日:2008-01-08

    申请号:US11478606

    申请日:2006-07-03

    IPC分类号: B24D11/00

    摘要: The present invention relates to a sheet for mounting a polishing workpiece. The sheet comprises a substrate and a surface layer. The substrate has a surface. The surface layer is located on the surface of the substrate, with no hole structure existing in the interior thereof, and has a plurality of through holes. Accordingly, when the polishing workpiece contacts the surface layer, the air therebetween is vented to the substrate via the through holes and then is easily vented out, without the phenomenon of air wrapping, which increases the adsorption force between the polishing workpiece and the sheet, thereby improving the polishing effect of the polishing workpiece.

    Method for producing environmental friendly artificial leather product
    98.
    发明申请
    Method for producing environmental friendly artificial leather product 审中-公开
    生产环保人造革产品的方法

    公开(公告)号:US20060249244A1

    公开(公告)日:2006-11-09

    申请号:US11486542

    申请日:2006-07-14

    IPC分类号: B44C1/17 B32B37/00

    CPC分类号: D06N3/0097 B44F9/12 D06N3/145

    摘要: A method for producing an environmental friendly artificial leather product includes coating a first solvent-free elastomer resin composition on a releasing paper to form a top layer, coating a polyurethane resin composition containing more than 50% by weight solid content on the top layer to form an intermediate layer, coating a second solvent-free elastomer resin composition on the intermediate layer to form an adhesive layer, and finally applying a substrate on the adhesive layer, and peeling the releasing paper.

    摘要翻译: 一种生产环保人造革制品的方法包括在脱模纸上涂布第一无溶剂弹性体树脂组合物以形成顶层,在顶层上涂覆含有多于50重量%固体含量的聚氨酯树脂组合物以形成 中间层,在中间层上涂布第二无溶剂弹性体树脂组合物以形成粘合剂层,最后在粘合剂层上涂布基材,剥离剥离纸。

    Elastic artificial leather
    100.
    发明申请
    Elastic artificial leather 审中-公开
    弹性人造革

    公开(公告)号:US20060057432A1

    公开(公告)日:2006-03-16

    申请号:US11106119

    申请日:2005-04-14

    摘要: Elastic artificial leather is disclosed. There are provided two polymers that include different crystallization degrees but similar fluidities. Fibers are made of the polymers. Non-woven cloth is made of the fibers. The non-woven cloth is soaked in water at 50 to 90° C. Thus, the fibers curl so that the non-woven cloth is elastic. The non-woven cloth is soaked in PU resin, washed and dried. Alternatively, the non-woven cloth includes, in addition to the fibers (“first type of fibers”), additional fibers (“second type of fibers”) that can be dissolved in water, alkali or solvent. The non-woven cloth is soaked in PU resin, washed and dried. The second type of fibers is removed from the non-woven cloth and the PU resin in order to leave elongated spaces. Thus, the artificial leather is elastic.

    摘要翻译: 公开了弹性人造革。 提供了两种聚合物,其包括不同的结晶度但具有类似的流动性。 纤维由聚合物制成。 无纺布由纤维制成。 将无纺布浸泡在50〜90℃的水中。因此,纤维卷曲,使得无纺布具有弹性。 将无纺布浸泡在PU树脂中,洗涤并干燥。 或者,除了纤维(“第一类纤维”)之外,无纺布还可以溶解在水,碱或溶剂中的附加纤维(“第二类纤维”)。 将无纺布浸泡在PU树脂中,洗涤并干燥。 从无纺布和PU树脂中除去第二种类型的纤维,以便留下细长的空间。 因此,人造革是弹性的。