Abstract:
A crosslinked metallocene-catalyzed polyethylene copolymer having a higher molecular weight (HMW) component and lower molecular weight (LMW) component wherein the HMW component is present in an amount of from about 10 wt. % to about 30 wt. % and wherein the LMW component is present in an amount of from about 70 wt. % to about 90 wt. %.
Abstract:
Disclosed herein are ethylene-based polymers having a density greater than 0.945 g/cm3, a high load melt index less than 25 g/10 min, a peak molecular weight ranging from 52,000 to 132,000 g/mol, and an environmental stress crack resistance of at least 250 hours. These polymers have the processability of chromium-based resins, but with improved impact strength and stress crack resistance, and can be used in large-part blow molding applications.
Abstract:
Disclosed herein are polymerization processes for the production of olefin polymers. These polymerization processes use a catalyst system containing three metallocene components, often resulting in polymers having a reverse comonomer distribution and a broad and non-bimodal molecular weight distribution.
Abstract:
Disclosed herein are ethylene-based polymers having a density greater than 0.945 g/cm3, a high load melt index less than 25 g/10 min, a peak molecular weight ranging from 52,000 to 132,000 g/mol, and an environmental stress crack resistance of at least 250 hours. These polymers have the processability of chromium-based resins, but with improved impact strength and stress crack resistance, and can be used in large-part blow molding applications.
Abstract:
Disclosed herein are polymerization processes for the production of olefin polymers. These polymerization processes can employ a catalyst system containing two or three metallocene components, resulting in ethylene-based copolymers that can have a medium density and improved stress crack resistance.
Abstract:
Disclosed herein are polymerization processes for the production of olefin polymers. These polymerization processes use a catalyst system containing three metallocene components, often resulting in polymers having a reverse comonomer distribution and a broad and non-bimodal molecular weight distribution.