摘要:
Thermoplastic moulding compositions based on polycarbonate and/or polyester-carbonate comprising graft polymer prepared by means of bulk, solution or bulk-suspension polymerization processes and phosphorus compounds of the general formula (I)
摘要:
The invention relates to flame-resistant poly-carbonate/ABS molding compounds which are considerably improved in their mechanical properties and thermal stability by an addition of polyalkylene terephthalate and an oligomeric phosphate.
摘要:
The present invention relates to moulding compositions which are treated with phosphazenes and are based on polycarbonate and graft polymers chosen from the group consisting of silicone rubbers, EP(D)M rubbers and acrylate rubbers as the graft base, and which have an excellent flameproofing and very good mechanical properties, such as resistance to stress cracking or notched impact strength.
摘要:
Thermoplastic polycarbonate/graft polymer moulding compositions containingA) 5 to 95 parts by weight of an aromatic polycarbonate,B) 1 to 50 parts by weight of at least one thermoplastic homopolymer, copolymer or terpolymer of styrene, .alpha.-methylstyrene, acrylonitrile, N-substituted maleimide or mixtures thereof,C) 1 to 50 parts by weight of at least one graft polymer ofC.1) 5 to 90 parts by weight of styrene, .alpha.-methylstyrene, acrylonitrile, N-substituted maleimide or mixtures thereof, onC.2) 95 to 10 parts by weight of a rubber with a glass transition temperature .ltoreq.0.degree. C. andD) 1 to 25 parts by weight (per 100 parts by weight A+B+C) of at least one additive selected from flame retardants, lubricants, antistatic agent, mould release agents or mixtures thereof,characterised in that the component B) is produced by bulk, solution or suspension polymerisation and has an oligomer content .ltoreq.1 wt. %, component C) is produced by emulsion polymerisation and the total oligomer content of the moulding compositions is .ltoreq.0.6 wt. %.
摘要翻译:含有A)5-95重量份的芳族聚碳酸酯的热塑性聚碳酸酯/接枝聚合物模塑组合物,B)1至50重量份的至少一种苯乙烯,α-甲基苯乙烯,丙烯腈,N-甲基苯乙烯的共聚物或三元共聚物, 取代的马来酰亚胺或其混合物,C)1至50重量份的至少一种C.1的接枝聚合物)C至5重量份的苯乙烯,α-甲基苯乙烯,丙烯腈,N-取代的马来酰亚胺或其混合物,在C .2)95至10重量份的玻璃化转变温度为0℃的橡胶和D)1至25重量份(每100重量份A + B + C)至少一种添加剂 选自阻燃剂,润滑剂,抗静电剂,脱模剂或其混合物,其特征在于组分B)通过本体,溶液或悬浮液聚合制备,并且具有低聚物含量为1重量%。 %,组分C)通过乳液聚合制备,并且模塑组合物的总低聚物含量为0.6重量%。 %。
摘要:
This invention relates to halogen-free flame retardant thermoplastic moulding compounds prepared from polycarbonate and graft polymer, which may contain thermoplastic copolymer and/or polyalkylene terephthalate, wherein the flame retardant used is polyphenylene oxide combined with phosphorus compounds.
摘要:
The present invention relates to polycyclic phosphoric acid esters of the formula (I) ##STR1## in which L is an n-valent linear or branched aliphatic hydrocarbon residue with 2 to 30 C atoms, which may be OH-substituted and may contain up to 8 ether linkages, Ar is an aryl residue or alkaryl residue and n is 2 to 6, to the use thereof as flame retardants in thermoplastics and to the thermoplastic moulding compounds.
摘要:
Thermoplastic molding compositions of A) 70 to 99.5% by weight of a thermoplastic aromatic polyether sulfone or mixtures of several thermoplastic polyether sulfones and B) 30 to 0.5% by weight of a hydrogenated nitrile rubber.
摘要:
The invention relates to high-impact polyether sulfone molding compositions containing aromatic polyether sulfones, diene graft polymers and, optionally, other thermoplastic resins, at most half the aromatic polyether sulfone being replaceable by other thermoplastic resins.
摘要:
A thermoplastic molding composition comprising (i) an aromatic polycarbonate having high thermal dimensional stability and based on a substituted dihydroxydiphenylcycloalkane, (ii) other aromatic polycarbonate resin and (iii) graft, particle-type diene rubbers is disclosed. The composition is characterized by its good Izod impact strength. A process for preparing the molding composition and their use for manufacturing molded bodies are also disclosed.
摘要:
Thermoplastic molding composition comprisingA. 5 to 99% by weight (based on A+B) of a polycarbonate based on substituted dihydroxydiphenyl cycloalkanesB. 1 to 95% by weight (based on A+B) of a graft polymer prepared by a special process of5 to 90 parts by weight of a mixture ofB.1.1. 50 to 95 parts by weight styrene, .alpha.-methyl styrene, C.sub.1-4 alkyl- or halogen-nucleus-substituted styrenes, C.sub.1-8 alkyl methacrylates, C.sub.1-8 alkyl acrylates or mixtures thereof andB.1.2. 5 to 50 parts by weight acrylonitrile, methacrylonitrile, C.sub.1-8 alkyl methacrylates, C.sub.1-8 alkyl acrylates, maleic anhydride, C.sub.1-4 alkyl-N-maleic imides, phenyl-N-maleic imides or mixtures thereof onB.2. 10 to 95 parts by weight of a diene rubber having an average particle diameter d50 of from 0.09 to 1 .mu.m and a gel content of more than 50% by weight and optionally at least one other thermoplastic resin which replaces up to 75% by weight of the polycarbonate A.