公开(公告)号:US20180265740A1
公开(公告)日:2018-09-20
申请号:US15983690
申请日:2018-05-18
Applicant: 3M INNOVATIVE PROPERTIES COMPANY
Inventor: Bert T. Chien , Christopher P. Gerlach , Gregory F. King , Peggy S. Willett , Christopher A. Haak , Ronald K. Thery
Abstract: Articles and laminates include a substrate with a first polyester surface and a second polyester surface, a crosslinked polyurethane-based primer coated on at least the first polyester surface, and an optically clear heat activated adhesive adjacent to the crosslinked polyurethane-based primer. The articles and laminates are prepared by applying a polyurethane-based dispersion and a crosslinker on at least one polyester surface, drying the applied coating, heating while stretching the substrate and the coating to form a crosslinked primer layer on the stretched polyester surface, and applying an optically clear heat activated adhesive onto the crosslinked primer layer.
-
12.
公开(公告)号:US20240280737A1
公开(公告)日:2024-08-22
申请号:US18650643
申请日:2024-04-30
Applicant: 3M INNOVATIVE PROPERTIES COMPANY
Inventor: Nicholas C. Erickson , David G. Freier , Robert L. Brott , Bing Hao , David A. Rosen , Stephen M. Menke , Bert T. Chien , Seong Taek Lee , Encai Hao , Zhaohui Yang , Albert I. Everaerts , Yongshang Lu , William Blake Kolb , Keith R. Bruesewitz , Adam D. Haag , Sun-Yong Park , Timothy J. Nevitt (Deceased) , Brianna N. Wheeler , Jody L. Peterson , Gilles J. Benoit
Abstract: An organic light emitting diode (OLED) display includes a pixelated OLED display panel and a color-correction component disposed on the pixelated OLED display panel. The pixelated OLED display panel has a ratio of blue-to-red color mixing weights at 30 degrees of β030, and a ratio of blue-to-red color mixing weights at 45 degrees of β045, where β045≥β030≥1.05 and 1.5≥β045≥1.1. The color-correction component is configured such that a ratio of blue-to-red color mixing weights at 45 degrees of the display is β45 and a ratio of blue-to-red color mixing weights at 30 degrees of the display is β30, where β045−0.1≥β45≥2.1−β045 and β030−0.05≥β30≥2.05−β030. Methods of making OLED displays are described.
-
公开(公告)号:US20240168204A1
公开(公告)日:2024-05-23
申请号:US18279267
申请日:2022-03-10
Applicant: 3M INNOVATIVE PROPERTIES COMPANY
Inventor: Bert T. Chien , William B. Kolb , Tri D. Pham , Daoyun Song , Daniel K. Bruesewitz , Stephen P. Maki , James A. Phipps , Jonah Shaver , Zhaohui Yang
CPC classification number: G02B5/005 , G02B5/003 , G06F3/0421 , G02B2207/123
Abstract: An optical construction includes a lens film having a plurality of optically transparent first beads at least partially embedded in a first layer. A light blocking second layer is disposed on the lens film and defines a plurality of through openings therein extending at least partially between opposite major top and bottom surfaces of the second layer. The through openings are aligned to the first beads in a one-to-one correspondence.
-
14.
公开(公告)号:US20210294002A1
公开(公告)日:2021-09-23
申请号:US17250318
申请日:2019-07-18
Applicant: 3M INNOVATIVE PROPERTIES COMPANY
Inventor: Mark B. O'Neill , Gary E. Gaides , Tri D. Pham , Aaron K. Nienaber , Ronald D. Jesme , Joseph B. Eckel , Shawn C. Dodds , Bert T. Chien
Abstract: According to one embodiment, a method of making an optical film for control of light comprising: positioning a first mixture on a substrate, wherein the first mixture comprises a first plurality of magnetizable particles dispersed in a first resin, assembling the first plurality of magnetizable particles into a desired structure for the control of the light by rotating modulation of at least a first magnetic field relative to the first plurality of magnetizable particles, and vitrifying the first resin while the first plurality of magnetizable particles are in the desired structure.
-
公开(公告)号:US20150044456A1
公开(公告)日:2015-02-12
申请号:US14375146
申请日:2013-01-28
Applicant: 3M INNOVATIVE PROPERTIES COMPANY
Inventor: Bert T. Chien , Christopher P. Gerlach , Gregory F. King , Peggy S. Willett , Christopher A. Haak , Ronald K. Thery
CPC classification number: C09J7/255 , B32B7/12 , B32B17/064 , B32B17/10 , B32B17/10036 , B32B17/10688 , B32B17/10761 , B32B17/10779 , B32B33/00 , B32B2250/02 , B32B2250/03 , B32B2250/40 , B32B2255/10 , B32B2255/26 , B32B2315/08 , B32B2367/00 , B32B2405/00 , B32B2419/00 , C08G18/0823 , C08G18/10 , C08G18/12 , C08G18/348 , C08G18/4808 , C08G18/4825 , C08G18/6692 , C08G18/758 , C09D175/08 , C09J7/50 , C09J2201/606 , C09J2201/61 , C09J2467/006 , C09J2475/003 , C09J2475/006 , G02B1/04 , Y10T428/2826 , Y10T428/31565 , C08L33/26 , C08L75/04 , C08G18/3228 , C08G18/3851 , C08G18/8061
Abstract: Articles and laminates include a substrate with a first polyester surface and a second polyester surface, a crosslinked polyurethane-based primer coated on at least the first polyester surface, and an optically clear heat activated adhesive adjacent to the crosslinked polyurethane-based primer. The articles and laminates are prepared by applying a polyurethane-based dispersion and a crosslinker on at least one polyester surface, drying the applied coating, heating while stretching the substrate and the coating to form a crosslinked primer layer on the stretched polyester surface, and applying an optically clear heat activated adhesive onto the crosslinked primer layer.
Abstract translation: 制品和层压材料包括具有第一聚酯表面和第二聚酯表面的基材,涂覆在至少第一聚酯表面上的交联的聚氨酯基底漆和邻近交联的聚氨酯基底漆的光学透明热活化粘合剂。 通过将聚氨酯基分散体和交联剂涂布在至少一个聚酯表面上,干燥所涂覆的涂层,同时拉伸基材和涂层进行加热,并在拉伸的聚酯表面上形成交联的底漆层,并施加 光学透明的热活化粘合剂到交联底漆层上。
-
-
-
-