公开(公告)号:US10391694B2
公开(公告)日:2019-08-27
申请号:US15108136
申请日:2014-12-22
Applicant: Kaneka Corporation
Inventor: Keisuke Hatano , Yutaka Fujiwara
IPC: B29D11/00 , B29C47/14 , B29C48/30 , B29C48/305 , B29C48/08 , B29C48/00 , C08J5/18 , B29K21/00 , B29K101/12 , B29K105/16 , B29L7/00 , B29L11/00 , B29K421/00
Abstract: Disclosed herein is a method of producing a film, the method being capable of suppressing formation of die lines in melt extrusion molding using a T die. A thermoplastic resin composition having a relaxation modulus of not less than 100 Pa and not more than 2,000 Pa is melted and kneaded, the relaxation modulus being measured under conditions of a temperature of 260° C., distortion of 1%, and a relaxation time of 1 second, and extrusion molding of the thermoplastic resin composition using the T die is performed to form the film. The thermoplastic resin composition may contain an acrylic resin and a rubber particle.
-
公开(公告)号:US20160326289A1
公开(公告)日:2016-11-10
申请号:US15107958
申请日:2014-12-24
Applicant: KANEKA CORPORATION
Inventor: Fuminobu Kitayama , Nobuyoshi Maizuru , Keisuke Hatano
IPC: C08F220/18 , C08K3/00 , G02B1/04 , C08J5/18
CPC classification number: C08F220/18 , C08F220/14 , C08F2220/185 , C08J5/18 , C08J2333/10 , C08J2333/12 , C08K3/013 , G02B1/04 , C08L33/08 , C08L33/10
Abstract: An optical thermoplastic resin has a rate of reduction in melt viscosity of less than 20%, an orientation birefringence of −1.7×10−4 to 1.7×10−4, a photoelastic constant of −3.7×10−12 to 3.7×10−12 Pa−1, and, when formed into a 2 mm-thick formed body, has a haze of 1% or less.
Abstract translation: 光学热塑性树脂的熔融粘度降低率小于20%,取向双折射率为-1.7×10 -4〜1.7×10 -4,光弹性常数为-3.7×10-12〜3.7×10- 12Pa-1,当形成2mm厚的成形体时,雾度为1%以下。
-