摘要:
The oxide matrix composite material is obtained by subjecting a fiber composed of at least one oxide or complex oxide and a matrix composed of at least one oxide or complex oxide to composite formation. For the fiber and the matrix, a component composition is selected such that the fiber and the matrix keep thermodynamic equilibrium to each other in a temperature range not exceeding the melting temperature, and a fiber diameter of the fiber at the time of equilibrium keeps ½ or more of a fiber diameter of the fiber at the start of the composite formation.
摘要:
The present invention provides a user-carriable mobile communication relay device that relays communication between an internal network and an external network, in which even when the device is moved, the device dynamically selects and connects the external network depending on a surrounding radio wave environment or a communication content. The device is provided with an internal network communication adapter 13 compatible with the internal network connecting to a specific terminal device 4; external network communication adapters 11, 12 compatible with external networks with a mobile telephone network and with a wireless LAN at an installation site; a network selection processing portion 102 automatically selecting one or more networks to be connected, out of the external networks, according to stored profile information 141; an internal network connection processing portion 104 establishing or reconfiguring the connection to an internal network selected for a predetermined opportunity; an external network connection processing portion 105 establishing or reconfiguring the connection to an external network selected for a predetermined opportunity; and a communication relay processing portion 101 relay-processing communication between the internal network and the external network.
摘要:
A wireless device and a communication method, which enable a position of the wireless device to be known and enable a frequency which does not interfere with that of another wireless station to be selected, are provided. A wireless device belonging to a second wireless system in which a frequency band to be used overlaps with that of a first wireless system, and a priority with which the overlapping frequency band is used is lower than that of the first wireless system, the wireless device includes: a location receiving unit receiving location information formed of a place name and indicating a location of the wireless device; a geographic coordinate acquiring unit acquiring, based on the location information, geographic coordinates including latitude and longitude corresponding to the location information; and a frequency setting unit accessing a frequency server in which a frequency assigned to a wireless device belonging to the first wireless system and geographic coordinates including latitude and longitude related to a position of the wireless device are stored by being corresponded to each other, by using the geographic coordinates acquired by the geographic coordinate acquiring unit, and acquiring at least one of a frequency that is not assigned to the wireless device belonging to the first wireless system and a frequency which is not at risk of interfering with that of the wireless device, to set the frequency as a transmission/reception frequency.
摘要:
There is provided a nickel alloy having an excellent creep strength as well as high-temperature oxidation resistance. The nickel alloy of the present invention comprises, by mass percent, Cr in a range of 11.5 to 11.9%, Co in a range of 25 to 29%, Mo in a range of 3.4 to 3.7%, W in a range of 1.9 to 2.1%, Ti in a range of 3.9 to 4.4%, Al in a range of 2.9 to 3.2%, C in a range of 0.02 to 0.03%, B in a range of 0.01 to 0.03%, Zr in a range of 0.04 to 0.06%, Ta in a range of 2.1 to 2.2%, Hf in a range of 0.3 to 0.4%, and Nb in a range of 0.5 to 0.8%, the balance being Ni and unavoidable impurities, and contains carbides and borides precipitating in crystal grains and at grain boundaries.
摘要:
The present invention provides a resin composition comprising: (A) a thermoplastic resin, (B) a granular material which has a number average particle diameter of 0.5 to 5 mm and is obtainable by granulating a fiber mainly having alumina with a number average fiber diameter of 1 to 50 μm, and (C) a filler composed of a material of which electric resistivity at 300 K is 102 Ωm or less. The resin composition can be molded into a molded article with electric insulation. The electric resistivity of the molded article has sufficient electric insulation in applications such as in electric and electronic parts.
摘要:
Provided is a spectrum sensor for cognitive wireless communication whereby it is possible to improve communication efficiency. In a cognitive wireless communication system, a spectrum sensor senses spectra in multiple frequency bands. A spectrum sensor is configured to be able to operate in one operation mode selected from among a spectrum sensing mode for sensing spectra, and a communication mode for communicating with a wireless communication device. Further, the spectrum sensor is provided with a controller for controlling the operation mode. The controller switches between the above-mentioned operation modes during the symbol period of an ultra-wideband physical layer (UWB PHY).
摘要:
The present invention provides a previously unattainable compact and high thrust electromagnetic stirrer coil, that is, an electromagnetic stirrer coil for stirring molten steel in a mold by electromagnetic force, in which electromagnetic stirrer coil a space factor of the yoke sectional area (-) with respect to an inside area in a vertical cross-section of said electromagnetic stirrer coil is 0.5 to 0.9 and a yoke width B is 100 mm to 300 mm. Preferably, a magnetomotive force F of said electromagnetic stirrer coil divided by the yoke width B, that is, a value of F/B, is 800 kAT/m or more.
摘要:
Provided is an Ni-based single crystal superalloy wherein the ingredients have a composition containing, as ratio by mass, from 5.0% by mass to 7.0% by mass of Al, from 4.0% by mass to 8.0% by mass of Ta, from 0% by mass to 2.0% by mass of Mo, from 3.0% by mass to 8.0% by mass of W, from 3.0% by mass to 8.0% by mass of Re, from 0% by mass to 0.50% by mass of Hf, from 3.0% by mass to 7.0% by mass of Cr, from 0% by mass to 9.9% by mass of Co and from 1.0% by mass to 10.0% by mass of Ru, with the balance of Ni and inevitable impurities. The alloy prevents TCP phase precipitation at high temperatures, therefore having improved strength at high temperatures and having oxidation resistance at high temperatures.The above-mentioned first-generation alloy CMSX-2 and second-generation alloy CMSX-4 are, though comparable thereto in point of creep strength at low temperatures, inferior to third-generation alloys in point of creep strength at high temperatures, since a large quantity of eutectic γ′-phase remains therein even after high-temperature solution treatment.
摘要:
A cement kiln chlorine/sulfur bypass system wherein the equipment cost is suppressed and the sulfur included in a combustion gas bled from a cement kiln is separated and effectively utilized. The cement kiln chlorine/sulfur bypass system comprises an air bleed means for bleeding a kiln exhaust gas passage, which runs from the end of the cement kiln to a bottom cyclone, of a part of the combustion gas, a separating means for separating dust in the gas bled by the air bleed means into coarse particles and fine particles, and a wet dust collector for collecting dust from the gas containing the fine particles separated by the separating means. The separating means is preferably a classifier in which the cut size is changeable. The wet dust collector is preferably a mixing scrubber. The mixing scrubber preferably comprises a circulating liquid tank to which dust slurry collected by the mixing scrubber is supplied and a circulating system by which a part of the dust slurry in the circulating liquid tank is returned to the mixing scrubber.
摘要:
A high-strength steel sheet includes: 0.03 to 0.20% of C, 0.08 to 1.5% of Si, 0.5 to 3.0% of Mn, 0.05% or less of P, 0.0005% or more of S, 0.008 to 0.20% of acid-soluble Ti, 0.0005 to 0.01% of N, more than 0.01% of acid-soluble Al, and 0.001 to 0.04% of one or both of Ce and La in terms of mass %; and the balance including Fe and inevitable impurities. The ratio of (Ce+La)/acid-soluble Al is equal to or more than 0.1 and the ratio of (Ce+La)/S is in the range of 0.4 to 50 in a mass base, and the density of the number of inclusions, having a circle equivalent diameter of 2 μm or less, which are present in the steel sheet is equal to or more than 15/mm2.