Abstract:
A strap comprising a propylene and 1-hexene copolymer containing from 0.3 wt % to less than 5 wt % of 1-hexene derived units said copolymer having a melt flow rate (MFR) determined according to ISO method 1133 (230° C., 2.16 kg ranging from 0.3 to less than 11 g/10 min.
Abstract:
Soft polyolefin composition with improved processability comprising from 8 to 45% by weight of a polypropylene component (A), from 45 to 82% by weight of a polyolefin component (B), and from 5 to 25% by weight of a butene-1 (co)polymer (C) having a flexural modulus of 60 MPa or less.
Abstract:
A propylene and 1-hexene copolymer containing from 0.5 wt % to less than 5 wt % of 1-hexene derived units said copolymer having: a) a melting point higher than 145° C.; b) a melt flow rate (MFR2) determined according to ISO method 1133 (230° C., 2.16 kg ranging from 10 dl/10 min to less than 60 dl/10 min; said copolymer being chemically degradated to MFR2 and wherein the ratio MFR2/MFR1 is comprised between 15 and 56; wherein MFR1 is the melt flow rate measured according to ISO method 1133 (230° C., 2.16 kg) of the propylene/1-hexene copolymer before the degradation
Abstract:
Polyolefin composition comprising, in percent by weight: A) 10-50% of a copolymer of propylene with one or more comonomer(s) selected from ethylene and CH2═CHR alpha-olefins where R is a 2-8 carbon alkyl, which copolymer contains from 1 to 8% of comonomer(s); B) 50-90% of a blend of copolymers (bI) and (bII), wherein copolymer (bI) contains from 18 to 40% of ethylene, and copolymer (bII) contains from 55 to 85% of ethylene, and the weight ratio (bI)/(bII) is from 0.2 to 2; in which composition the copolymer component (bI) is present in amounts of 15% or more with respect to the total weight of (A)+(B), the weight ratio C2II/C2I of the content C2II of ethylene in copolymer component (bII) to the content C2I of ethylene in copolymer component (bI) is of 1.8 or more, and the intrinsic viscosity [η] of the fraction XS soluble in xylene at room temperature (about 25° C.), referred to the total weight of (A)+(B), is of 2 dl/g or more.
Abstract:
A foamed polyolefin composition comprising (all percent amounts being by weight): A) 50%-90% of a polypropylene component; and B) 10%-50% of a copolymer component of ethylene and at least one C3-C10 α-olefin, the copolymer containing from 15% to 50% of ethylene, and optionally minor amounts of a diene; the said amounts of (A) and (B) being referred to the total weight of (A) and (B); said composition having at least one of the following features i) and ii), or both: i) a Polydispersity Index of component (A) of 4 or more; ii) a value of viscosity [η] of the fraction soluble in xylene at room temperature equal to or higher than 3.5 dl/g.
Abstract:
A catalyst system for the polymerization of olefins comprising (A) a catalyst component obtained by reacting a Mg(OR1)(OR2) compound, in which R1 and R2 are identical or different and are each an alkyl radical having 1 to 10 carbon atoms, with a tetravalent transition metal compound having at least a Metal-halogen bond, used in amounts such that the molar ratio Met-al/Mg is from 0.05 to 10; (B) an aluminum alkyl compound and (C) a linear or branched halogenated alkyl compound.
Abstract:
Polyolefin compositions comprising, all percentages being by weight: A) from 70 to 95%, of a compositions comprising (by weight): AI) 15-80% of one or more copolymers of propylene; AII) 20-85% of one or more copolymers with different comonomer(s) content than in A) B) from 5 to 30% of an elastomeric or plastomeric polyolefin or polyolefin composition.
Abstract:
Random copolymers of propylene with ethylene, and optionally other olefins, comprising from 3.5% to 6.5% by weight of ethylene and having a melt flow rate (MFR) according to ISO 1133 (230° C., 2.16 Kg) of less than 10 g/10 min and a melting temperature (Tm), determined by DSC, satisfying the relation: 45° C.≦Tm+C≦150° C. wherein C is the quantity (by weight) of ethylene in the copolymer. The random copolymers of the invention are specifically suited for cast film and/or sheet applications.
Abstract translation:丙烯与乙烯和任选的其它烯烃的无规共聚物,其包含3.5重量%至6.5重量%的乙烯,并且具有根据ISO 1133(230℃,2.16Kg)的熔体流动速率(MFR)小于10g / 10分钟,通过DSC测定的熔融温度(Tm)满足关系:45℃,Tm + C @ 150℃。其中C是共聚物中乙烯的量(以重量计)。 本发明的无规共聚物特别适用于流延薄膜和/或薄片应用。
Abstract:
A polymer composition comprising (percent by weight):a) 57%-74%, of a crystalline propylene polymer having an amount of isotactic pentads (mmmm), measured by 13C-MNR on the fraction insoluble in xylene at 25° C., higher than 97.5 molar % and a polydispersity index ranging from 5 to 10;b) 8 to 15%, of an elastomeric copolymer of ethylene and propylene, the copolymer having an amount of recurring units deriving from ethylene ranging from 30 to 50%, and being partially soluble in xylene at ambient temperature; the polymer fraction soluble in xylene at ambient temperature having an intrinsic viscosity value ranging from 2.5 to 3.5 dl/g; and c) 18-28%, of ethylene homopolymer having an intrinsic viscosity value ranging from 1.5 to 4 dl/g; said composition having a value of melt flow rate ranging from 35 to 60 g/10 min, and the amount of hexane extractables lower than 4.0 wt %.
Abstract:
Filled polyolefin compositions comprising: A) from 10% to 75% by weight of a polypropylene component; B) from 20% to 80% by weight of a filler; C) from 3% to 50% of a polybutene-1 component; wherein the percentages of A), B) and C) are referred to the sum of A) B) and C).