公开(公告)号:US11098143B2
公开(公告)日:2021-08-24
申请号:US16649044
申请日:2018-09-13
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: Antonio Mazzucco , Enrico Balestra , Roberto Pantaleoni , Davide Tartari , Riccardo Rinaldi
IPC: B01J8/26 , C08F210/06 , B01J8/22
Abstract: A process for the polymerization of olefins in gas phase carried out in a reactor having two interconnected polymerization zones, a first zone (riser) and a second zone (downcomer), wherein growing polymer particles: a) flow through the riser under fast fluidization conditions established by feeding a mixture of gas and liquid; b) leave the riser and enter the downcomer, through which the growing polymer particles flow downward in a densified form; and c) leave the downcomer and are reintroduced into the riser, thereby establishing a circulation of polymer between the riser and the downcomer; the reactor is operated at a temperature between 0° C. and 5° C. above the dew point of the riser gas at the operating pressure, and in the riser, besides the growing polymer particles and gas flow, an amount of liquid is present.
-
公开(公告)号:US20210253837A1
公开(公告)日:2021-08-19
申请号:US17253435
申请日:2019-06-19
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: TAKESHI NAKAJIMA , KAZUHIKO SAKAI , KUNIO YAMAMOTO , MASASHI UCHIDA
IPC: C08L23/12
Abstract: A polypropylene composition made from or containing (i) component (1) made from or containing a propylene homopolymer or copolymer containing 0 to 0.5% by weight of an ethylene-derived unit; (ii) component (2) made from or containing an ethylene/propylene copolymer containing 15 to 30% by weight of an ethylene-derived unit; and (iii) 0.01 to 1.0 parts by weight of a crystal nucleating agent based on a total of 100 parts by weight of component (1) and component (2); wherein 1) the Mw/Mn value of xylene insolubles (XI) is in the range of 6 to 20, 2) the weight ratio of component (1) to component (2) is in the range of 82:18 to 90:10, 3) the intrinsic viscosity of xylene solubles (XSIV) is in the range of 2.5 to 3.4 dl/g, 4) the MFR (at 230° C. under a load of 2.16 kg) is in the range of 3 to 10 g/10 min.
-
公开(公告)号:US20210074447A1
公开(公告)日:2021-03-11
申请号:US16965794
申请日:2019-01-21
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: CINDY FLENNIKEN , CHUN D. LEE , CLAUDIO CAVALIERI , MONICA GALVAN , VINCENT BAUDIER , GISELLA BIONDINI
Abstract: A cable article made from or containing a polyolefin composition made from or containing from 20.0 wt % to 80.0 wt % of component T1) being an interpolymer of ethylene and less than 7 wt %, of a polymerizable comonomer; from 0.5 wt % to 5.0 wt % of a peroxide; and from 20.0 wt % to 80.0 wt % of component T2) made from or containing A) 5-35% by weight of a propylene homopolymer or a propylene ethylene copolymer; B) 20-50% by weight; of a copolymer of ethylene and a C3-C8 alpha-olefin containing from 0.1% to 20% by weight of alpha-olefin units; and C) 30-60% by weight of a copolymer of ethylene and propylene containing from 25% to 75% by weight of ethylene units, wherein the cable article is selected from the group consisting of cable insulation and cable jacketing.
-
公开(公告)号:US20210070958A1
公开(公告)日:2021-03-11
申请号:US17015506
申请日:2020-09-09
Applicant: Basell Poliolefine Italia S.r.l.
Inventor: Diego Brita , Sheri E. Davis , Volker Fraaije , Simona Guidotti , Dario Liguori , Sandor Nagy , David L. Ramage , Shahram Mihan , Christopher D. Smith , Daniel F. White , Xueyong Yang
Abstract: A method of depolymerizing plastics using a halloysite catalyst is described herein. The method reduces the energy required for the depolymerization process while achieving improved depolymerization results.
-
公开(公告)号:US20200339794A1
公开(公告)日:2020-10-29
申请号:US16758526
申请日:2018-11-05
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: ROBERTO DE PALO , CLAUDIO CAVALIERI
Abstract: A polyolefin composition made from or containing:T1) 70-95 wt %, of a polyolefin component containing: a1) from 30 wt % to 70 wt % of a propylene based polymer; and a2) from 30 wt % to 70 wt % of an ethylene based polymer; and T2) 5-30 wt % of a polyolefin component containing: A) 5-35% by weight of a propylene homopolymer or a propylene ethylene copolymer; B) 25-50% by weight of a copolymer of ethylene and a C3-C8 alpha-olefin containing 0.1-20% by weight of C3-C8 alpha-olefin units; and C) 30-60% by weight of a copolymer of ethylene and propylene containing 25-75% by weight of ethylene units.
-
公开(公告)号:US10759933B2
公开(公告)日:2020-09-01
申请号:US16341584
申请日:2017-10-05
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: Paola Massari , Andrea Felisati , Marco Izzi , Claudio Cavalieri , Marco Ciarafoni , Silvia Guerra , Roberto Pantaleoni , Federica Malizia
Abstract: A nucleated propylene polymer composition made from or containing: A) a propylene homopolymer; B) a copolymer of propylene with ethylene derived units; the nucleated composition having a fraction soluble in xylene at 25° C. between 9.0 and 21.0 wt %, an intrinsic viscosity of the fraction soluble in xylene at 25° C. between 1.0 and 1.9 dl/g, a total melt flow rate between 1.5 and 5 g/10 min and the value of the relation (I): 22.5+0.2*MFR−1.2*Xs+0.2*IV (I) is higher than 5.9; wherein MFR is the melt flow rate of the nucleated composition; IV is the intrinsic viscosity of the fraction soluble in xylene at 25° C.; and Xs is the fraction soluble in xylene at 25° C., the amount of A+B is equal to 100 wt %, and the nucleating agent is selected from the group consisting of aromatic or aliphatic carboxylic acids, aromatic metal phosphates, sorbitol derivatives and talc.
-
公开(公告)号:US10759882B2
公开(公告)日:2020-09-01
申请号:US16337779
申请日:2017-09-25
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: Simona Guidotti , Tiziano Dall'Occo , Dario Liguori , Giampiero Morini
IPC: C08F10/02 , C08F210/16
Abstract: A process for the preparation of a solid catalyst component for the homo or copolymerization of olefins, wherein the solid catalyst component is made from or contains Mg, Ti, halogen and an electron donor selected from cycloalkyl ethers, wherein the process includes the steps of (a) dissolving a Mg based compound and a TiCl3 based compound in a liquid medium further made from or containing a cycloalkyl ether and a compound of formula R2OH where R2 is a C1-C20 hydrocarbon group, in which the Ti/Mg molar ratio ranges from 0.1 to 0.5, the cycloalkyl ether/Mg ratio ranges from 1 to 4 and the ROH/Mg molar ratio ranges from 1 to 4; and (b) adding, to the solution coming from step (a), SiCl4 in an amount such that the R2OH/SiCl4 molar ratio ranges from 0.5 to 1.5 and maintaining the temperature in the range 50-150° C. thereby precipitating the solid catalyst component particles.
-
公开(公告)号:US20200216587A1
公开(公告)日:2020-07-09
申请号:US16647672
申请日:2018-08-30
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: PAOLA MASSARI , CLAUDIO CAVALIERI , DAVIDE TARTARI , TIZIANA CAPUTO , ISABELLA MARIA VITTORIA CAMURATI
IPC: C08F210/06 , C08F2/34 , C08L23/14
Abstract: A propylene ethylene copolymer having: i) xylene soluble fraction at 25° C. ranging from 14 wt % to 27 wt %; ii) intrinsic viscosity of the fraction soluble in xylene at 25° C. ranging from 1.0 to 2.4 dl/g; iii) melt flow rate, MFR, ranging from 1.0 g/10 min to 50.0 g/10 min; iv) an ethylene derived units content ranging from 5.0 wt % to 12.0 wt %; v) the ethylene derived units content on the fraction insoluble in xylene at 25° C. ranging from 2.5 wt % to 6.0 wt %; vi) the ethylene derived units content on the fraction soluble in xylene at 25° C. ranging from 15.2. wt % to 30.2 wt %; and vii) C13 NMR sequences PEP measured on the fraction insoluble in xylene at 25° C. ranging from 3.5 mol % to 5.5 mol % and C13 NMR sequences PEP measured on the fraction soluble in xylene at 25° C. ranging from 11.0 mol % to 14.2 mol %.
-
公开(公告)号:US20200165424A1
公开(公告)日:2020-05-28
申请号:US16629104
申请日:2018-06-20
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: MONICA GALVAN , CLAUDIO CAVALIERI , JAUME MARTI PORQUERES , RENAUD LEMAIRE , ROBERTO DE PALO
Abstract: A polyolefinic fiber made from or containing from 2 wt % to 20 wt % relative to the total weight of the fiber of a polyolefin composition made from or containing: A) 5-35% by weight of a propylene homopolymer or a propylene ethylene copolymer; B) 20-50% by weight of a copolymer of ethylene and a C3-C8 alpha-olefin containing from 0.1% to 20% by weight of alpha-olefin units and containing 25% by weight or less of a fraction soluble in xylene at 25° C.; and C) 30-60% by weight of a copolymer of ethylene and propylene containing from 25% to 75% by weight of ethylene units and containing from 40% to 95% by weight of a fraction soluble in xylene at 25° C.; the amounts of (A), (B) and (C) being referred to the total weight of (A)+(B)+(C), the sum of the amount of (A)+(B)+(C) being 100.
-
公开(公告)号:US10550212B2
公开(公告)日:2020-02-04
申请号:US15511976
申请日:2015-09-09
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: Mara Destro , Marco Ciarafoni , Paola Massari , Tiziana Caputo , Thomas Bohm
IPC: B65D1/02 , C08F2/00 , C08F210/06 , C08F4/646 , C08F4/654 , C08F210/08 , C08F210/16
Abstract: The present disclosure provides an article of manufacture made from or containing a propylene-based terpolymer, having (i) ethylene-derived units in the range from about 0.5 wt. % to about 1.8 wt. %; (ii) 1-butene-derived units in the range from about 1.5 wt. % to about 2.5 wt. %; (iii) a ratio of C2 wt %/C4 wt % in the range from about 0.40 to about 0.80, wherein C2 wt % is the weight percent of ethylene-derived units and C4 wt % is the weight percent of 1-butene-derived units; (iv) a melt flow rate in the range from about 30 g/10 min to about 80 g/10 min; (v) a xylene soluble fraction at 25° C. lower than about 5.0 wt. %; and (vi) a melting point higher than about 140° C. The article can be a container, which can be used for food applications.
-
-
-
-
-
-
-
-
-