Abstract:
A plastic forming mold made from a stainless steel, having in weight % (wt. %): C 0.32-0.50, Si 0.1-1.0, Mn 0.1-0.8, Cr 11-14, Mo 1.8-2.6, V 0.35-0.70, N 0.05-0.19, optional elements, and a balance of Fe apart from impurities. The stainless steel is hardened and tempered and has a matrix comprising ≥90 vol. % martensite.
Abstract:
The invention relates to a stainless steel. The stainless steel consists of in weight % (wt. %): C 0.32-0.50 Si 0.1-1.0 Mn 0.1-0.8 Cr11-14 Mo 1.8-2.6 V 0.35-0.70 N 0.05-0.19 optional elements, balance Fe and impurities.
Abstract:
An alloy produced by powder metallurgy including a non-amorphous matrix. The alloy consists of, in weight % (wt. %): C 0-0.15, Si 0-2.5, Mn 0-15, Cr 0-25, Mo 4-35, B 0.2-2.8, optional elements, balance Fe and/or Ni apart from impurities. The alloy comprises 3-35 volume % hard phase particles, the hard phase particles comprises at least one of borides, nitrides, carbides and/or combinations thereof, at least 90% of the hard phase particles have a size of less than 5 μm, and at least 50% of the hard phase particles have a size in the range of 0.3-3 μm.
Abstract:
The invention relates hot work tool steel. The steel comprises the following main components (in wt. %): C 0.27-0.38 Si 0.10-0.35 Mn 0.2-0.7 Cr 4.5-5.5 Mo 2.05-2.90 V 0.4-0.6 N 0.01-0.12 H ≤0.0004 S ≤0.0015 balance optional elements, iron and impurities.
Abstract:
The invention relates to an alloy produced by powder metallurgy and having a non-amorphous matrix, the alloy consists of in weight % (wt. %): C 0-2.5 Si 0-2.5 Mn 0-15 Cr 0-25 Mo 4-35 B 0.2-2.8 optional elements, balance Fe and/or Ni apart from impurities, wherein the alloy comprises 3-35 volume % hard phase particles, the hard phase particles comprises at least one of borides, nitrides, carbides and/or combinations thereof, at least 90% of the hard phase particles have a size of less than 5 μm and at least 50% of the hard phase particles have a size in the range of 0.3-3 μm.
Abstract:
The invention relates cold work tool steel. The steel includes the following main components (in wt. %): C 2.2-2.4, Si 0.1-0.55, Mn 0.2-0.8, Cr 4.1-5.1, Mo 3.1-4.5, V 7.2-8.5, balance optional elements, iron and impurities.
Abstract:
THIS INVENTION RELATES TO ELASTIC ELEMENTS, PRIMARILY SPRINGS ON WHICH THE REQUIRED STANDARDS OF FATIGUE RESISTANCE AND/OR FLATNESS, ETC. ARE OF A HIGH ORDER. MORE SPECIFICALLY, THIS INVENTION RELATES TO SPRINGS WHICH ARE PRODUCED FROM A STEEL ALLOY, THE COMPOSITION OF WHICH IS SUCH
THAT IN A TEMPERATURE RANGE BETWEEN 500 AND 700*C. THE STEEL MAY HAVE A MATRIX THAT IS PRIMARILY FERRITIC.
Abstract:
Articles are degreased by being lowered into a zone of vapour originating from a pool of boiling solvent. The vapour condenses on the articles, dissolving oil and other impurities, and the impure solvent is allowed to flow into the pool of boiling solvent. The articles are now dipped into a pool of comparatively cold solvent. Finally, the articles are lifted up into the vapour zone, and the pure solvent formed by condensation on the articles is allowed to flow into the pool of comparatively cold solvent.