Abstract:
The present invention provides a positive active material including a lithium-containing compound represented by the following Chemical Formula 1 and a rechargeable lithium battery including the positive active material. LiFe1-x-zMxM′zPyO4 Chemical Formula 1
Abstract:
Provided is a positive electrode for a rechargeable lithium battery including a positive active material including a lithium phosphate compound particle and fiber-type carbon attached inside the lithium phosphate compound particle, a method of preparing the same, and a rechargeable lithium battery including the same.
Abstract:
A phosphor composition including a first phosphor represented by Formula 1: Ba1-bMg1-aAl10O17:Mna,Eub (1). In Formula 1, a and b satisfy the relations: 0.05≦a≦0.4, and 0.006≦b
Abstract translation:一种荧光体组合物,包括由式1表示的第一荧光体:Ba1-bMg1-aAl10O17:Mna,Eub(1)。 在式1中,a和b满足关系:0.05&nlE; a&nlE; 0.4和0.006&nlE; b <0.05。
Abstract:
Phosphor paste compositions, phosphor layers and electron emitting devices are provided. The phosphor paste composition includes a phosphor, a binder including a photocurable monomer and an acrylic resin with an acid value ranging from about 150 mgKOH/g to about 200 mgKOH/g, a photoinitiator, and a solvent. The phosphor layer is obtained from the phosphor paste composition, and the electron emission device includes the phosphor layer. The phosphor paste compositions provide superior phosphor layer pattern resolution, plasticity, printability, and storage stability.
Abstract:
Disclosed is a low-voltage blue color fluorescent substance which is doped with 0.5 to 3 weight % of P, and a manufacturing method of the same. The above blue color fluorescent substance is manufactured by mixing phosphoric compound as flux with a mixture of zinc oxide (ZnO) and gallium oxide (Ga2O3); carrying out a primary burn on the mixture at a temperature of 1,200 to 1,300° C.; ball milling and washing; and carrying out a secondary burn on the resultant material at a temperature of 900 to 1,100° C., and then classifying the substance.
Abstract translation:公开了掺杂有0.5〜3重量%的P的低电压蓝色荧光物质及其制造方法。 上述蓝色荧光物质通过将磷化合物作为助熔剂与氧化锌(ZnO)和氧化镓(Ga 2 O 3)的混合物混合而制备; 在1,200〜1300℃的温度下对混合物进行初级燃烧; 球磨和洗涤; 并在900〜1100℃的温度下在所得材料上进行二次燃烧,然后对物质进行分级。
Abstract:
A lithium secondary battery including lithium molybdate. The lithium molybdate is a composite including amorphous lithium molybdate as a minor component and crystalline lithium molybdate as a major component.
Abstract:
A white phosphor including: 40 to 50 parts by weight of a blue phosphor selected from the group consisting of ZnS:(Ag,Cl), ZnS:(Ag,Al), ZnS:(Ag,Al,Cl), and a combination thereof; 20 to 30 parts by weight of a green phosphor (Sr1−xCax)Ga2S4:Eu (0≦x
Abstract translation:一种白色荧光体,包括:40〜50重量份的选自ZnS:(Ag,Cl),ZnS:(Ag,Al),ZnS:(Ag,Al,Cl)的组合物和组合 的; 20〜30重量份绿色荧光体(Sr1-xCax)Ga2S4:Eu(0 <= x <0.2); 和20〜30重量份选自Y 2 O 3:Eu,Y 2 O 3:(Eu,Tb),Y 2 O 2 S:Eu,Y 2 O 2 S:(Eu,Tb)的红色荧光体及其组合。 白色荧光体可以包含在发光装置中。 发光装置可以包括在液晶显示器中。
Abstract:
An yttrium based phosphor, a process for preparing the yttrium based phosphor, and a display device using the yttrium based phosphor, the yttrium based phosphor including a conducting material such as WO3 or SnO2, and exhibiting an enhanced luminance characteristic under low voltage, and high current density conditions.
Abstract:
An yttrium based phosphor, a process for preparing the yttrium based phosphor, and a display device using the yttrium based phosphor, the yttrium based phosphor including a conducting material such as WO3 or SnO2, and exhibiting an enhanced luminance characteristic under low voltage, and high current density conditions.
Abstract:
A low-voltage excited blue phosphor is provided. The phosphor comprises a matrix represented by general formula ZnO.Ga2O3, and Bi doped in the matrix. To prepare the phosphor, ZnO, Ga2O3, Bi compound, and a flux are mixed to produce a mixture, and the mixture is fired at 1100-1300° C. to produce a fired material. Then the fired material is milled, and washed with an acid. The washed material is fired at 800-1100° C. and sieved to produce the blue phosphor.
Abstract translation:提供了低压激发蓝色荧光体。 磷光体包括由通式ZnO.Ga 2 O 3表示的基体和掺杂在基质中的Bi。 为了制备荧光体,将ZnO,Ga 2 O 3,Bi化合物和助熔剂混合以产生混合物,并将混合物在1100-1300℃下烧制以产生烧制材料。 然后将烧制的材料研磨,并用酸洗涤。 将洗涤的材料在800-1100℃下烧制并过筛以产生蓝色荧光体。