Abstract:
Improved aluminum-copper-lithium alloys are disclosed. The alloys may include 3.4-4.2 wt. % Cu, 0.9-1.4 wt. % Li, 0.3-0.7 wt. % Ag, 0.1-0.6 wt. % Mg, 0.2-0.8 wt. % Zn, 0.1-0.6 wt. % Mn, and 0.01-0.6 wt. % of at least one grain structure control element, the balance being aluminum and incidental elements and impurities. The alloys achieve an improved combination of properties over prior art alloys.
Abstract:
Heat treatable aluminum alloy strips and methods for making the same are disclosed. The heat treatable aluminum alloy strips are continuously cast and quenched, with optional rolling occurring before and/or after quenching. After quenching, the heat treatable aluminum alloy strip is neither annealed nor solution heat treated.
Abstract:
Aluminum alloy products, such as plate, forgings and extrusions, suitable for use in making aerospace structural components like integral wing spars, ribs and webs, comprises about: 6 to 10 wt. % Zn; 1.2 to 1.9 wt. % Mg; 1.2 to 2.2 wt. % Cu, with Mg≦(Cu+0.3); and 0.05 to 0.4 wt. % Zr, the balance Al, incidental elements and impurities. Preferably, the alloy contains about 6.9 to 8.5 wt. % Zn; 1.2 to 1.7 wt. % Mg; 1.3 to 2 wt. % Cu. This alloy provides improved combinations of strength and fracture toughness in thick gauges. When artificially aged per the 3-stage method of preferred embodiments, this alloy also achieves superior SCC performance, including under seacoast conditions.
Abstract:
Decorative shape cast products and methods, systems, compositions and apparatus for producing the same are described. In one embodiment, the decorative shape cast products are produced from an Al—Ni or Al—Ni—Mn alloy, with a tailored microstructure to facilitate production of anodized decorative shape cast product having the appropriate finish and mechanical properties.
Abstract:
Decorative shape cast products and methods, systems, compositions and apparatus for producing the same are described. In one embodiment, the decorative shape cast products are produced from an Al—Ni or Al—Ni—Mn alloy, with a tailored microstructure to facilitate production of anodized decorative shape cast product having the appropriate finish and mechanical properties.
Abstract:
The present application discloses wrought 2xxx Al—Li alloy products that are work insensitive. The wrought aluminum alloy products generally include from about 2.75 wt. % to about 5.0 wt. % Cu, from about 0.2 wt. % to about 0.8 wt. % Mg, where the ratio of copper-to-magnesium ratio (Cu/Mg) in the aluminum alloy is in the range of from about 6.1 to about 17, from about 0.1 wt. % to 1.10 wt. % Li, from about 0.3 wt. % to about 2.0 wt. % Ag, from 0.50 wt. % to about 1.5 wt. % Zn, up to about 1.0 wt. % Mn, the balance being aluminum, optional incidental elements, and impurities. The wrought aluminum alloy products may realize a low strength differential and in a short aging time due to their work insensitive nature.
Abstract:
New 2xxx aluminum alloy bodies and methods of producing the same are disclosed. The new 2xxx aluminum alloy bodies may be produced by preparing the aluminum alloy body for post-solutionizing cold work, cold working by at least 25%, and then thermally treating. The new 2xxx aluminum alloy bodies may realize improved strength and other properties.
Abstract:
New 2xxx aluminum alloys containing vanadium are disclosed. In one embodiment, the aluminum alloy includes 3.3-4.1 wt. % Cu, 0.7-1.3 wt. % Mg, 0.01-0.16 wt. % V, 0.05-0.6 wt. % Mn, 0.01 to 0.4 wt. % of at least one grain structure control element, the balance being aluminum, incidental elements and impurities. The new alloys may realize an improved combination of properties, such as in the T39 or T89 tempers.
Abstract:
Molten metal of a first composition is fed into a mold cavity, via a first control apparatus, wherein the control apparatus is open, wherein the feeding comprises flowing out of a first feed chamber. The first control apparatus is closed. A second control apparatus is opened. Molten metal of a second composition is fed into the mold cavity, via the second control apparatus, wherein at least a portion of the metal of the first composition in the mold cavity is sufficiently molten so that an initial feed of molten metal of the second composition mixes with the molten metal of the first composition in the mold cavity, wherein the feeding comprises flowing out of a second feed chamber, wherein the second composition is different from the first composition. An ingot is removed from the mold cavity, wherein the ingot has a top section, a middle section, and a bottom section, wherein the bottom section is composed of metal of the first composition, wherein the top section is composed of metal of the second composition, wherein the middle section is composed of a mixture of metal of the first composition and the second composition.
Abstract:
New 5xxx-lithium aluminum alloys and related products are disclosed. The new 5xxx-lithium aluminum alloy may contain from 3.75 to 5.0 wt. % Mg, from 1.6 to 2.3 wt. % Li, and from 0.50 to 2.5 wt. % Zn, among others.