Abstract:
The invention relates to a polymer composition comprising polyolefin (a), which is other than low density polyethylene (LDPE), and polyolefin (b), which is an LDPE polymer and obtainable by a high pressure process which process comprises the steps: (i) compressing one or more monomer(s) under pressure in a compressor, using a compressor lubricant for lubrication, (ii) polymerising a monomer optionally together with one or more comonomer(s) in a polymerisation zone, (iii) separating the obtained polyolefin (b) from the unreacted products and recovering the separated polyolefin in a recovery zone, wherein in step (i) the compressor lubricant comprises a non-mineral oil; a power cable, e.g. of a direct current (DC) power cable, use of a polymer composition and a process for producing a DC power cable.
Abstract:
The present invention relates to a crosslinked polymer composition comprising a crosslinked polyolefin, wherein the polymer composition comprises, prior to crosslinking, a polyolefin and peroxide which is in an amount of less than 35 mmol —O—O-/kg polymer composition, characterized in that the crosslinked polymer composition has been in a direct contact with a semiconductive composition for 24 h at 70° C., and that the crosslinked polymer composition thereafter has an electrical DC-conductivity of 150 fS/m or less, wherein the electrical DC-conductivity is measured in accordance with “DC conductivity method”, as described under “Determination methods”, on a plaque of the crosslinked polymer composition at 70° C. and 30 kV/mm mean electric field from a non-degassed and 1 mm thick plaque sample of the crosslinked polymer composition; a layered structure, cable, e.g. a power cable, use of the crosslinked polymer composition and the structured layer, both, for producing a crosslinked power cable, e.g., a cross linked direct current (DC) power cable; and a process for producing a cable.
Abstract:
A cable comprising one or more conductors surrounded by at least an inner semiconductive layer, an insulation layer and an outer semiconductive layer, in that order, wherein the insulation layer is not crosslinked and comprises at least 90 wt % of a polymer composition, said polymer composition comprising: (I) 85.0 to 99.5 wt % of an LDPE; and (II) 0.5 to 15.0 wt % of an HDPE having a density of at least 940 kg/m3 or 1.5 to 15.0 wt % of an ultra-high molecular weight polyethylene having a Mw of at least 1,000,000.
Abstract:
The invention provides a polymer composition comprising a) a low density polyethylene (LDPE); and b) a conjugated aromatic polymer. The invention also relates to cables comprising said polymer composition and the use of the polymer composition in the manufacture of an insulation layer of cable.
Abstract:
The invention relates to a polymer composition with improved DC electrical properties, to the use of the composition for producing a cable layer and to a cable surrounded by at least one layer comprising the polymer composition.
Abstract:
The present invention relates to a crosslinked polymer composition comprising a crosslinked polyolefin, wherein the polymer composition comprises, prior to crosslinking, a polyolefin and peroxide which is in an amount of less than 35 mmol —O—O-/kg polymer composition, characterized in that the crosslinked polymer composition has been in a direct contact with a semiconductive composition for 24 h at 70° C., and that the crosslinked polymer composition thereafter has an electrical DC-conductivity of 150 fS/m or less, wherein the electrical DC-conductivity is measured in accordance with “DC conductivity method”, as described under “Determination methods”, on a plaque of the crosslinked polymer composition at 70° C. and 30 kV/mm mean electric field from a non-degassed and 1 mm thick plaque sample of the crosslinked polymer composition; a layered structure, cable, e.g. a power cable, use of the crosslinked polymer composition and the structured layer, both, for producing a crosslinked power cable, e.g., a cross linked direct current (DC) power cable; and a process for producing a cable.
Abstract:
The present invention relates to a crosslinked polymer composition, which is obtained by crosslinking a polymer composition, which polymer composition has a melt flow rate (MFR) of less than 1.7 and comprises a polyolefm, peroxide and sulphur containing antioxidant, characterised by that the crosslinked polymer composition has an Oxidation Induction Time, determined according to ASTM-D3895, ISO/CD 11357 and EN 728 using a Differential Scanning Calorimeter (DSC), which Oxidation Induction Time corresponds to Z minutes, and comprises an amount of peroxide by-products which corresponds to W ppm determined according to BTM2222 using HPLC, wherein Z1≦Z≦Z2, W1≦W≦W2, and W≦p−270*Z, wherein Z1 is 0, Z2 is 60, W1 is 0 and W2 is 9500, and p is 18500; and use thereof, a power cable insulation and a power cable, useful in high voltage (HV) and extra high voltage (EHV) cable applications direct current (DC) applications.
Abstract:
A polymer composition comprising: (i) at least 40 wt % LDPE; (ii) a polypropylene homopolymer; and (iii) a random heterophasic polypropylene copolymer.
Abstract:
The present invention relates to a polypropylene composition comprising (A) a copolymer of propylene and comonomer units selected from ethylene and alpha-olefins having from 4 to 12 carbon atoms with a total amount of comonomer units of from 10.0 to 16.0 wt %, based on the total amount of monomer units in the polypropylene composition, and (B) an alpha-nucleating agent; wherein the polypropylene composition has a xylene cold soluble (XCS) fraction in a total amount of from 25.0 to 50.0 wt %, based on the total weight amount of the polypropylene composition, with an amount of comonomer units of at least 23.0 wt %, based on the total amount of monomer units in the xylene cold soluble (XCS) fraction, a melt flow rate MFR2 of from 0.5 to 5.0 g/10 min, and a flexural modulus of not more than 470 MPa, an article comprising said polypropylene composition, preferably a cable comprising an insulation layer comprising said polypropylene composition and the use of said polypropylene composition as cable insulation for medium and high voltage cables.
Abstract: