    摘要: Disclosed is a gaming machine. According to the gaming machine, when a combination of symbols relating to a winning is displayed on a one line, the symbols constituting the combination of symbols relating to the winning and symbols constituting a combination of specific symbols in accordance with the combination of symbols relating to the winning are respectively arranged on peripheries of reels so that the combination of specific symbols is displayed on a line different from the one line. In addition, an image display unit of the gaming machine displays a specific image representing a corresponding relationship between a prize in accordance with the combination of symbols relating to the winning and the combination of specific symbols in accordance with the combination of symbols relating to the winning.

    摘要翻译: 公开了一种游戏机。 根据游戏机,当在一行上显示与胜利有关的符号的组合时,构成与胜利有关的符号的组合的符号和构成特定符号的组合的符号根据与 获胜分别设置在卷轴的周边,使得特定符号的组合显示在与一条线不同的线上。 此外,游戏机的图像显示单元根据与获胜相关的符号的组合,根据与获胜相关的符号的组合和特定符号的组合,显示表示奖品之间的对应关系的特定图像 。

    Water-swellable polymer gel and process for preparing the same
    22.
    发明授权
    Water-swellable polymer gel and process for preparing the same 有权
    水溶胀性聚合物凝胶及其制备方法

    公开(公告)号:US06486285B2

    公开(公告)日:2002-11-26

    申请号:US09767227

    申请日:2001-01-23

    申请人: Akio Fujita

    发明人: Akio Fujita

    IPC分类号: C08G1206

    摘要: A water-swellable polymer gel prepared by reacting an ester of a carboxyl group-containing polysaccharide with a compound having at least two &agr;-amino groups, which is derived from a natural amino acid, and a foamed article thereof. The water-swellable polymer gel can be used in the fields such as industry, agriculture, food and medicine. The applications of the water-swellable gel in the medical field include wound dressings, adhesion-preventing materials, dialysis membranes, hemostatic materials, adhesive materials, sealants, contact lenses, materials for tissue regeneration, microcapsule materials and drug delivery systems.

    摘要翻译: 通过使含羧基的多糖的酯与具有至少两个α-氨基的化合物(其衍生自天然氨基酸)和其发泡制品反应制备的水溶胀性聚合物凝胶。 水溶胀性聚合物凝胶可用于工业,农业,食品和医药等领域。 水溶胀性凝胶在医疗领域的应用包括伤口敷料,防粘连材料,透析膜,止血材料,粘合剂材料,密封剂,隐形眼镜,用于组织再生的材料,微胶囊材料和药物递送系统。

    Production method for grain oriented silicion steel sheet having
excellent magnetic characteristics
    23.
    发明授权
    Production method for grain oriented silicion steel sheet having excellent magnetic characteristics 失效
    具有优异磁特性的晶粒取向硅酸钢板的制造方法

    公开(公告)号:US5667598A

    公开(公告)日:1997-09-16

    申请号:US622390

    申请日:1996-03-27

    摘要: Method for producing a grain oriented silicon steel sheet comprises heating a silicon steel slab containing about:C : 0.01 to 0.10 wt %, Si: 2.5 to 4.5 wt %,Mn: 0.02 to 0.12 wt %, Al: 0.005 to 0.10 wt %,N : 0.004 to 0,015 wt %,to about 1280.degree. C. or higher and then subjecting it to hot rolling to prepare a hot-rolled steel sheet, subjecting the steel sheet to hot-rolled sheet annealing according to necessity, then subjecting it to one cold-rolling step or two or more cold-rolling steps with interposed intermediate annealing steps to prepare a cold-rolled steel sheet, and subjecting the cold-rolled steel sheet to decarburization annealing and finishing annealing, wherein the finishing rolling terminating temperature of the hot-rolling step is controlled to a range of about 900.degree. to 1100.degree. C., and the rolled sheet is processed so that the steel sheet temperature T(t) (.degree. C.) after time t falling in a range determined by an equation (1) which elapses from the termination of said hot finishing rolling approximately satisfies the equation (2):2 seconds.ltoreq.t.ltoreq.6 seconds (1)T(t).ltoreq.FDT-(FDT-700)/6.times.t (2)wherein FDT represents the hot finishing termination temperature (.degree. C.).

    摘要翻译: 晶粒取向硅钢板的制造方法包括加热含有C:0.01〜0.10重量%,Si:2.5〜4.5重量%,Mn:0.02〜0.12重量%,Al:0.005〜0.10重量%的硅钢板, N:0.004〜0.015wt%〜约1280℃以上,然后热轧制备热轧钢板,根据需要对钢板进行热轧板退火,然后将其 一个冷轧步骤或两个或多个冷轧步骤,其中间中间退火步骤以制备冷轧钢板,并对冷轧钢板进行脱碳退火和精加工退火,其中,最终轧制终止温度 将热轧步骤控制在约900〜1100℃的范围内,对轧制板进行加工,使得在时间t之后的钢板温度T(t)(℃)落在由 从sai终止过去的方程(1) d热精轧大致满足式(2):2秒

    Process for producing extruded noodle capable of being instantly cooked
    24.
    发明授权
    Process for producing extruded noodle capable of being instantly cooked 失效
    生产挤压面条的方法能够立即煮熟

    公开(公告)号:US5332592A

    公开(公告)日:1994-07-26

    申请号:US689876

    申请日:1991-05-24

    IPC分类号: A23L7/109 A23L7/113 A23L1/16

    CPC分类号: A23L7/111

    摘要: In accordance with this invention, a starting powder mixture composed of raw tapioca starch mixed with durum semolina and/or wheat flour is kneaded together with water added thereto, and the resulting kneaded dough material is passed through an extruder, whereby the dough material is extruded to provide extruded raw noodle strings each having at least one groove extending longitudinally in the noodle string. Or alternatively, said kneaded dough material is extruded through an extruder to form a web of the dough for use in the formation of noodle, and the resulting noodle-forming, extruded dough web is engraved to form therein a plurality of parallel grooves extending in the direction of the extrusion molding. The resulting noodle-forming dough web having a plurality of the grooves is cut by means of cutting blade(s) at the zones of the web interposed between the respective grooves of the web to provide raw noodle strings each having at least one groove extending longitudinally in the noodle string. Then, the resulting extruded raw noodle strings having the grooves are steamed in a steamer and subsequently treated so as to absorb water therein in order to increase the water content of the noodle strings to a water content of 38 to 50% by weight, followed by frying the these noodle strings in oil. Thereby, such extruded noodle capable of being instantly cooked can be produced, which is useful as a food product.

    摘要翻译: PCT No.PCT / JP89 / 00995 Sec。 371日期1991年5月24日 102(e)日期1991年5月24日PCT提交1989年9月29日PCT公布。 WO90 / 03120PC PCT出版物 1990年4月5日。根据本发明,将与硬粒小麦粉混合的粗木薯淀粉和/或小麦粉组成的起始粉末混合物与加入的水一起捏合,并将所得捏合的面团材料通过挤出机 由此面团材料被挤出以提供挤压的生面条,其每个具有在面条串中纵向延伸的至少一个凹槽。 或者,所述捏合的面团材料通过挤出机挤出以形成用于形成面条的生面团的网状物,并且将所形成的面条形挤出的面团网片雕刻成多个平行的凹槽, 挤出成型的方向。 所形成的具有多个槽的面条形面团网通过在幅材的相应槽之间的纤维网区域上的切割刀片被切割,以提供生面条,每个具有至少一个纵向延伸的凹槽 在面条串里。 然后,将所得到的具有凹槽的挤出的生面条串蒸汽蒸发并随后处理以吸收其中的水,以便将面条的含水量增加到38至50重量%的水含量,随后 油炸这些面条。 因此,可以制造能够立即煮熟的这种挤出的面条,其可用作食品。

    Silver halide photographic light-sensitive material improved on pinhole
production
    25.
    发明授权
    Silver halide photographic light-sensitive material improved on pinhole production 失效
    卤化银照相感光材料在针孔生产上得到改善

    公开(公告)号:US4978602A

    公开(公告)日:1990-12-18

    申请号:US417745

    申请日:1989-10-05

    摘要: A silver halide photographic light-sensitive material is disclosed, which is suitable for contact printing in photomechanical process and capable of being handled in daylight room. The light-sensitive material comprises a support having thereon a silver halide emulsion layer containing a silver halide emulsion and a hydrazine compound or a tetrazolium compound, a layer being provided on the surface of said emulsion layer farther from said support and containing a compound having a maximum spectral absorption at a wavelength of at least 50 nm longer than that of the maximum spectral sensitivity of said silver halide emulsion, and a layer being interposed between said support and said emulsion layer and containing a macromolecular compound having a heterocyclic group having a sulfo group or an alkylsulfo group. The light-sensitive material is excellent in reverse-text quality and inhibited in formation of pin-holes.

    摘要翻译: 公开了一种卤化银照相感光材料,其适用于光机械过程中的接触印刷并且能够在日光室中处理。 感光材料包括其上具有包含卤化银乳剂和肼化合物或四唑鎓化合物的卤化银乳剂层的载体,在所述乳剂层的表面上提供比所述载体更远的层,并且含有具有 波长比所述卤化银乳剂的最大光谱灵敏度长至少50nm的最大光谱吸收,以及介于所述载体和所述乳剂层之间并含有具有具有磺基的杂环基的高分子化合物的层 或烷基磺基。 感光材料具有优异的反文本质量并且抑制了针孔的形成。