COVER WINDOW, MANUFACTURING METHOD OF COVER WINDOW, AND DISPLAY DEVICE INCLUDING COVER WINDOW

    公开(公告)号:US20220321159A1

    公开(公告)日:2022-10-06

    申请号:US17481021

    申请日:2021-09-21

    Abstract: A cover window, a manufacturing method of a cover window, and a display device including a cover window are provided. A cover window includes a folding portion and a non-folding portion, and the folding portion includes an inside surface that is compressed when folded and an outside surface that is stretched when folded, the folding portion includes a first layer adjacent to the outside surface, a second layer adjacent to the inside surface, and a third layer between the first layer and the second layer, the folding portion and the non-folding portion include at least one metal ion, a concentration of the metal ion included in the second layer is higher than a concentration of the metal ion included in the first layer, and the first layer includes a plurality of depletion regions.

    WINDOW SUBSTRATE AND DISPLAY DEVICE HAVING THE SAME

    公开(公告)号:US20210212229A1

    公开(公告)日:2021-07-08

    申请号:US17210440

    申请日:2021-03-23

    Abstract: A window substrate for protecting an electronic display device, the window substrate includes: a first substrate; a second substrate; and an interlayer having opposed sides disposed between the first substrate and the second substrate, with one side of the interlayer being in contact with the first substrate, and the other side of the interlayer being in contact with the second substrate, wherein the first substrate has a first thickness, the second substrate has a second thickness, and the interlayer has a third thickness, and wherein the sum of the first thickness, the second thickness, and the third thickness is about 190 μm or less.

    DISPLAY DEVICE AND MANUFACTURING METHOD OF DISPLAY DEVICE

    公开(公告)号:US20250031557A1

    公开(公告)日:2025-01-23

    申请号:US18657088

    申请日:2024-05-07

    Abstract: A display device according to an embodiment of the disclosure includes a panel; a camera that does not overlap the panel in a plan view; a polarization layer disposed on the panel; a transmission layer extending to at least a portion of the polarization layer; and a coating layer having a larger area than the panel and disposed over the polarization layer and the transmission layer, wherein the transmission layer overlaps the camera in a plan view.

    GLASS STRENGTH EVALUATION APPARATUS AND METHOD

    公开(公告)号:US20230184647A1

    公开(公告)日:2023-06-15

    申请号:US17870834

    申请日:2022-07-22

    Abstract: A glass strength evaluation apparatus includes a support unit, a plate disposed on the support unit and including a surface on which a glass article, which is a target to be tested, is disposed, a fixing jig disposed on the plate and a power unit lifting up or down the fixing jig in a vertical direction toward the surface of the plate. The fixing jig includes a body portion, which extends in the vertical direction and lower fixing bolts. A press-fitting member insertion opening is recessed from a bottom of the body portion to extend in an upward direction, lower fixing bolt insertion holes penetrate the body portion, from one side of the body portion, in a first horizontal direction intersecting the vertical direction, to be extended to the press-fitting insertion opening, and lower fixing bolts are coupled into the lower fixing bolt insertion holes.

    GLASS ARTICLE AND METHOD OF MANUFACTURING THE SAME

    公开(公告)号:US20210206692A1

    公开(公告)日:2021-07-08

    申请号:US16998062

    申请日:2020-08-20

    Inventor: Hoi Kwan LEE

    Abstract: A glass article includes a first surface, a second surface which is opposite the first surface, a first compressive region which extends to a first compression depth in a thickness direction from the first surface, a second compressive region which extends to a second compression depth from the second surface, and a tensile region which is disposed between the first compressive region and the second compressive region. A stress profile of the first compressive region includes a first point and a first inflection point, the first inflection point is located between the first point and the first surface, a depth from the first surface to the first point is 45 to 55% of the first compression depth from the first surface, stress at the first point is greater than 50% of compressive stress of the first surface, and a thickness of the glass article is 0.01 to 0.05 mm.

    GLASS PRODUCT AND DISPLAY DEVICE INCLUDING THE SAME

    公开(公告)号:US20210179489A1

    公开(公告)日:2021-06-17

    申请号:US16931142

    申请日:2020-07-16

    Abstract: A glass product includes: a first compressive region at a first surface; a second compressive region at a second surface; and a tensile region between the first and second compression regions. A stress profile of the first compressive region includes a first trend line between the first surface and a first transition point, a second trend line between the first transition point and a second transition point, and a third trend line between the second transition point and a point at a first compression depth from the first surface. A depth from the first surface to the first transition point is 10 μm or less, a stress at the first transition point is 200 MPa or greater, a depth from the first surface to the second transition point is 50 μm to 80 μm, and a stress at the second transition point is 40 MPa to 100 MPa.