Lithium secondary battery comprising tungsten composite oxide
    26.
    发明授权
    Lithium secondary battery comprising tungsten composite oxide 有权
    包含钨复合氧化物的锂二次电池

    公开(公告)号:US06403258B1

    公开(公告)日:2002-06-11

    申请号:US09533670

    申请日:2000-03-23

    IPC分类号: H01M450

    摘要: In a lithium secondary battery provided with a positive electrode, a negative electrode, and a non-aqueous electrolyte, a tungsten oxide W20O58 or W18O49, or the tungsten oxide to which lithium is added, or a tungsten composite oxide comprising a tungsten oxide containing at least one type of metal element selected from the group consisting of Mn, Cu, V, Cr, Fe, Co, and Ni and having a W20O58-type or W18O49-type crystal structure or the tungsten composite oxide to which lithium is added is used as a positive electrode active material for said positive electrode or a negative electrode active material for said negative electrode.

    摘要翻译: 在设置有正极,负极和非水电解质的锂二次电池中,添加有氧化钨W20O58或W18O49,或者添加有锂的氧化钨,或包含含有氧化钨的钨复合氧化物 使用选自Mn,Cu,V,Cr,Fe,Co和Ni中的至少一种类型的具有W20O58型或W18O49型晶体结构的金属元素或添加了锂的钨复合氧化物 作为所述正极的正极活性物质或所述负极的负极活性物质。

    Non-Aqueous Electrolyte Battery
    27.
    发明申请
    Non-Aqueous Electrolyte Battery 有权
    非水电解质电池

    公开(公告)号:US20080286655A1

    公开(公告)日:2008-11-20

    申请号:US10568420

    申请日:2005-02-14

    IPC分类号: H01M4/58

    摘要: A non-aqueous battery with improved volume energy density and enhanced load characteristics is made available even when using olivine-type lithium phosphate as a positive electrode active material.The non-aqueous electrolyte battery of the present invention is provided with a positive electrode (1) containing lithium iron phosphate as a positive electrode active material, a negative electrode (2), and a non-aqueous electrolyte (4). In the positive electrode (1), a positive electrode active material-containing layer that is made of the positive electrode active material, a conductive agent, and a binder agent is formed on a positive electrode current collector. The positive electrode current collector has a thickness of less than 20 μm and its surface that is in contact with the positive electrode active material-containing layer has a mean surface roughness Ra of greater than 0.026.

    摘要翻译: 即使使用橄榄石型磷酸锂作为正极活性物质,也可以获得体积能量密度提高和负荷特性提高的非水电池。 本发明的非水电解质电池设有含有磷酸铁锂作为正极活性物质的正极(1),负极(2)和非水电解质(4)。 在正极(1)中,在正极集电体上形成由正极活性物质,导电剂和粘合剂构成的含正极活性物质的层。 正极集电体的厚度小于20μm,与正极活性物质含有层接触的表面的平均表面粗糙度Ra大于0.026。