摘要:
The present disclosure relates to an electrode composite material. The electrode composite material includes a number of electrode composite material particles. Each of the plurality of electrode composite material particles includes an electrode active material particle and a doped aluminum phosphate layer coated on a surface of the electrode active material particle. A material of the doped aluminum phosphate layer is a semiconducting doped aluminum phosphate.
摘要:
A lithium titanate composite material includes lithium titanate particles and an AlPO4/C composite layer disposed on a surface of the lithium titanate particles. The AlPO4/C composite layer includes aluminum phosphate and carbon. The lithium titanate composite material, as an anode active material, can be applied to a lithium ion battery to increase its electrochemical stability.
摘要:
The present disclosure relates to a lithium ion battery. The lithium ion battery cathode includes a cathode, a separator, an anode, and a nonaqueous electrolyte solution. The cathode includes a cathode current collector and a cathode material layer disposed on a surface of the cathode current collector. The cathode material layer comprises cathode active material, conductive agent, and adhesive uniformly mixed together. The cathode active material comprises cathode active material particles and AlPO4 layers coated on surfaces of the cathode active material particles. The separator includes a porous membrane and a protective layer coated on a surface of the porous membrane. The protective layer prevents the separator from being melted during charging or discharging of the lithium ion battery.
摘要:
A solid electrolyte includes an interpenetrating polymer network, a plasticizer and a lithium salt. The plasticizer and the lithium salt are dispersed in the interpenetrating polymer network. The interpenetrating polymer network includes CH2—CH2—On segments, and is formed by polymerizing a first monomer R1—OCH2—CH2—OnR2 with a second monomer R3—OCH2—CH2—OmR4 under an initiator. The “R1”, “R2” or “R3” respectively includes —C═C— group or —C≡C— group. The “R4” includes an alkyl group or a hydrogen atom. The “m” and “n” are integers. A molecular weight of the first monomer or a molecular weight of the second monomer is greater than or equal to 100, and less than or equal to 800. The first monomer is less than or equal to 50% of the second monomer by weight. The lithium salt is less than or equal to 10% the second monomer by weight. A lithium based battery using the solid electrolyte is also provided.
摘要:
A method for making a lithium battery cathode composite is provided. First, a plurality of lithium vanadium phosphate particles is provided. A lithium iron phosphate layer is then formed on an outer surface of each of the lithium vanadium phosphate particle by coating a lithium iron phosphate precursor slurry, thereby forming the lithium battery cathode composite.
摘要:
The present disclosure relates to a sulfurized polyacrylonitrile and a lithium-ion battery cathode active material. The sulfurized polyacrylonitrile includes a structural unit. A general molecular formula of the structural unit is C3HNSn, in which n is a positive integer. The lithium-ion battery cathode active material includes sulfurized polyacrylonitrile and a sulfurized polyacrylonitrile with inserted ions.
摘要:
The present disclosure relates to a method for making a conjugated polymer. In the method, polyacrylonitrile, a solvent, and a catalyst are provided. The polyacrylonitrile is dissolved in the solvent to form a polyacrylonitrile solution. The catalyst is uniformly dispersed into the polyacrylonitrile solution. The polyacrylonitrile solution with the catalyst is heated to induce a cyclizing reaction of the polyacrylonitrile, thereby forming a conjugated polymer solution with conjugated polymer.
摘要:
In a method for making sulfurized polyacrylonitrile, polyacrylonitrile, a first solvent, a catalyst, and sulfur or sodium thiosulfate are provided. The polyacrylonitrile is dissolved in the first solvent to form a polyacrylonitrile solution. The catalyst is uniformly dispersed in the polyacrylonitrile solution. The polyacrylonitrile solution with the catalyst is heated to induce a cyclizing reaction of the polyacrylonitrile, thereby forming a first conjugated polymer solution with a conjugated polymer. The sulfur or sodium thiosulfate is uniformly mixed with the conjugated polymer to form a mixture. The mixture is heated to form sulfurized polyacrylonitrile.
摘要:
The present disclosure relates to a method for making a conjugated polymer. In the method, polyacrylonitrile, a solvent, and a catalyst are provided. The polyacrylonitrile is dissolved in the solvent to form a polyacrylonitrile solution. The catalyst is uniformly dispersed into the polyacrylonitrile solution. The polyacrylonitrile solution with the catalyst is heated to induce a cyclizing reaction of the polyacrylonitrile, thereby forming a conjugated polymer solution with the conjugated polymer dissolved therein.
摘要:
A method for making a composite of cobalt oxide is disclosed. An aluminum nitrate solution is provided. Lithium cobalt oxide particles are introduced into the aluminum nitrate solution. The lithium cobalt oxide particles are mixed with the aluminum nitrate solution to form a mixture. A phosphate solution is added into the mixture to react with the aluminum nitrate solution and form an aluminum phosphate layer on surfaces of the lithium cobalt oxide particles. The lithium cobalt oxide particles with the aluminum phosphate layer formed on the surfaces thereof are heat treated to form a lithium cobalt oxide composite. The lithium cobalt oxide composite is electrochemical lithium-deintercalated at a voltage of Vx, wherein 4.5V