Abstract:
Ethylene-based polymers having a density of 0.952 to 0.965 g/cm3, a high load melt index (HLMI) from 5 to 25 g/10 min, a weight-average molecular weight from 275,000 to 450,000 g/mol, a number-average molecular weight from 15,000 to 40,000 g/mol, a viscosity at HLMI from 1400 to 4000 Pa-sec, and a tangent delta at 0.1 sec−1 from 0.65 to 0.98 degrees. These polymers have the processability of chromium-based resins, but with improved stress crack resistance, and can be used in large-part blow molding applications.
Abstract:
A method of determining multimodal polyethylene quality comprising the steps of (a) providing a multimodal polyethylene resin sample; (b) determining, in any sequence, the following: that the multimodal polyethylene resin sample has a melt index within 30% of a target melt index; that the multimodal polyethylene resin sample has a density within 2.5% of a target density; that the multimodal polyethylene resin sample has a dynamic viscosity deviation (% MVD) from a target dynamic viscosity of less than about 100%; that the multimodal polyethylene resin sample has a weight average molecular weight (Mw) deviation (% MwD) from a target Mw of less than about 20%; and that the multimodal polyethylene resin sample has a gel permeation chromatography (GPC) curve profile deviation (% GPCD) from a target GPC curve profile of less than about 15%; and (c) responsive to step (b), designating the multimodal polyethylene resin sample as a high quality resin.
Abstract:
Disclosed herein are ethylene-based polymers generally characterized by a Mw ranging from 70,000 to 200,000 g/mol, a ratio of Mz/Mw ranging from 1.8 to 20, an IB parameter ranging from 0.92 to 1.05, and an ATREF profile characterized by one large peak. These polymers have the dart impact, tear strength, and optical properties of a metallocene-catalyzed LLDPE, but with improved processability, melt strength, and bubble stability, and can be used in blown film and other end-use applications.
Abstract:
Disclosed herein are ethylene-based polymers generally characterized by a Mw ranging from 70,000 to 200,000 g/mol, a ratio of Mz/Mw ranging from 1.8 to 20, an 1B parameter ranging from 0.92 to 1.05, and an ATREF profile characterized by one large peak. These polymers have the dart impact, tear strength, and optical properties of a metallocene-catalyzed LLDPE, but with improved processability, melt strength, and bubble stability, and can be used in blown film and other end-use applications.
Abstract:
Disclosed are ethylene polymer compositions containing a homogeneously-branched first ethylene polymer component and a homogeneously-branched second ethylene polymer component of higher density than the first ethylene polymer component. The ethylene polymer composition can be characterized by a density from 0.912 to 0.925 g/cm3, a melt index less than 3.5 g/10 min, and a CY-a parameter at 190° C. from 0.25 to 0.65. These polymer compositions have the excellent dart impact strength and optical properties of a metallocene-catalyzed LLDPE, but with improved machine direction tear resistance, and can be used in blown film and other end-use applications.
Abstract:
Disclosed herein are ethylene-based polymers having a density greater than 0.945 g/cm3, a high load melt index less than 25 g/10 min, a peak molecular weight ranging from 52,000 to 132,000 g/mol, and an environmental stress crack resistance of at least 250 hours. These polymers have the processability of chromium-based resins, but with improved impact strength and stress crack resistance, and can be used in large-part blow molding applications.
Abstract:
A crosslinked metallocene-catalyzed polyethylene copolymer having a higher molecular weight (HMW) component and lower molecular weight (LMW) component wherein the HMW component is present in an amount of from about 10 wt. % to about 30 wt. % and wherein the LMW component is present in an amount of from about 70 wt. % to about 90 wt. %.
Abstract:
A crosslinked metallocene-catalyzed polyethylene copolymer having a higher molecular weight (HMW) component and lower molecular weight (LMW) component wherein the HMW component is present in an amount of from about 10 wt. % to about 30 wt. % and wherein the LMW component is present in an amount of from about 70 wt. % to about 90 wt. %.
Abstract:
Disclosed herein are polymerization processes for the production of olefin polymers. These polymerization processes can employ a catalyst system containing two or three metallocene components, resulting in ethylene-based copolymers that can have a medium density and improved stress crack resistance.
Abstract:
A metallocene-catalyzed polymer comprising (i) a higher molecular weight component and (ii) a lower molecular weight component wherein the polymer has a polydispersity index of from about 10 to about 26; a zero shear viscosity of from about 5×105 Pa·s to about 2×1014 Pa·s and a smooth-to-matte transition critical stress of from about 20 kPa to about 85 kPa at a shear rate of from about 1.5 s−1 to about 17 s−1. A dual metallocene catalyzed polyethylene comprising (i) a higher molecular weight component and (ii) a lower molecular weight component wherein the polymer has a polydispersity index of from about 10 to about 26; a zero shear viscosity of from about 5×105 Pa·s to about 2×1014 Pa·s and a smooth-to-matte transition stress of from about 20 kPa to about 85 kPa at a shear rate of from about 1.5 s−1 to about 17 s−1.