Abstract:
Embodiments of a glass substrate including an alkali-containing bulk and an alkali-depleted surface layer, including a substantially homogenous composition are disclosed. In some embodiments, the alkali-depleted surface layer includes about 0.5 atomic % alkali or less. The alkali-depleted surface layer may be substantially free of hydrogen and/or crystallites. Methods for forming a glass substrate with a modified surface layer are also provided.
Abstract:
A glass element having a thickness from 25 μm to 125 μm, a first primary surface, a second primary surface, and a compressive stress region extending from the first primary surface to a first depth, the region defined by a compressive stress σI of at least about 100 MPa at the first primary surface. Further, the glass element has a stress profile such that it does not fail when it is subject to 200,000 cycles of bending to a target bend radius of from 1 mm to 20 mm, by the parallel plate method. Still further, the glass element has a puncture resistance of greater than about 1.5 kgf when the first primary surface of the glass element is loaded with a tungsten carbide ball having a diameter of 1.5 mm.
Abstract:
A glass element having a thickness from 25 μm to 125 μm, a first primary surface, a second primary surface, and a compressive stress region extending from the first primary surface to a first depth, the region defined by a compressive stress σI of at least about 100 MPa at the first primary surface. Further, the glass element has a stress profile such that it does not fail when it is subject to 200,000 cycles of bending to a target bend radius of from 1 mm to 20 mm, by the parallel plate method. Still further, the glass element has a puncture resistance of greater than about 1.5 kgf when the first primary surface of the glass element is loaded with a tungsten carbide ball having a diameter of 1.5 mm.
Abstract:
A glass element having a thickness from 25 μm to 125 μm, a first primary surface, a second primary surface, and a compressive stress region extending from the first primary surface to a first depth, the region defined by a compressive stress σI of at least about 100 MPa at the first primary surface. Further, the glass element has a stress profile such that it does not fail when it is held at a bend radius from about 1 mm to about 20 mm for at least 60 minutes at about 25° C. and about 50% relative humidity. Still further, the glass element has a puncture resistance of greater than about 1.5 kgf when the first primary surface of the glass element is loaded with a tungsten carbide ball having a diameter of 1.5 mm.
Abstract:
A glass element having a thickness from 25 μm to 125 μm, a first primary surface, a second primary surface, and a compressive stress region extending from the first primary surface to a first depth, the region defined by a compressive stress σI of at least about 100 MPa at the first primary surface. Further, the glass element has a stress profile such that when the glass element is bent to a target bend radius of from 1 mm to 20 mm, with the center of curvature on the side of the second primary surface so as to induce a bending stress σB at the first primary surface, σI+σB
Abstract translation:一种玻璃元件,其厚度为25μm至125μm,第一主表面,第二主表面和从第一主表面延伸到第一深度的压应力区域,该区域由压缩应力和 在第一主表面处至少约100MPa。 此外,玻璃元件具有应力分布,使得当玻璃元件弯曲到目标弯曲半径为1mm至20mm时,具有在第二主表面侧的曲率中心以引起弯曲应力 &sgr; B在第一个主表面,&sgr; I +&sgr; B <0。 此外,当玻璃元件的第一主表面装载有直径为1.5mm的碳化钨球时,玻璃元件具有≥1.5kgf的耐刺穿性。