摘要:
A method includes heating a glass preform having a plurality of glass layers and drawing the glass preform in a distal direction to form a drawn glass sheet extending distally from the glass preform and having the plurality of glass layers. The drawn glass sheet is thinner than the glass preform. The drawn glass sheet can be rolled onto a collection spool. At least a portion of a glass layer can be removed from the drawn glass sheet. An exemplary glass sheet includes a first glass layer, a second glass layer adjacent to the first glass layer, and a thickness of at most about 0.1 mm. An exemplary ion exchanged glass sheet includes a thickness of at most about 0.1 mm and a surface layer that is under a compressive stress and extends into an interior of the glass sheet to a depth of layer.
摘要:
A glass element having a thickness from 25 μm to 125 μm, a first primary surface, a second primary surface, and a compressive stress region extending from the first primary surface to a first depth, the region defined by a compressive stress σI of at least about 100 MPa at the first primary surface. Further, the glass element has a stress profile such that it does not fail when it is subject to 200,000 cycles of bending to a target bend radius of from 1 mm to 20 mm, by the parallel plate method. Still further, the glass element has a puncture resistance of greater than about 1.5 kgf when the first primary surface of the glass element is loaded with a tungsten carbide ball having a diameter of 1.5 mm.
摘要:
A glass element having a thickness from 25 μm to 125 μm, a first primary surface, a second primary surface, and a compressive stress region extending from the first primary surface to a first depth, the region defined by a compressive stress GI of at least about 100 MPa at the first primary surface. Further, the glass element has a stress profile such that it does not fail when it is subject to 200,000 cycles of bending to a target bend radius of from 1 mm to 20 mm, by the parallel plate method. Still further, the glass element has a puncture resistance of greater than about 1.5 kgf when the first primary surface of the glass element is loaded with a tungsten carbide ball having a diameter of 1.5 mm.
摘要:
According to one or more embodiments described herein, a laminate glass article may be produced by a method that includes providing a first glass sheet and a second glass sheet, assembling the first glass sheet and second glass sheet into a glass stack, and bonding the first glass sheet to the second glass sheet to form the laminate glass article. In one or more embodiments, an intermediate layer may be positioned between the first bonding surface and the second bonding surface, the first bonding surface and the second bonding surface may be roughened surfaces, or the first bonding surface and the second bonding surface may be chemically treated by vacuum deposition.
摘要:
A method includes contacting a glass sheet with a forming surface to form a shaped glass article. An effective viscosity of the glass sheet during the contacting step is less than a contact viscosity of the glass sheet in contact with the forming surface during the contacting step.
摘要:
A glass element having a thickness from 25 μm to 125 μm, a first primary surface, a second primary surface, and a compressive stress region extending from the first primary surface to a first depth, the region defined by a compressive stress σI of at least about 100 MPa at the first primary surface. Further, the glass element has a stress profile such that it does not fail when it is subject to 200,000 cycles of bending to a target bend radius of from 1 mm to 20 mm, by the parallel plate method. Still further, the glass element has a puncture resistance of greater than about 1.5 kgf when the first primary surface of the glass element is loaded with a tungsten carbide ball having a diameter of 1.5 mm.
摘要:
A glass element having a thickness from 25 μm to 125 μm, a first primary surface, a second primary surface, and a compressive stress region extending from the first primary surface to a first depth, the region defined by a compressive stress σI of at least about 100 MPa at the first primary surface. Further, the glass element has a stress profile such that it does not fail when it is subject to 200,000 cycles of bending to a target bend radius of from 1 mm to 20 mm, by the parallel plate method. Still further, the glass element has a puncture resistance of greater than about 1.5 kgf when the first primary surface of the glass element is loaded with a tungsten carbide ball having a diameter of 1.5 mm.
摘要:
A glass element having a thickness from 25 μm to 125 μm, a first primary surface, a second primary surface, and a compressive stress region extending from the first primary surface to a first depth, the region defined by a compressive stress GI of at least about 100 MPa at the first primary surface. Further, the glass element has a stress profile such that it does not fail when it is subject to 200,000 cycles of bending to a target bend radius of from 1 mm to 20 mm, by the parallel plate method. Still further, the glass element has a puncture resistance of greater than about 1.5 kgf when the first primary surface of the glass element is loaded with a tungsten carbide ball having a diameter of 1.5 mm.
摘要:
A method includes heating a glass preform having a plurality of glass layers and drawing the glass preform in a distal direction to form a drawn glass sheet extending distally from the glass preform and having the plurality of glass layers. The drawn glass sheet is thinner than the glass preform. The drawn glass sheet can be rolled onto a collection spool. At least a portion of a glass layer can be removed from the drawn glass sheet. An exemplary glass sheet includes a first glass layer, a second glass layer adjacent to the first glass layer, and a thickness of at most about 0.1 mm. An exemplary ion exchanged glass sheet includes a thickness of at most about 0.1 mm and a surface layer that is under a compressive stress and extends into an interior of the glass sheet to a depth of layer.
摘要:
A glass element having a thickness from 25 μm to 125 μm, a first primary surface, a second primary surface, and a compressive stress region extending from the first primary surface to a first depth, the region defined by a compressive stress σI of at least about 100 MPa at the first primary surface. Further, the glass element has a stress profile such that it does not fail when it is subject to 200,000 cycles of bending to a target bend radius of from 1 mm to 20 mm, by the parallel plate method. Still further, the glass element has a puncture resistance of greater than about 1.5 kgf when the first primary surface of the glass element is loaded with a tungsten carbide ball having a diameter of 1.5 mm.