摘要:
A process for the continuous anionic polymerization or copolymerization of styrene or diene monomers using an alkali metal alkyl compound as polymerization initiator is carried out in the presence of an alkyl- or arylmetal compound of an element which occurs in at least divalent form as rate regulator, preferably under non-isothermal conditions and without back-mixing in a tubular or tube-bundle reactor, preferably using an alkyl- or arylmetal compound A of the formula R1M1 and an alkyl- or arylmetal compound B of the formula R2nM2 in a molar ratio between B and A of from 0.1:1 to 500:1, where M1 is Li, Na or K; R1 is hydrogen, C1-C20-alkyl, C6-C20-aryl, or C7-C20-alkyl-substituted aryl; M2 is an n-valent element from group 2a, 2b or 3a of the Periodic Table; and R2 is hydrogen, halogen, C1-C20-alkyl or C6-C20-aryl; and a special anionic polymerization initiator containing no Lewis base.
摘要:
Polymer mixtures comprise P1) from 1 to 85% by weight of an elastomeric block copolymer which has been built up from hard blocks S made from vinylaromatic monomers and from random soft blocks B/S made up from dienes and from vinylaromatic monomers, and which contains at least the block structure S-B/S-S, where the diene content is less than 50 percent by weight and the proportion of the soft phase formed from the blocks B/S is at least 60 percent by weight, based in each case on the entire block copolymer, P2) from 5 to 89% by weight of a block copolymer differing from P1) and made from vinylaromatic monomers and from dienes, P3) from 10 to 94% by weight of glass-clear or impact-modified polystyrene or mixtures thereof, and P4) from 0 to 84% by weight of other additives, where the total of components P1) to P4) is 100%.
摘要:
A molding material as based on from 60 to 98% by weight of a hard matrix A comprising polymerized or copolymerized units of at least one vinylaromatic monomer or at least one vinylaromatic monomer and at least one polar comonomer and from 2 to 40% by weight, the percentages in each case being based on the molding material comprising A and B, of a soft phase B formed from a hydrogenated or unhydrogenated block copolymer prepared by anionic polymerization and comprising a vinylaromatic monomer V and a diene D, having at least one random or quasi-random block (V/D) of vinylaromatic monomer and diene and containing from 10 to 80% by weight, based on the soft phase B, of occlusions of matrix material (a) formed during the polymerization of the hard matrix A in the presence of the block rubber, and said molding material is used for the production of films, sheets or moldings.
摘要:
Thermoplastic molding compositions comprise:______________________________________ A) from 20 to 96% by weight of star polymers obtainable by polymerizing vinylaromatic monomers with a branched monomer building block which contains at least two vinylaromatic functions, B) from 3 to 50% by weight of copolymers comprising vinylaromatic monomers, 1,1-diphenylethylene and, if desired, dienes, C) from 1 to 15% by weight of polyarylene ethers, D) from 0 to 5% by weight of nucleating agents, E) from 0 to 5% by weight of antioxidants, F) from 0 to 5% by weight of stabilizers, and G) from 0 to 50% by weight of fibrous or particulate fillers. ______________________________________
摘要:
A polydiene which is obtainable by anionic polymerization of a diene using a bifunctional Li initiator followed by polymer-like reaction and which contains at least one ethanolamine or oligoetherolamine terminal group of the general structure I ##STR1## in which R.sup.1 denotes alkyl or aryl, Ar denotes aryl, R.sup.2 denotes alkyl or hydrogen, and R.sup.3 denotes aryl, alkyl, or hydrogen and X can assume a value from 1 to 10, and the hydrogenation products thereof.
摘要:
A process for preparing bifunctional living polymers which are able to forth bifunctional telechelic polymers or block copolymers with at least 3 blocks of conjugated dienes and/or vinylaromatics with molecular weights of from 1,500 to 500,000, by bifunctional initiators whose anionic centers are aliphatic carbon atoms which are substituted by lithium and an aliphatic hydrocarbon radical as well as by either 2 aryl radicals or by one aryl radical and one hydrogen radical, where one of the aryl radicals can also be part of the two anionic centers, in a first stage being reacted in the presence of not more than 2.5 moles of an aliphatic ether or a tertiary amine per mole of lithium and not less than 2 mol/l of a conjugated diene at from -40.degree. to +35.degree. C. with not less than two moles of diene, resulting in the formation of low molecular weight diene oligomers which in turn act as bifunctional initiators, and using the latter in a second reaction stage in a conventional manner at above 40.degree. C., with or without the addition of other monomers, to obtain polymers of the required molecular weight.
摘要:
A process for the preparation of polymers of isobutene having tertiary chloride groups by reaction of appropriate polymers which have been prepared by cationic polymerization of isobutene with hydrogen chloride.
摘要:
A mixture which comprises from 5 to 50% by weight of a block copolymer A, which comprises one or more copolymer blocks (B/S)A each composed of from 65 to 95% by weight of vinylaromatic monomers and from 35 to 5% by weight of dienes and of a glass transition temperature TgA in the range from 40° to 90° C.; from 95 to 50% by weight of a block copolymer B, which comprises at least one hard block S composed of vinylaromatic monomers and comprises one or more copolymer blocks (B/S)B each composed of from 20 to 60% by weight of vinylaromatic monomers and from 80 to 40% by weight of dienes and of a glass transition temperature TgB in the range from −70° to 0° C.; from 0 to 45% by weight of polystyrene or of a block copolymer C other than A and B; and from 0 to 6% by weight of a plasticizer; and its use for production of shrink films.
摘要:
Elastomeric block copolymers having star-shaped molecular architecture, where the star-shaped molecular architecture has at least two different arms of the star, a process for producing the elastomeric block copolymers, the use of the elastomeric block copolymers for producing moldings, or as adhesive layer in multilayer foils; as seal; as adhesion promoter or thermoplastic component in wood-plastics composites; as hot-melt adhesive component; for impact-modifying thermoplastics or elastomers, or for compatibilization, and to foils, foams, thermomoldings, injection moldings, flexible tubing, or profile extrudates composed of at least one elastomeric block copolymer.
摘要:
The present invention relates to a thermoplastic molding composition comprising (A) as component A, particles composed of at least one oxidatively crosslinked vegetable oil as core, encapsulated by at least one thermoplastic, (B) as component B, at least one further thermoplastic compatible with the at least one thermoplastic present in the shell of component A, (C) as component C, at least one resin compatible with the at least one thermoplastic present in the shell of component A, (D) as component D, at least one filler, and (E) as component E, if appropriate, further additives, and also to a process for the production of the thermoplastic molding composition.