Abstract:
Disclosed herein are sealing solutions for sealing water-soluble films, in particular aqueous mixtures including one or more polymeric solvents such as polyols. Aqueous sealing solutions including a relatively dilute solvent for one or more polymeric components of the water-soluble film (e.g., water-soluble polymeric components thereof, such as polyvinyl alcohol (PVOH)) can exhibit one or more benefits, including a reduction in dissolution of the film by the sealing solution and an increase in seal strength. Also disclosed are sealed articles formed with the sealing solutions, for example water-soluble packets containing various liquid or solid compositions.
Abstract:
Disclosed herein are sealing solutions for sealing water-soluble films, in particular aqueous mixtures including one or more polymeric solvents such as polyols. Aqueous sealing solutions including a relatively dilute solvent for one or more polymeric components of the water-soluble film (e.g., water-soluble polymeric components thereof, such as polyvinyl alcohol (PVOH)) can exhibit one or more benefits, including a reduction in dissolution of the film by the sealing solution and an increase in seal strength. Also disclosed are sealed articles formed with the sealing solutions, for example water-soluble packets containing various liquid or solid compositions.
Abstract:
Provided herein are water-soluble films comprising a water soluble polymer such as polyvinyl alcohol (PVOH) and high content of water-soluble starch, and related water-soluble film forming solutions, articles made therefrom e.g., pouches or packets, and methods of preparation and use of same.
Abstract:
A water-soluble film, comprising a first water-soluble film, wherein the first water soluble film disintegrates in water within less than about 24 hours and dissolves in water within less than about 48 hours as measured by the MSTM-205 at 20° C. The disclosure provides a water-soluble film comprising a first water-soluble film that disintegrates in water within less than 24 hours and dissolves in water within less than 48 hours as measured by MSTM-205 at 20° C. The first water-soluble film optionally may be further characterized in that it does not disintegrate in water for at least about 1 hour and does not dissolve in water for at least about 1 hour as measured by MSTM-205 at 20° C. The disclosure further provides a water-soluble film comprising a first water-soluble film characterized in that the degradation and/or dissolution of the first water-soluble film is adapted to be activated by consumer handling.
Abstract:
A fiber having a surface region and an interior region includes a polymer comprising at least one of a vinyl acetate moiety or a vinyl alcohol moiety, the fiber having a transverse cross-section including the interior region comprising the polymer having a first degree of hydrolysis and the surface region comprising the polymer having a second degree of hydrolysis greater than the first degree of hydrolysis.
Abstract:
Thermoformed articles comprising a film thermoformed to be in the form of a pouch defining an interior pouch volume, the film comprising a mixture of a polyvinyl alcohol resin and a plasticizer, wherein the plasticizer is provided in an amount in a range of about 5 to about 30 weight parts, based on 100 weight parts of total polyvinyl alcohol resin; wherein the thermoformed film in the form of a pouch defining an interior pouch volume is characterized by a draw ratio in a range of about 2.3 to about 2.9; the article is characterized by a release time of at least 30 seconds when formed into a sealed packet and tested in accordance with the Liquid Release Test; and the article is characterized by a residue value of at most 9%, as determined by the Residue Test.
Abstract:
Disclosed herein are multilayer water-dispersible articles, optionally a film, comprising a water-soluble polymer and a wax. Also disclosed are multilayer water-dispersible articles including a water-dispersible substrate layer having a thickness in a range of about 5 μm to about 10 mm, and a water-dispersible coating layer on the substrate layer, the coating layer having a thickness in a range of about 0.5 to about 250 μm, wherein water-dispersible article has a moisture vapor transmission rate (MVTR) of about 60 g H2O/m2/day to about 300 g H2O/m2/day or less.
Abstract:
Disclosed herein are water-soluble films and/or water soluble unit dose articles comprising a water soluble mixture comprising a polyvinyl alcohol (PVOH) and a polyvinylpyrrolidone (PVP), and methods of making and using the same.
Abstract:
The present disclosure relates to pouches made from a combination of chemically different water-soluble films and optionally containing a composition (e.g. a household care composition or non-household care composition) that is at least partially enclosed by the water-soluble films in at least one compartment.
Abstract:
Perfume microcapsule-containing films, related solutions, and containers including the films (e.g. detergent packets) are disclosed, together with their methods of preparation and use.