New Asphalt Mixtures
    82.
    发明申请

    公开(公告)号:US20210139705A1

    公开(公告)日:2021-05-13

    申请号:US17053101

    申请日:2019-05-15

    发明人: Zeev Livnat

    IPC分类号: C08L95/00 C08L19/00

    摘要: The invention provides a new additive for replacing a part of asphalt in road construction mixtures, while enhancing their capability to withstand severe traffic and weather stresses in a cost-effective and environmentally friendly way.

    RECYCLED ASPHALT COMPOSITIONS AND METHODS THEREOF

    公开(公告)号:US20210079599A1

    公开(公告)日:2021-03-18

    申请号:US17104738

    申请日:2020-11-25

    发明人: John Corcoran

    摘要: A pavement composition includes a recycled hot mix asphalt (HMA) sheet mix composition including more than 50% and up to 100% recycled fines mixed with a rejuvenating agent. The recycled fines of the HMA sheet mix are separated from a reclaimed asphalt pavement (RAP) composition and substantially all of the recycled fines are capable of passing through a sieve having an opening size of ⅜ inch (9.5 mm). Pavement systems include an existing pavement layer and a thin-lift overlay made of the recycled HMA sheet mix on the existing pavement layer. Pavement systems also include a three-layer system including a leveling course layer, an interlayer, and a surface course layer in which the leveling course layer and/or the surface course layer include a recycled HMA sheet mix composition.

    Asphalt composition for road pavement

    公开(公告)号:US10934434B2

    公开(公告)日:2021-03-02

    申请号:US16071316

    申请日:2017-01-18

    摘要: Asphalt composition for road pavement, excellent in drying strength, strength after immersion in water, and strength after immersion in petroleum, method for producing same, and road paving method. Composition comprises asphalt, polyester, and aggregate. Polyester has alcohol component-derived constituent unit containing ≥65 mol % bisphenol A/alkylene oxide adduct and carboxylic acid component-derived constituent unit containing ≥50 mol % terephthalic or isophthalic acid. Composition has softening point of 95°−130° C., hydroxyl group value of 20-50 mgKOH/g, and ratio of polyester resin of 5-50 parts by mass based on 100 parts by mass of the asphalt. Production method comprising mixing asphalt, the polyester, and aggregate at 130-200° C. for ≥30 seconds. Polyester resin is mixed in ratio of 5-50 parts by mass based on 100 parts by mass of asphalt. Road paving method comprises laying asphalt composition obtained by production method as set forth, thereby forming an asphalt paving material layer.