摘要:
A method for passivating a metallic surface, by treating the surface with a basic aqueous composition comprising one polymer comprising acidic groups, a cationic crosslinker and a volatile basic compound, allows a durable passivation of fragile metal surfaces.
摘要:
Aqueous leachant compositions and processes for using the same comprising: (a) providing a metal-containing compound; and (b) subjecting the metal-containing compound to an acid digestion comprising contacting the metal-containing compound with an aqueous leachant; wherein the aqueous leachant comprises a mixture selected from the group consisting of: (i) sulfuric acid and one or more alkanesulfonic acids having alkane moieties selected from the group consisting of propyl, ethyl and methyl groups, at a weight ratio of alkanesulfonic acid to sulfuric acid of 1:1000 to 1:1; (ii) sulfuric acid and one or more salts of alkanesulfonic acids having alkane moieties selected from the group consisting of propyl, ethyl and methyl groups, at a weight ratio of salt of alkanesulfonic acid to sulfuric acid of 1:9 to 1:99.
摘要:
The invention relates to a process for obtaining gold-colored aluminum oxide layers in which the coloring of the oxidized surface of the aluminum or aluminum alloys is carried out by an electrolytic process in an electrolyte comprising an alkanesulfonic acid and an alkanesulfonate of silver, and to the use of the gold-colored workpieces based on aluminum or aluminum alloys produced by this process for decorative purposes.The invention furthermore relates to an electrolyte solution for coloring the oxidized surface of aluminum or aluminum alloys gold by an electrolytic process, and to the use of an electrolyte comprising an alkanesulfonate of silver for coloring aluminum oxide layers based on aluminum or aluminum alloys gold in an electrolytic process.
摘要:
A continuous method for surface treatment of metal strips applies a finish coat having a thickness of not more than 3 μm, the apparatus employed for application being equipped with at least one IR sensor which faces a coated side of the strip, operates in reflection geometry, and serves to measure the coat thickness of the finish coat, with the strip running.
摘要:
A continuous method for surface treatment of metal strips applies a finish coat having a thickness of not more than 3 μm, the apparatus employed for application being equipped with at least one IR sensor which faces a coated side of the strip, operates in reflection geometry, and serves to measure the coat thickness of the finish coat, with the strip running.
摘要:
Aqueous leachant compositions and processes for using the same comprising: (a) providing a metal-containing compound; and (b) subjecting the metal-containing compound to an acid digestion comprising contacting the metal-containing compound with an aqueous leachant; wherein the aqueous leachant comprises a mixture selected from the group consisting of: (i) sulfuric acid and one or more alkanesulfonic acids having alkane moieties selected from the group consisting of propyl, ethyl and methyl groups, at a weight ratio of alkanesulfonic acid to sulfuric acid of 1:1000 to 1:1; (ii) sulfuric acid and one or more salts of alkanesulfonic acids having alkane moieties selected from the group consisting of propyl, ethyl and methyl groups, at a weight ratio of salt of alkanesulfonic acid to sulfuric acid of 1:9 to 1:99.
摘要:
A method for passivating a metallic surface, by treating the surface with a basic aqueous composition comprising one polymer comprising acidic groups, a cationic crosslinker and a volatile basic compound, allows a durable passivation of fragile metal surfaces.
摘要:
A method for passivating metallic surfaces, wherein the surface is contacted with an aqueous composition comprising at least one water-soluble polymer (X) comprising acidic groups and with at least one surfactant (T) based on alkoxylated alcohols, the pH of the composition being in the range from 0.5 to 5, enables durable protection of the surface.
摘要:
A method for passivating metallic surfaces, wherein the surface is contacted with an aqueous composition comprising at least one water-soluble polymer (X) comprising acidic groups and with at least one surfactant (T) based on alkoxylated alcohols, the pH of the composition being in the range from 0.5 to 5, enables durable protection of the surface.
摘要:
Aqueous leachant compositions and processes for using the same comprising: (a) providing a metal-containing compound; and (b) subjecting the metal-containing compound to an acid digestion comprising contacting the metal-containing compound with an aqueous leachant; wherein the aqueous leachant comprises a mixture selected from the group consisting of: (i) sulfuric acid and one or more alkanesulfonic acids having alkane moieties selected from the group consisting of propyl, ethyl and methyl groups, at a weight ratio of alkanesulfonic acid to sulfuric acid of 1:1000 to 1:1; (ii) sulfuric acid and one or more salts of alkanesulfonic acids having alkane moieties selected from the group consisting of propyl, ethyl and methyl groups, at a weight ratio of salt of alkanesulfonic acid to sulfuric acid of 1:9 to 1:99.