公开(公告)号:US08986469B2
公开(公告)日:2015-03-24
申请号:US12741818
申请日:2008-11-10
CPC分类号: C22C45/02 , B22F2998/00 , C21D1/26 , C21D8/0215 , C21D2201/03 , C21D2211/004 , C22C1/002 , C22C1/0458 , C22C33/0278 , C22C33/0285 , C22C45/00 , C22C45/10 , C22C2200/02 , B22F3/14 , B22F3/1035
摘要: Design and fabrication processes and compositions for bulk metallic glass materials. Examples of bulk metallic glasses based on the described compositions may contain a high atomic percent of titanium or iron, which is alloyed with metalloid elements and refractory metals. The compositions can be designed using theoretical calculations of the liquidus temperature to have substantial amounts of refractory metals, while still maintaining a depressed liquidus temperature. The alloying elements are molybdenum, tungsten, chromium, boron, and carbon may be used. Some of the resulting alloys are ferromagnetic at room temperature, while others are non-ferromagnetic. These amorphous alloys have increased specific strengths and corrosion resistance compared to conventional high strength steels.
摘要翻译: 散装金属玻璃材料的设计和制造工艺及组成。 基于所述组合物的块状金属玻璃的实例可以包含与准金属元素和难熔金属合金化的高原子百分比的钛或铁。 可以使用液相线温度的理论计算来设计组合物以具有大量的难熔金属,同时仍保持液相线温度降低。 合金元素是钼,钨,铬,硼,可以使用碳。 一些所得合金在室温下是铁磁性的,而另一些则是非铁磁性的。 与常规高强度钢相比,这些非晶合金具有增加的比强度和耐腐蚀性。
-
公开(公告)号:US20110048587A1
公开(公告)日:2011-03-03
申请号:US12741818
申请日:2008-11-10
IPC分类号: C22C45/10
CPC分类号: C22C45/02 , B22F2998/00 , C21D1/26 , C21D8/0215 , C21D2201/03 , C21D2211/004 , C22C1/002 , C22C1/0458 , C22C33/0278 , C22C33/0285 , C22C45/00 , C22C45/10 , C22C2200/02 , B22F3/14 , B22F3/1035
摘要: Design and fabrication processes and compositions for bulk metallic glass materials. Examples of bulk metallic glasses based on the described compositions may contain a high atomic percent of titanium or iron, which is alloyed with metalloid elements and refractory metals. The compositions can be designed using theoretical calculations of the liquidus temperature to have substantial amounts of refractory metals, while still maintaining a depressed liquidus temperature. The alloying elements are molybdenum, tungsten, chromium, boron, and carbon may be used. Some of the resulting alloys are ferromagnetic at room temperature, while others are non-ferromagnetic. These amorphous alloys have increased specific strengths and corrosion resistance compared to conventional high strength steels.
摘要翻译: 散装金属玻璃材料的设计和制造工艺及组成。 基于所述组合物的块状金属玻璃的实例可以包含与准金属元素和难熔金属合金化的高原子百分比的钛或铁。 可以使用液相线温度的理论计算来设计组合物以具有大量的难熔金属,同时仍保持液相线温度降低。 合金元素是钼,钨,铬,硼,可以使用碳。 一些所得合金在室温下是铁磁性的,而另一些则是非铁磁性的。 与常规高强度钢相比,这些非晶合金具有增加的比强度和耐腐蚀性。
-