Bulk Hydroprocessing Catalyst Comprising A Group VIII Metal And Molybdenum, Preparation And Use Thereof
    1.
    发明申请
    Bulk Hydroprocessing Catalyst Comprising A Group VIII Metal And Molybdenum, Preparation And Use Thereof 有权
    包含VIII族金属和钼的大量加氢催化剂,其制备和使用

    公开(公告)号:US20090139904A1

    公开(公告)日:2009-06-04

    申请号:US12091328

    申请日:2006-10-25

    Abstract: The invention relates to a bulk catalyst comprising at least 60 wt % metal oxidic particles comprising one or more Group VIII metals and Group VIB metal molybdenum, comprising less than 10 mole % of a second Group VIB metal (relative to the total amount of Group VIB metals) and comprising a Group V metal in an amount less than 10 mole % (relative to the total of the Group VIB metals), which bulk catalyst has been calcined at a temperature below a temperature where the hexagonal metastable crystal structure changes to an inactive crystalline structure, preferably below 450° C. and which bulk catalyst has a metastable hexagonal phase characterized by an X-ray diffraction pattern having reflections at 33-35 and 58-61° 2θ. Preferably, the main reflections have a full width at half maximum (FWHM) of less than 2.5. The invention further relates to a process for the manufacture of the bulk catalyst, to the corresponding sulphided bulk catalyst and to the use of said catalyst or sulphided catalyst in the hydroprocessing, in particular the hydrodesulphurisation and hydrodenitrogenation, of a hydrocarbon feedstock.

    Abstract translation: 本发明涉及一种本体催化剂,其包含至少60重量%的包含一种或多种第VIII族金属和VIB族金属钼的金属氧化物颗粒,其包含小于10摩尔%的第二族VIB金属(相对于VIB族的总量) 金属),并且包含少于10摩尔%(相对于第VIB族金属的总量)的第V族金属,该体积催化剂在低于六方晶系亚稳晶体结构变为不活泼的温度的温度下被煅烧 晶体结构,优选低于450℃,并且该体积催化剂具有亚稳态六方晶相,其特征在于具有在33-35和58-61°2θ之间的反射的X射线衍射图。 优选地,主反射具有小于2.5的半高宽(FWHM)。 本发明还涉及一种用于制造本体催化剂的方法,相应的硫化体积催化剂以及所述催化剂或硫化催化剂在烃原料的加氢处理,特别是加氢脱硫和加氢脱氮中的用途。

    Bulk hydroprocessing catalyst comprising a group VIII metal and molybdenum, preparation and use thereof
    3.
    发明授权
    Bulk hydroprocessing catalyst comprising a group VIII metal and molybdenum, preparation and use thereof 有权
    包含第VIII族金属和钼的本体加氢处理催化剂,其制备和用途

    公开(公告)号:US08486259B2

    公开(公告)日:2013-07-16

    申请号:US12091328

    申请日:2006-10-25

    Abstract: The invention relates to a bulk catalyst comprising at least 60 wt % metal oxidic particles comprising one or more Group VIII metals and Group VIB metal molybdenum, comprising less than 10 mole % of a second Group VIB metal (relative to the total amount of Group VIB metals) and comprising a Group V metal in an amount less than 10 mole % (relative to the total of the Group VIB metals), which bulk catalyst has been calcined at a temperature below a temperature where the hexagonal metastable crystal structure changes to an inactive crystalline structure, preferably below 450° C. and which bulk catalyst has a metastable hexagonal phase characterized by an X-ray diffraction pattern having reflections at 33-35 and 58-61° 2θ. Preferably, the main reflections have a full width at half maximum (FWHM) of less than 2.5. The invention further relates to a process for the manufacture of the bulk catalyst, to the corresponding sulphided bulk catalyst and to the use of said catalyst or sulphided catalyst in the hydroprocessing, in particular the hydrodesulphurisation and hydrodenitrogenation, of a hydrocarbon feedstock.

    Abstract translation: 本发明涉及一种本体催化剂,其包含至少60重量%的包含一种或多种第VIII族金属和VIB族金属钼的金属氧化物颗粒,其包含小于10摩尔%的第二族VIB金属(相对于VIB族的总量) 金属),并且包含少于10摩尔%(相对于第VIB族金属的总量)的第V族金属,该体积催化剂在低于六方晶系亚稳晶体结构变为不活泼的温度的温度下被煅烧 晶体结构,优选低于450℃,并且该体积催化剂具有亚稳态六方晶相,其特征在于具有在33-35和58-61°2θ之间的反射的X射线衍射图。 优选地,主反射具有小于2.5的半高宽(FWHM)。 本发明还涉及一种用于制造本体催化剂的方法,相应的硫化体积催化剂以及所述催化剂或硫化催化剂在烃原料的加氢处理,特别是加氢脱硫和加氢脱氮中的用途。